Early corrosion behaviour of irradiated FeCrAl alloy in a simulated pressurized water reactor environment
Source abstract
Abstract
Abstract The early corrosion behaviour of an irradiated FeCrAl alloy in a simulated pressurized water reactor environment was investigated. The irradiated alloy showed a Cr-rich oxide layer, which was not observed in the as-received alloy. The corrosion induced the formation of a duplex-layer oxide structure consisting of an outer hematite α-Fe2O3 layer and an inner spinel Cr-rich oxide layer. In the initial corrosion stage, the smooth surface formed by ion sputtering and the formation of the Cr-rich oxide layer suppressed the corrosion. However, in the later corrosion stage, the irradiated alloys exhibited severe corrosion because of the presence of irradiation-induced defects.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Development of low-Cr ODS FeCrAl alloys for accident-tolerant fuel cladding10.1016/j.jnucmat.2017.12.035 ↗
2. Growth of oxide particles in FeCrAl- oxide dispersion strengthened steels at high temperature10.1016/j.jnucmat.2017.06.018 ↗
3. A study of the oxidation of FeCrAl alloy in pressurized water and high-temperature steam environment10.1016/j.corsci.2015.02.027 ↗
4. Influence of irradiation on the oxide film formed on 316 l stainless steel in PWR primary water10.1007/s11085-013-9401-3 ↗
5. Effect of irradiation on corrosion of 304 nuclear grade stainless steel in simulated PWR primary water10.1016/j.corsci.2017.08.010 ↗
6. Uniform corrosion of FeCrAl alloys in LWR coolant environments10.1016/j.jnucmat.2016.06.047 ↗
7. Effects of chromium on the oxidation performance of β-FeAlCr coatings10.1023/A:1004669126961 ↗
8. Influence of preoxidation on high-temperature corrosion of a FeCrAl alloy under conditions relevant to biomass firing
9. Growth rates of alumina scales on Fe–Cr–Al alloys10.1023/B:OXID.0000016274.78642.ae ↗
10. Oxidation kinetics of Y-doped FeCrAl-alloys in low and high pO2 gases10.1002/maco.200905432 ↗
11. Effect of the θ-α-Al2O3 transformation on the oxidation behavior of β-NiAl+Zr10.1007/BF00846690 ↗
12. Effect of electropolishing on corrosion of nuclear grade 316L stainless steel in deaerated high temperature water10.1016/j.corsci.2016.09.002 ↗
13. Effect of dissolved hydrogen on corrosion of 316NG stainless steel in high temperature water10.1016/j.nucengdes.2015.08.030 ↗
14. Composition, structure and properties of the oxide films formed on the stainless steel 316L in a primary type PWR environment10.1016/S0010-938X(97)00158-3 ↗
15. The mechanism and kinetics of corrosion product release from stainless steel in lithiated high temperature water10.1016/0010-938X(87)90068-0 ↗
16. The mechanism of oxide film formation on austenitic stainless steels in high temperature water10.1016/S0010-938X(97)00140-6 ↗
17. Electropolishing effects on corrosion behavior of 304 stainless steel in high temperature, hydrogenated water10.1016/j.corsci.2008.06.032 ↗
18. Corrosion behavior of stainless steels in simulated PWR primary water-effects of chromium content in alloys and dissolved hydrogen10.1080/18811248.2008.9711883 ↗
19. Influence of dissolved oxygen concentration on the oxide film formed on 304 stainless steel in high temperature water10.1016/j.corsci.2012.06.007 ↗
20. Characterization of the oxide film formed on type 316 stainless steel in 288 C water in cyclic normal and hydrogen water chemistries10.5006/1.3293562 ↗
21. Analysis of oxide film formed on type 304 stainless steel in 288 C water containing oxygen, hydrogen, and hydrogen peroxide10.5006/1.3283969 ↗
22. Effects of hydrogen peroxide on corrosion of stainless steel, (V) characterization of oxide film with multilateral surface analyses10.1080/18811248.2006.9711173 ↗
23. Influence of oxygen concentration of 288 C water and alloy composition on the films formed on Fe–Ni–Cr alloys10.5006/1.3278328 ↗
24. Radiation hardening and IASCC susceptibility of extra high purity austenitic stainless steel10.1016/j.jnucmat.2010.12.154 ↗
25. Role of radiation-induced grain boundary segregation in irradiation assisted stress corrosion cracking10.1080/18811248.2004.9715522 ↗
26. Oxidation kinetics and mechanisms of Ni-base alloys in pressurised water reactor primary conditions: influence of subsurface defects
27. Oxidation of Zircaloy-4 during in situ proton irradiation and corrosion in PWR primary water10.1557/jmr.2014.408 ↗
28. Oxidation of a proton-irradiated 316 stainless steel in simulated BER NWC environment
29. Light ion irradiation-induced phase transformation in the monoclinic polymorph of zirconia10.1016/j.jnucmat.2008.07.045 ↗
30. The mechanism of high temperature aqueous corrosion of steel10.1016/0010-938X(89)90120-0 ↗
31. Electropolishing effects on corrosion behavior of 304 stainless steel in high temperature10.1016/j.corsci.2008.06.032 ↗
32. Effect of surface preparation on the corrosion of austenitic stainless steel 304L in high temperature steam and simulated PWR primary water10.1016/j.corsci.2011.12.007 ↗
33. Effect of surface roughness on the development of protective Al2O3 on Fe–10Al (at.%) alloys containing 0–10 at.% Cr10.1016/j.apsusc.2006.01.027 ↗
34. Development and property evaluation of nuclear grade wrought FeCrAl fuel cladding for light water reactors10.1016/j.jnucmat.2015.10.019 ↗
35. Development and property evaluation of nuclear grade wrought FeCrAl fuel cladding for light water reactors10.1016/j.scriptamat.2010.08.015 ↗
36. Microstructural stability of Fe-Cr-Al alloys at 450-550 C10.1016/j.jnucmat.2014.11.101 ↗
37. The effect of Al on the 475 C embrittlement of Fe-Cr alloys10.1016/j.commatsci.2013.03.021 ↗
38. The adsorption of oxygen on the Fe(1 0 0) surface10.1016/0039-6028(89)90265-3 ↗
39. Influence of dissolved oxygen on oxide films of alloy 690TT with different surface status in simulated primary water10.1016/j.corsci.2011.07.012 ↗
40. On the mechanism of radiation-induced segregation in austenitic Fe-Cr-Ni alloys10.1016/S0022-3115(98)00010-5 ↗
41. Theory of steady-state passive films10.1149/1.2086949 ↗
42. Sintering and reactive sintering by spark plasma sintering(SPS)[M]
43. Theoretical and experimental investigation of the thermochemistry of CrO2(OH)2(g)10.1021/jp0647380 ↗
44. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
45. Design requirements for plasma facing materials in ITER10.1016/S0022-3115(96)00317-0 ↗