Abstract

Abstract The inhibition effect of cerium salts on iron/aluminum galvanic coupling was investigated by electrochemical microcell and Scanning Vibrating Electrochemical Technique (SVET). The importance of the electrode geometry on the SVET responses was evidenced. The effect of concentration and the influence of the anionic part of cerium salts on the inhibitive efficiencies and protective mechanisms were studied. Cerium salts inhibit the corrosion of iron/aluminum galvanic coupling by reducing the cathodic activity. Microcell analysis confirmed the passivation of aluminum. (SEM + EDS) analyses allowed to understand how the cerium salts act to improve the corrosion behavior.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (65)

Show source-provided references
1. Effective corrosion inhibition performance of Ce3+ doped sol–gel nanocomposite coating on aluminum alloy10.1016/j.porgcoat.2012.10.004 ↗
2. Long-term atmospheric corrosion behaviour of aluminium alloys 2024 and 7075 in urban, coastal and industrial environments10.1016/j.corsci.2009.01.016 ↗
3. Experimental and computational evaluation of the protection provided by an aluminum cladding to AA2024-T3 exposed at a seacoast environment10.5006/1.3278271 ↗
4. The effect of nickel on alloy microstructure and electrochemical behaviour of AA1050 aluminium alloy in acid and alkaline solutions10.1016/j.electacta.2012.04.106 ↗
5. The mechanism of electrograining aluminium sheet in nitric/boric acid electrolyte10.1016/S0010-938X(98)00101-2 ↗
6. Investigation of the initial stage of crevice corrosion on Al99.5 by electrochemical noise analysis10.1002/maco.200704092 ↗
7. Electrochemical characteristics of intermetallics phases in aluminium alloys. experimental survey and discussion10.1149/1.1869984 ↗
8. Localized corrosion inhibition by cerium species on clad AA2024 aluminium alloy investigated by means of electrochemical micro-cell10.1016/j.corsci.2012.08.053 ↗
9. Mechanism of corrosion inhibition of AA2024 by rare earth compounds10.1021/jp0560664 ↗
10. Influence of inhibitor addition on the corrosion protection performance of sol–gel coatings on AA202410.1016/j.porgcoat.2007.12.002 ↗
11. The corrosion resistance of hot dip galvanised steel and AA2024-T3 pre-treated with bis-[triethoxysilylpropyl]tetrasulfide solutions doped with Ce(NO3)310.1016/j.corsci.2006.01.010 ↗
12. An electrochemical and superficial assessment of the corrosion behavior of AA2024-T3 treated with metacryloxypropylmethoxysilane and cerium nitrate10.1016/j.surfcoat.2008.06.173 ↗
13. XANES investigation of the role of cerium compounds as corrosion inhibitors for aluminum10.1016/0010-938X(91)90113-4 ↗
14. The influence of pH on corrosion inhibitor selection for 2024-T3 aluminium alloy assessed by high-throughput multielectrode and potentiodynamic testing10.1016/j.electacta.2009.12.013 ↗
15. Electrochemical techniques for practical evaluation of corrosion inhibitor effectiveness. Performance of cerium nitrate as corrosion inhibitor for AA2024-T3 alloy10.1016/j.corsci.2010.06.012 ↗
16. A combinatorial matrix of rare earth chloride mixtures as corrosion inhibitors of AA2024-T3: optimisation using potentiodynamic polarisation and EIS10.1016/j.electacta.2012.02.004 ↗
17. Lanthanide salts as corrosion inhibitors for AA5083. corrosion inhibition10.1149/1.2844341 ↗
18. Cerium molybdate nanowires for active corrosion protection of aluminium alloys10.1016/j.corsci.2012.01.012 ↗
19. Investigation of AA2024-T3 surfaces modified by cerium compounds: a localized approach10.1016/j.corsci.2013.10.001 ↗
20. The use of cerium and praseodymium mercaptoacetate as thiol-containing inhibitors for AA2024-T310.1016/j.corsci.2013.12.001 ↗
21. Localized electrochemical study of corrosion inhibition in microdefects on coated AZ31 magnesium alloy10.1016/j.electacta.2010.04.064 ↗
22. Photoelectrochemical investigation of corrosion using scanning electrochemical techniques10.1016/S0013-4686(99)00442-9 ↗
23. Inhibition of magnesium localised corrosion in chloride containing electrolyte10.1016/j.electacta.2010.03.023 ↗
24. The investigation of cerium as a cathodic inhibitor for aluminium–copper alloys10.1149/1.2049985 ↗
25. Localized electrochemical methods applied to cut edge corrosion10.1149/1.1393954 ↗
26. Cathodic electrodeposition of cerium-based oxides on carbon steel from concentrated cerium nitrate solutions Part I. Electrochemical and analytical characterisation10.1016/j.matchemphys.2008.08.027 ↗
27. Comparaison between the inhibition efficiencies of Ce(III) and Ce(IV) ammonium nitrates against corrosion of AA2024 aluminium alloy in solutions of low chloride concentration10.1016/j.corsci.2012.03.039 ↗
28. Effect of the anionic part of various Ce(III) salts on the corrosion inhibition efficiency of AA2024 aluminium alloy10.1016/j.corsci.2013.01.008 ↗
