Abstract The influence of eight different chlorides (BaCl 2 , CaCl 2 , KCl, LiCl, MgCl 2 , NaCl, PbCl 2 , and ZnCl 2 ) on the oxidation of metallic chromium powder was studied at four different temperatures (400 °C, 500 °C, 550 °C, and 600 °C) under dry conditions in synthetic air by using a DTA/TG-apparatus. BaCl 2 , CaCl 2 , and MgCl 2 did not react with chromium at any of the studied temperatures. ZnCl 2 evaporated already before the air was introduced. KCl, LiCl, NaCl, and PbCl 2 were all found to be reactive and to accelerate the oxidation of chromium. LiCl reacted only at 600 °C, whereas the other three chlorides mentioned above reacted from 500 °C upwards.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. The implications of chlorine-associated corrosion on the operation of biomass-fired boilers10.1016/S0360-1285(00)00003-4 ↗
2. Utilizing biomass and waste for power production – a decade of contributing to the understanding, interpretation and analysis of deposits and corrosion products10.1016/j.fuel.2004.08.026 ↗
3. Salt melt induced corrosion of metallic materials in waste incineration plants10.1002/(SICI)1521-4176(199907)50:7<373::AID-MACO373>3.0.CO;2-T ↗
4. Ellipsometric examination of the thermal oxidation process for plated chromium films10.1016/0040-6090(81)90321-7 ↗
5. The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
6. KCl induced corrosion of a 304-type austenitic stainless steel at 600 °C; the role of potassium10.1007/s11085-005-5704-3 ↗
7. Accelerated oxidation rate of chromium induced by sodium chloride10.1007/BF00659274 ↗
8. NaCl-induced accelerated oxidation of chromium10.1007/BF00659184 ↗
9. High temperature interaction of pure Cr with KCl10.4028/www.scientific.net/MSF.461-464.1047 ↗
10. Corrosion behavior of Fe–Ni–Cr alloys in the molten salt of LiCl–Li2O at high temperature10.1016/j.jnucmat.2003.10.011 ↗
11. Corrosion behavior of pure Cr with a solid NaCl deposit in O2 plus water vapor10.1023/A:1004690518225 ↗
12. Local reactions of KCl particles with iron, nickel and chromium surfaces10.1002/maco.200503903 ↗
13. The role of chloride salts on high temperature corrosion of 321 stainless steel
14. Effect of ZnCl2 vapor on high temperature oxidation of pure chromium10.1023/A:1023776615336 ↗
15. Vapor pressure measurement of zinc oxychloride10.1016/j.jpcs.2004.06.085 ↗
16. Corrosion behavior of 12CrMoV steel in waste incineration environments: hot corrosion by molten chlorides10.1023/A:1018851029023 ↗
17. Fe, Ni, Cr and several Fe-based alloys induced by ZnCl2–KCl at 450 °C in oxidizing environment10.1016/S0921-5093(02)00386-6 ↗
18. Kinetic investigations on salt melt induced high-temperature corrosion of pure metals10.4028/www.scientific.net/MSF.461-464.61 ↗
19. Thermodynamic and kinetic consideration on the corrosion of Fe, Ni and Cr beneath a molten KCl–ZnCl2 mixture10.1016/j.corsci.2005.02.015 ↗
20. Corrosion of three commercial steels under ZnCl2–KCl deposits in a reducing atmosphere containing HCl and H2S at 400–500 °C10.1007/s11085-006-9047-5 ↗
21. Accelerated corrosion of five commercial steels under a ZnCl2–KCl deposit in a reducing environment typical of waste gasification at 673–773 K10.1016/j.corsci.2008.03.004 ↗
22. Corrosion of iron (ARMCO) in KCl–LiCl melts10.1016/S0010-938X(72)91224-3 ↗
23. Effect of oxide ion donors on the corrosion and dechromization of stainless steels in KCl–NaCl–BaCl2 melt10.1023/A:1003499002185 ↗
24. A thermodynamic approach on vapor-condensation of corrosive salts from flue gas on boiler tubes in waste incinerators10.1016/j.corsci.2008.02.004 ↗
25. The role of molten salts in the corrosion of metals in waste incineration plants
26. S. Enestam, D. Bankiewicz, J. Tuiremo, K. Mäkelä, M. Hupa, The corrosivity of alkali chlorides on superheater steels: are KCl and NaCl equally corrosive? Corrosion Science, submitted for publication
27. SGTE data for pure elements10.1016/0364-5916(91)90030-N ↗
28. M.W. Chase Jr., NIST-JANAF Thermochemical Tables, Journal of Physical and Chemical Reference Data, Monograph No. 9, Parts I and II, fourth ed., American Chemical Society and the American Institute of Physics, New York, 1998.
29. Thermodynamic evaluation and optimization of the (NaCl+KCl+MgCl2+CaCl2+ZnCl2) system10.1016/j.jct.2010.10.013 ↗
30. FactSage thermochemical software and databases – recent developments10.1016/j.calphad.2008.09.009 ↗