Synthesis of nanoporous Cu films by dealloying of electrochemically deposited Cu–Zn alloy films
Source abstract
Abstract
Abstract Crack-free nanoporous Cu films were synthesized by electrochemical deposition of Cu–Zn alloy films by chronoamperometry (CA) at −0.5 V(Ag/AgCl), followed by a two-step chemical dealloying process. Various nanoporous structures were successfully created with very low concentration of less-noble element (3–4 at.% Zn), by a wet-chemical process. In addition to the Zn, less noble constituent, it is believed that Cu oxide formed during the electrochemical deposition might act as less-noble constituent as well.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nanoporous metals and alloys · Electrocatalysts for Energy Conversion · Anodic Oxide Films and Nanostructures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Evolution of nanoporosity in dealloying10.1038/35068529 ↗
2. Nanoporous metals with controlled multimodal pore size distribution10.1021/ja035318g ↗
3. Ashby · 2000
4. Zur Theorie der Resistenzgrenzen in Mischkristallen10.1002/zaac.19211180127 ↗
5. Pre-Columbian surface metallurgy10.1038/scientificamerican0684-56 ↗
6. Anion effects in the stress-corrosion cracking of copper and brass10.1149/1.2129510 ↗
7. Characteristic features of alloy polarization curves10.1016/0010-938X(83)90092-6 ↗
8. Passivity breakdown and pitting corrosion of binary alloys10.1038/350216a0 ↗
9. Metallic corrosion10.1126/science.263.5154.1708 ↗
10. Ductile–brittle transition in random porous Au10.1103/PhysRevLett.68.1168 ↗
11. Microfabrication and mechanical properties of nanoporous gold at the nanoscale10.1016/j.scriptamat.2006.08.069 ↗
12. Volume change during the formation of nanoporous gold by dealloying10.1103/PhysRevLett.97.035504 ↗
13. A multi-step dealloying method to produce nanoporous gold with no volume change and minimal cracking10.1016/j.scriptamat.2007.12.008 ↗
14. Microstructure, stability and thermomechanical behavior of crack-free thin films of nanoporous gold10.1016/j.scriptamat.2008.01.036 ↗
15. Fabrication of nanoporous gold thin films on silicon substrate by multilayer deposition of Au and Ag10.1016/j.jallcom.2009.05.067 ↗
16. Fabrication of crack-free nanoporous gold blanket thin films by potentiostatic dealloying10.1016/j.scriptamat.2010.07.025 ↗
17. Fabrication of crack-free blanket nanoporous gold thin films by galvanostatic dealloying10.1016/j.jallcom.2011.02.115 ↗
18. Nanoporous Ag prepared from the melt-spun Cu–Ag alloys10.1016/j.solidstatesciences.2011.04.007 ↗
19. Formation and characterization of monolithic nanoporous copper by chemical dealloying of Al−Cu Alloys10.1021/jp810742z ↗
20. Fabrication and characterization of monolithic nanoporous copper through chemical dealloying of Mg–Cu alloys10.1016/j.corsci.2009.05.043 ↗
21. Monolithic nanoporous copper by dealloying Mn–Cu10.1557/jmr.2006.0322 ↗
22. Synthesis of porous copper from nanocrystalline two-phase Cu–Zr film by dealloying10.1016/j.scriptamat.2006.09.009 ↗
23. Morphology, oxidation, and mechanical behavior of nanoporous Cu foams10.1002/adem.201100252 ↗
24. Fabrication of nanoporous copper film for electrochemical detection of glucose10.1002/elan.200904697 ↗
25. Electrochemical preparation of porous copper surfaces in zinc chloride-1-ethyl-3-methyl imidazolium chloride ionic liquid10.1149/1.2724154 ↗
26. Joseph R. Davis (Ed.), Copper and copper alloys, Handbook.
27. Fontana · 1978
28. Bard · 1985
29. Sawyer · 1995
30. Deborah · 2010
31. On the role of buffers and anions in NiFe electrodeposition10.1149/1.2128816 ↗
32. Morphology and composition of electrodeposited cobalt–zinc alloys and the influence of boric acid10.1149/1.2096991 ↗
33. Effects of boric acid on the electrodeposition of iron, nickel and iron–nickel10.1016/0257-8972(94)02410-3 ↗
34. Pattern formation during dealloying10.1016/S1359-6462(03)00471-8 ↗
35. An atomistic description of dealloying: porosity evolution, the critical potential, and rate-limiting behavior10.1149/1.1784820 ↗