Improvement of oxidation resistance of 9 mass% chromium steel for advanced-ultra supercritical power plant boilers by pre-oxidation treatment
Source abstract
Abstract
Abstract Effect of pre-oxidation treatment on oxidation resistance in steam at 650 °C has been investigated for 9 mass% chromium (Cr) steel for advanced ultra-supercritical power plants. The formation of thin scale of Cr 2 O 3 -rich oxides is achieved by pre-oxidation in argon gas containing 0.3 ppm oxygen, which significantly improves the oxidation resistance of the steel in steam at 650 °C for a long time exceeding 20,000 h. Effects of pre-oxidation conditions, such as oxygen concentration in argon gas and pre-oxidation temperature and time, and of silicon concentration in the steel on the oxidation resistance in stream are systematically investigated.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Blum · 2003 · 498
2. The European way to 700°C coal fired power plant
3. W
4. Di Gianfrancesco · 2013 · 19
5. Viswanathan · 2005 · 3
6. Shingledecker · 2013 · 41
7. Fukuda · 2013 · 24
8. Sun · 2013 · 1
9. Mathur · 2013 · 53
10. Abe · Sci. Technol. Adv. Mater · 2008 · 9 · 01300210.1088/1468-6996/9/1/013002 ↗
11. Structural Alloys in Power Plants
12. Kofstad · 1966 · 264
13. Wallwork · Rep. Prog. Phys. · 1976 · 39 · 40110.1088/0034-4885/39/5/001 ↗
14. Viswanathan · J. Mater. Eng. Perform. · 2006 · 15 · 25510.1361/105994906X108756 ↗
15. Mito · 2013 · 627
16. Wang · Corros. Sci. · 2016 · 111 · 1310.1016/j.corsci.2016.04.020 ↗
17. Guo · Corros. Sci. · 2015 · 100 · 57910.1016/j.corsci.2015.08.034 ↗
18. Tang · Corros. Sci. · 2014 · 80 · 37410.1016/j.corsci.2013.11.054 ↗
19. Liu · Corros. Sci. · 2015 · 91 · 19510.1016/j.corsci.2014.11.020 ↗
20. Cheng · Corros. Sci. · 2016 · 108 · 1110.1016/j.corsci.2016.02.042 ↗
21. Nishimura · Mater. High Temp. · 2005 · 22 · 110.3184/096034005782750554 ↗
22. Sabau · 2010 · 213
23. Itagaki · Corrosion · 2005 · 61 · 30710.5006/1.3279882 ↗
24. Kutsumi · 2002 · 1629
25. Kutsumi · 2004 · 463
26. Abe · 2012
27. Haruyama · 2004 · 412
28. Sundararajan · ISIJ Int. · 2003 · 43 · 9510.2355/isijinternational.43.95 ↗
29. Sundararajan · ISIJ Int. · 2003 · 43 · 10410.2355/isijinternational.43.104 ↗
30. Sundararajan · ISIJ Int. · 2004 · 44 · 13910.2355/isijinternational.44.139 ↗
31. Sundararajan · Materi. Trans. · 2004 · 45 · 129910.2320/matertrans.45.1299 ↗
32. Sundararajan · Metall. Mater. Trans. · 2004 · 35A · 318710.1007/s11661-004-0063-2 ↗
33. Sundararajan · Corros. Sci. · 2005 · 47 · 112910.1016/j.corsci.2004.06.023 ↗
34. Sundararajan · Surf. Coat. Technol. · 2005 · 194 · 29010.1016/j.surfcoat.2004.05.033 ↗
35. Lowell · Oxid. Met. · 1973 · 7 · 9510.1007/BF00611450 ↗
36. Sarver · 2004 · 1326
37. Moreau · J. Inst. Metals · 1954 · 83 · 87
38. Abendroth · Trans. AIME · 1964 · 230 · 1735