journal article·2011-07

Influence of the applied stress rate on the stress corrosion cracking of 4340 and 3.5NiCrMoV steels under conditions of cathodic hydrogen charging

S. Ramamurthy, W.M.L. Lau, A. Atrens

Corrosion Science· Volume 53· Issue 7
Publisher page

Abstract

Stress corrosion cracking (SCC) of as-quenched 4340 and 3.5NiCrMoV steels was studied under hydrogen charging conditions, with a cathodic current applied to the gauge length of specimens subjected to Linearly Increasing Stress Test (LIST) in 0.5M HSO solution containing 2g/l arsenic trioxide (AsO) at 30°C. Applied stress rates were varied from 20.8 to 6×10MPas. Both the fracture and threshold stress decreased with decreasing applied stress rate and were substantially lower than corresponding values measured in distilled water at 30°C at the open circuit potential. The threshold stress values correspond to 0.03-0.08 σ for 4340 and 0.03-0.2 σ for the 3.5NiCrMoV steel. SCC velocities, at the same applied stress rate, were an order of magnitude greater than those in distilled water. However, the plots of the crack velocity versus applied stress rate had similar slopes, suggesting the same rate-limiting step. The fracture surface morphology was mostly intergranular, with quasi-cleavage features.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Stress-corrosion cracking
2. Stress corrosion cracking in metals
3. Review of stress corrosion cracking of pipeline steels in “Low” and “High” pH solutions10.1023/A:1021126202539 ↗
4. A critical review of the stress corrosion cracking (SCC) of magnesium alloys10.1002/adem.200500071 ↗
5. R.P. Gangloff, Hydrogen assisted cracking of high strength alloys, in: I. Milne, R.O. Ritchie, B. Karihaloo (Eds.), Comprehensive Structural Integrity, J. Petit, P. Scott (vol. Eds.), vol. 6, Elsevier Science, New York, NY, 2003, pp. 31–101.10.1016/B0-08-043749-4/06134-6 ↗
6. UK experience of stress corrosion cracking in steam turbine discs
7. Design of large steam turbines for fossil and nuclear power stations10.1243/PIME_PROC_1972_186_037_02 ↗
8. Prediction of failures of low-pressure steam turbine disks10.1115/1.2842321 ↗
9. Hydrogen effects on material behaviour and corrosion deformation interactions
10. Stress corrosion cracking of high strength steels
11. Effect of threshold stress intensity on fracture mode transitions for hydrogen-assisted cracking in AISI 4340 steel10.1007/BF02647003 ↗
12. Strength effect in stress corrosion cracking of high-strength steel in aqueous solution10.5006/1.3290352 ↗
13. Characteristics of hydrogen embrittlement, stress corrosion cracking and tempered martensite embrittlement in high-strength steels10.1016/S1350-6307(01)00009-7 ↗
14. Environmental effects on the stress corrosion cracking susceptibility of 3.5NiCrMoV steels in high temperature water10.1016/j.corsci.2004.09.022 ↗
15. The effect of acetic acid on the stress corrosion cracking of 3.5NiCrMoV turbine steels in high temperature water10.1016/j.corsci.2008.04.023 ↗
16. S.P. Lynch, Progress towards Understanding Mechanisms of Hydrogen Embrittlement and Stress Corrosion Cracking, Paper 07493, Corrosion 2007, NACE Press, Houston, 2007, pp. 074931–0749355.
17. Stress corrosion cracking of carbon steels and low alloy steels10.1533/wint.2007.3718 ↗
18. SCC of commercial steels exposed to high hydrogen fugacity10.1016/j.engfailanal.2007.10.004 ↗
19. Steam turbines part 2-stress corrosion cracking of turbine disc steels10.1179/147842203770226906 ↗
20. S. Zhou, Environment Assisted Cracking of Turbine Blade Steels – A Review, NPL Report, DEPC-MPE 033, March 2007.
21. The stress corrosion cracking of as-quenched 4340 and 3.5NiCrMoV steels under stress rate control in distilled water at 90°C10.1016/0010-938X(93)90235-9 ↗
22. The influence of applied stress rate on the SCC of 4340 and 3.5 NiCrMoV steels in distilled water 30°C10.1016/j.corsci.2009.11.033 ↗
23. Linearly increasing stress test (LIST) for SCC research10.1088/0957-0233/4/11/017 ↗
