Effect of hydrogen and inclusions on the tensile properties and fracture behaviour of A350LF2 steels after exposure to wet H2S environments
Source abstract
Abstract
Abstract The tensile properties and fracture behaviour of A350LF2 steels after exposure to wet H 2 S environments were investigated by corrosion and tensile testing. The results suggest that relative tensile strength and plasticity loss increased as hydrogen concentration increased. Greater tensile property damage occurred in steel that contained more large-size inclusions. When hydrogen was released, the degree of relative strength and plasticity loss decreased. Fractography of the corroded samples exhibited mixed ductile–brittle rupture. Fractured areas with quasi-cleavage features increased with increasing hydrogen concentration. Flakes appeared in the steel with a low sulphur content and low hydrogen concentration.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Conditions of hydrogen-induced corrosion occurrence of X65 grade line pipe steels in sour environments10.5006/1.3299225 ↗
2. S.N. Smith, M.W. Joosten, Corrosion of carbon steel by H2S in CO2 containing oilfield environments, NACE Corrosion/2006, San Diego, CA, 12–16 March 2006, paper 06115.
3. Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of line pipe steel10.1016/j.corsci.2008.03.007 ↗
4. Sensitivity of pipelines with steel API X52 to hydrogen embrittlement10.1016/j.ijhydene.2008.09.020 ↗
5. Effect of CO2 and R-ratio on near-neutral pH stress corrosion cracking initiation under a disbonded coating of pipeline steel10.1016/j.corsci.2011.03.017 ↗
6. Chu · 1988
7. Hydrogen electrode reaction and hydrogen embrittlement of mild steel in hydrogen sulfide solutions10.5006/0010-9312-32.8.321 ↗
8. Hydrogen-induced crack growth rate in steel plates exposed to sour environments10.5006/1.3290278 ↗
9. The role of hydrogen and other interstitials in the mechanical behaviour of metals
10. Whitney award lecture – 1987: hydrogen-the versatile embrittler10.5006/1.3583875 ↗
11. Roles of micro-alloying elements in hydrogen induced cracking resistant property of HSLA steels10.5006/1.3316066 ↗
12. Evaluation of susceptibility of high strength steels to delayed fracture by using cyclic corrosion test and slow strain rate test10.1016/j.corsci.2010.02.005 ↗
13. Effects of hydrogen-charging on the susceptibility of X100 pipeline steel to hydrogen-induced cracking10.1016/j.ijhydene.2009.09.090 ↗
14. Hydrogen induced shear localisation of the plastic flow in metals and alloys10.1016/S0997-7538(01)01179-2 ↗
15. Hydrogen induced plasticity in stress corrosion cracking of engineering systems10.1016/S0013-7944(00)00121-1 ↗
16. Influence of sandblasting and hydrogen on tensile and fatigue properties of pipeline API 5L X52 steel10.1016/j.ijhydene.2010.11.081 ↗
17. Characterization of inclusions in clean steels: a review including the statistics of extremes methods10.1016/S0079-6425(02)00014-2 ↗
18. Ciszewski · 1977
19. Effect of non-metallic inclusions on hydrogen-induced cracking of API5L X100 steel10.1016/j.ijhydene.2010.05.089 ↗
20. Characterization of inclusions of X80 pipeline steel and its correlation with hydrogen-induced cracking10.1016/j.corsci.2010.12.011 ↗
21. Effect of environmental and metallurgical factors on hydrogen induced cracking of HSLA steels10.1016/j.corsci.2008.09.030 ↗
22. Influence of sulphur content and inclusion distribution on the hydrogen induced blister cracking in pressure vessel and pipeline steels10.1016/S0010-938X(00)00084-6 ↗
23. Some observations on the role of inclusions in the hydrogen induced blister cracking of linepipe steels in sulfide environments10.5006/0010-9312-36.11.625 ↗
24. NACE standard TM0284-2003. Evaluation of pipeline and pressure vessel steels for resistance to hydrogen-induced cracking, NACE International, Houston, Texas, 2003.
25. JIS, Method for Measurement of Hydrogen Evolved from Deposited Metal, Japan, 1975.
26. Hydrogen damage and delayed fracture in bulk metallic glass10.1016/j.corsci.2004.07.045 ↗
27. Effect of heat treatment on H2S corrosion of a micro-alloyed C–Mn steel10.1016/j.corsci.2009.06.022 ↗
28. Mechanics and thermodynamics on the stress and hydrogen interaction in crack tip stress corrosion: experiment and theory10.1016/S0022-5096(97)00054-9 ↗
29. Mechanism of hydrogen induced softening10.1016/0036-9748(86)90131-6 ↗
30. Micro-electrochemical characterization of corrosion of welded X70 pipeline steel in near-neutral pH solution10.1016/j.corsci.2009.04.030 ↗
31. Hydrogen effect on fracture toughness of pipeline steel welds, with in situ hydrogen charging10.1016/j.ijhydene.2011.06.140 ↗
32. Dubovoy · 1950
33. The removal of hydrogen from steel
34. Hydrogen and transformation characteristics in steel
35. G.M. Pressourye, Current Solution to Problems in Steels, ASM, Metals Park, OH, 1982.
36. Flake and sulphide inclusions in low carbon steel