Interfacial corrosion of copper in concentrated chloride solution and the formation of copper hydroxychloride
Source abstract
Abstract
Abstract This work aims to investigate the waterline corrosion of pure copper in 4 M NaCl solution. Three distinct regions are identified. Corrosion products formed at the waterline are characterized by micro-Raman spectroscopy, complemented by SEM/EDS, as a function of immersion time. The co-existence of four copper species is explained by thermodynamic equilibrium consideration. The composition of spreading region is determined and compared with the oxide film formation in different pH NaOH solutions. The anodic dissolution of copper exposed to the bulk electrolyte is investigated by electrochemical methods. The pH and potential profiles across three regions are proposed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Electrodeposition and Electroless Coatings · Electrochemical Analysis and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Francis · 2010
2. Leygraf · 2016
3. Scott · 2002
4. Electrochemical aspects of copper atmospheric corrosion in the presence of sodium chloride10.1016/j.electacta.2018.04.184 ↗
5. Jones · 1996
6. In situ Raman spectroscopic identification of rust formation in Evans’ droplet experiments10.1016/j.elecom.2012.02.014 ↗
7. In situ studies of the effect of CO2 on the initial NaCl-induced atmospheric corrosion of copper10.1149/1.1984448 ↗
8. The initiation mechanism of corrosion of zinc by sodium chloride particle deposition10.1016/S0010-938X(01)00056-7 ↗
9. A study by voltammetry and the photocurrent response method of copper electrode behavior in acidic and alkaline solutions containing chloride ions10.1016/0022-0728(94)03577-P ↗
10. Kinetics and mechanisms of Cu electrodissolution in chloride media10.1149/1.2108335 ↗
11. Measurement of temperature-dependent stability constants of Cu(I) and Cu(II) chloride complexes by voltammetry at a Pt ultramicroelectrode10.1021/acs.analchem.5b00052 ↗
12. Electrochemistry of high concentration copper chloride complexes10.1021/ac4016769 ↗
13. A spectrophotometric study of copper(I) chloro-complexes in aqueous 5M Na(Cl, ClO4) solutions10.1246/bcsj.49.82 ↗
14. Raman spectra and solvent-extractions of cuprous halides10.1039/jr9630005134 ↗
15. Voltammetry study of copper in chloride solution10.1016/0013-4686(88)80192-0 ↗
16. Oxygen reduction on copper in neutral NaCl solution10.1016/0022-0728(94)03705-8 ↗
17. Electrochemical corrosion of unalloyed copper in chloride media––a critical review10.1016/S0010-938X(02)00257-3 ↗
18. Modelling of copper etching in aerated chloride solutions10.1023/A:1003218422689 ↗
19. Mechanism of pitting corrosion of copper in supply waters10.1179/000705967798326731 ↗
20. Developments leading to the present understanding of the mechanism of pitting corrosion of copper10.1179/000705972798323332 ↗
21. Pourbaix · 1974
22. An EQMB examination of Cu surface oxides in borate buffer10.1016/j.electacta.2003.11.033 ↗
23. Passivity and pit stability behavior of copper as a function of selected water chemistry variables10.1149/1.2999351 ↗
24. Use of coupled multielectrode arrays to elucidate the pH dependence of copper pitting in potable water10.1149/1.3251288 ↗
25. Effect of chlorine concentration on natural pitting of copper as a function of water chemistry10.1149/1.3337005 ↗
26. Effects of aluminum solids on the under deposit corrosion of copper in synthetic potable water: the arguments for and against a semi-permeable membrane10.1149/2.002309jes ↗
27. King · 2002
28. In situ AFM observations of oxide film formation o n Cu(111) and Cu (100) surfaces under aqueous alkaline solutions10.1016/0039-6028(94)00671-7 ↗
29. Nano-scale oxidation of copper in aqueous solution10.1016/j.elecom.2012.09.042 ↗
30. Cathodic formation of a hydroxyde adsorbate on copper (111) electrodes in alkaline electrolyte10.1016/0022-0728(95)04297-5 ↗
31. Electrochemical STM observation of well-ordered adsorbate on Cu(111) electrode surfaces in an alkaline electrolyte10.1246/cl.1998.947 ↗
32. In situ STM study of the initial stages of oxidation of Cu(111) in aqueous solution10.1016/S0039-6028(00)00442-8 ↗
33. A new look at oxide formation at the copper/electrolyte interface by in situ spectroscopies10.1039/C5CP05172J ↗
34. Selective synthesis of clinoatacamite Cu2(OH)3Cl and tenorite CuO nanoparticles by pH control10.1007/s11051-014-2562-4 ↗
35. ASTM G5-14 · 2014
36. Calculations of the cathodic current delivery capacity and stability of crevice corrosion under atmospheric environments10.1149/1.2926557 ↗
37. Osmotic coefficients and mean activity coefficients of uni-univalent electrolytes in water at 25° C10.1063/1.3253108 ↗
38. 2017
39. Micro-Raman study of copper hydroxychlorides and other corrosion products of bronze samples mimicking archaeological coins10.1007/s00216-011-5268-9 ↗
40. ASTM G1-03 · 2011
41. Lafuente · 2015
42. Raman spectroscopy of selected copper minerals of significance in corrosion10.1016/S1386-1425(02)00315-3 ↗
43. Corrosion behaviour of copper under chloride-containing thin electrolyte layer10.1016/j.corsci.2011.06.004 ↗
44. Influence of residual stress, surface roughness and crystallographic texture induced by machining on the corrosion behaviour of copper in salt-fog atmosphere10.1016/j.corsci.2012.04.032 ↗
45. Some aspects of the atmospheric corrosion of copper in the presence of sodium chloride10.1149/1.1838422 ↗
46. Raman spectroscopy of the basic copper chloride minerals atacamite and paratacamite: implications for the study of copper, brass and bronze objects of archaeological significance10.1002/jrs.921 ↗
47. Raman investigation of artificial patinas on recent bronze – part I: climatic chamber exposure10.1002/jrs.4068 ↗
48. Goldstein · 2018
49. Formation of paratacamite nanomaterials via the conversion of aged and oxidized copper nanoparticles in hydrochloric acidic media10.1039/c0jm03705b ↗
50. Oxidation of the Cu(100) surface induced by local alkalization10.1149/1.2435701 ↗
51. The measurement and prediction of the corrosion potential of copper in chloride solutions as a function of oxygen concentration and mass-transfer coefficient10.1016/0010-938X(95)80013-1 ↗
52. Schock · 1995
53. Puigdomenech · 2000
54. Investigations of copper in aqueous alkaline solutions by cyclic voltammetry10.1016/S0022-0728(73)80344-4 ↗
55. Rotating copper disk electrode studies of the mechanism of the dissolution-passivation step on copper in alkaline solutions10.1016/S0022-0728(73)80345-6 ↗
56. Cyclic voltammetry of copper in sodium hydroxide solutions10.1016/S0022-0728(81)80091-5 ↗
57. Study of the air-formed oxide layer at the copper surface and its impact on the copper corrosion in an aggressive chloride medium10.1016/j.electacta.2017.12.187 ↗
58. A mechanism for the atmospheric corrosion of copper determined by voltammetry with a strongly alkaline electrolyte10.1149/1.3465636 ↗
59. Atacamite and paratacamite from the ultramafic-hosted Logatchev seafloor vent field (14°45′N, mid-Atlantic Ridge)