24. Characterisation of stress corrosion cracking (SCC) of Mg–Al alloys10.1016/j.msea.2007.11.064 ↗
25. Comparison of the linearly increasing stress test and the constant extension rate test in the evaluation of transgranular stress corrosion cracking of magnesium10.1016/j.msea.2007.03.021 ↗
26. Analysis of service stress corrosion cracking in a natural gas transmission pipeline, active or dormant?10.1016/j.engfailanal.2003.08.001 ↗
27. SCC initiation for X65 pipeline steel in the “High” pH carbonate/bicarbonate solution10.1016/S0010-938X(03)00044-1 ↗
28. Linearly increasing stress testing of carbon steel in 4N NaNO3 and in Bayer liquor10.1023/A:1004314517742 ↗
29. Initiation of stress corrosion cracking for pipeline steels in a carbonate–bicarbonate solution10.1007/BF02652362 ↗
30. Stress corrosion crack propagation in AerMet 10010.1023/A:1004362400904 ↗
31. SCC of copper using the linearly increasing stress test10.1016/0956-716X(92)90664-Z ↗
32. R.M. Magdowski, SCC of Low Alloy Steel in Water, D. Tech. Sc. Thesis, Swiss Federal Institute of Technology, Zurich, 1987.
33. Stress corrosion cracking of steam turbine steels – an overview
34. The role of crack tip strain rate in the stress corrosion cracking of high strength steels in water10.1007/BF02651655 ↗
35. Failures of structures and components by environmentally assisted cracking10.1016/1350-6307(94)90009-4 ↗
36. Microstructure of as-quenched 3.5NiCrMoV Rotor steel: I. General structure and retained austenite10.1002/mawe.19870180508 ↗
37. The stress corrosion cracking of reactor pressure vessel steel in high temperature water10.1016/0010-938X(85)90003-4 ↗
38. Analysis of slow strain rate stress-corrosion data10.1016/0010-938X(81)90019-6 ↗
39. Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test10.1016/j.corsci.2007.03.038 ↗
40. Hydrogen-facilitated corrosion and stress corrosion cracking of austenitic stainless steel of type 31010.1007/BF02656517 ↗
41. Hydrogen-assisted cracking of T-250 maraging steel10.1016/j.msea.2005.06.080 ↗
42. Quantitative observations of hydrogen induced slow crack growth in a low alloy steel
43. Prediction of the maximum corrosion fatigue crack propagation rate in the low alloy steel-de-oxygenated water system at 288 degree C10.1016/0010-938X(85)90005-8 ↗
44. Effects of nominal, crack-tip strain rate on IGSCC susceptibility in cert tests
45. F.P. Ford, A Mechanism of Environmentally Controlled Crack-Growth of Structural Steels in High Temperature Water, General Electric Co., Report 81CRD125, Schenectady, NY, 1981.
46. Prediction of environmental and strain-rate effects on the stress corrosion cracking of austenitic stainless steels10.1115/1.3264843 ↗
47. Estimation of crack tip strain rate parameters characterising environment assisted crack growth data
48. Effect of strain rate on stress corrosion crack velocity: difference between intergranular and transgranular cracking10.1016/S0010-938X(98)00118-8 ↗
49. Corrosion in power generating equipment
50. Clean steels for steam turbine rotors-their stress corrosion cracking resistance10.1007/BF02674033 ↗
51. The interaction of strain-rate and repassivation rate in stress corrosion crack propagation10.1016/0010-938X(80)90080-3 ↗
52. The stress corrosion of steel in sodium hydroxide solution: a film-rupture model10.1016/0010-938X(81)90078-0 ↗
53. A film rupture model for stress corrosion crack propagation
54. Corrosion in nuclear systems: environmentally assist cracking in light water reactors
55. Unified interpretation of crack growth rates of Ni-base alloys in LWR environments10.1115/1.2217964 ↗
56. The influence of strain on hydrogen entry and transport in a high strength steel in sodium chloride solution10.1149/1.2095978 ↗
57. Conceptual model of stress corrosion cracking of low-alloy steels in high-temperature water
58. ESEM observations of SCC Initiation for 4340 high strength steel in distilled water10.1023/A:1004328031430 ↗