29. Corrosion inhibition of aluminium by rare earth chlorides10.1016/j.matchemphys.2007.02.079 ↗
30. Lanthanide compounds as environmentally-friendly corrosion inhibitors of aluminium alloys: a review10.1016/S0010-938X(98)00077-8 ↗
31. Concerning the efficiency of corrosion inhibitors as given by SVET10.4152/pea.200801047 ↗
32. The effect of height on the current distribution measured with a vibrating electrode probe10.1149/1.2085665 ↗
33. Solution conductivity influence on pitting corrosion studies by SVET10.1016/S1452-3981(23)18214-9 ↗
34. Electric field analysis in a dilute solution for the vibrating electrode technique10.1016/S0022-0728(02)01268-8 ↗
35. Effect of probe tip inclination on the response of the scanning vibrating electrode technique to an idealised pit-like feature10.1016/j.electacta.2012.01.062 ↗
36. Scanning vibrating reference electrode technique: a calibration study to evaluate the optimum operating parameters for maximum signal detection of point source activity10.1016/j.electacta.2004.01.069 ↗
37. Artifacts induced by large amplitude probe vibrations in localized corrosion measured by svet10.1149/1.1623494 ↗
38. Microelectrochemical studies of pit initiation at single inclusions in Al2024-T310.1149/1.1344530 ↗
39. Electrochemical characterisation of aluminium AA7075-T6 and solution heat treated AA7075 using a micro-capillary cell10.1016/S0013-4686(03)00379-7 ↗
40. Corrosion behaviour of different tempers of AA7075 aluminium alloy10.1016/j.electacta.2004.01.046 ↗
41. Investigation and discussion of characteristics for intermetallic phases common to aluminum alloys as a function of solution pH10.1149/1.2829897 ↗
42. The influence of MgSi particle reactivity and dissolution processes on corrosion in Al–Mg–Si alloys10.1016/j.electacta.2008.05.078 ↗
43. Electrochemical evaluation of constituent intermetallics in aluminium alloy 2024-T3 exposed to aqueous vanadate inhibitors10.1149/1.3076147 ↗
44. Inhibition of AA2024-T3 on a phase-by-phase basis using an environmentally benign inhibitor, cerium dibutyl phosphate10.1149/1.2073672 ↗
45. Study of the effect of cerium nitrate on AA2024-T3 by means of electrochemical micro-cell technique10.1016/j.electacta.2012.02.099 ↗
46. Galvanic corrosion between zinc and carbon steel investigated by local electrochemical impedance spectroscopy10.1016/j.electacta.2012.10.002 ↗
47. Localized approach to galvanic coupling in an aluminium–magnesium system10.1149/1.3148833 ↗
48. Galvanic coupling between pure copper and pure aluminium: experimental approach and mathematical model10.1149/1.2803506 ↗
49. Influence of oxidizing ability of the medium on the growth of lanthanide layers on galvanized steel10.1016/j.corsci.2010.01.011 ↗
50. SVET, AFM and AES study of pitting corrosion initiated on MnS inclusions by microinjection10.1016/S0010-938X(02)00222-6 ↗
51. Reliability of numerical models for simulating galvanic corrosion processes10.1016/j.electacta.2012.04.068 ↗
52. Investigations of self-healing mechanism on galvanized steels cut edges by coupling SVET and numerical modeling10.1016/j.electacta.2008.02.066 ↗
53. SVET method for characterizing anti-corrosion performance of metal-rich coatings10.1016/j.corsci.2010.04.012 ↗
54. Effect of aluminium spacer on galvanic corrosion between magnesium and mild steel using numerical model and SVET experiments10.1016/j.corsci.2012.05.013 ↗
55. Experimental investigation of galvanic corrosion: comparison between SVET and immersion techniques10.1016/j.corsci.2010.04.023 ↗
56. Influence of edge effects on local corrosion rate of magnesium alloy/mild steel galvanic couple10.1021/ac3022955 ↗
57. Quantitative analysis of scanning electric current density and pH-value observations in corrosion studies
58. Investigating corrosion processes in the micrometric range: a SVET study of the galvanic corrosion of zinc coupled with iron10.1016/j.corsci.2007.04.016 ↗
59. Cut-edge corrosion study on painted aluminum rich metallic coated steel by scanning vibrating electrode and micro-potentiometric techniques10.1016/j.electacta.2011.11.110 ↗
60. Localized corrosion of magnesium in chloride-containing electrolyte studied by a scanning vibrating electrode technique10.1149/1.2918900 ↗
61. The localised corrosion of Mg alloy AZ31 in chloride containing electrolyte studied by a scanning vibrating electrode technique10.1016/j.electacta.2013.07.134 ↗
62. The corrosion inhibition of zinc with cerous chloride10.1016/0010-938X(89)90087-5 ↗
63. Protection against corrosion in marine environments of AA6060 aluminium alloy bt cerium chlorides10.1016/j.jallcom.2009.11.042 ↗
64. Corrosion protection of AA2024-T3 using rare earth diphenylphosphates10.1016/j.electacta.2006.11.028 ↗
65. Cerium dibutylphosphate as a corrosion inhibitor for AA2024-T3 aluminium alloys10.1149/1.2217260 ↗