Thermogravimetric studies of high temperature reactions between potassium salts and chromium
Source abstract
Abstract
Abstract This study compares the high temperature reactions of potassium chloride (KCl) and potassium carbonate (K 2 CO 3 ), two salts found in fly ashes formed in biomass combustion, with both pure metallic chromium (Cr) and chromium oxide (Cr 2 O 3 ). The reactions were investigated with thermogravimetric measurements and the results discussed based on thermodynamic calculations. In simple terms: potassium chloride reacted with chromium forming potassium chromate (K 2 CrO 4 ) and chromium oxide. Potassium chloride did not react with chromium oxide. Potassium carbonate reacted with chromium oxide, but not with chromium. The presence of potassium is sufficient to initiate accelerated oxidation, but chloride is needed to sustain it.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Thermal and Kinetic Analysis · Iron and Steelmaking Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. The effects of chlorides, hydrogen chloride and sulfur dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
2. Corrosion behavior of 12CrMoV steel in waste incineration environments: Hot corrosion by molten chlorides10.1023/A:1018851029023 ↗
3. High temperature corrosion mechanisms and effect of alloying elements for materials used in waste incineration environment10.1016/S0010-938X(01)00058-0 ↗
4. Deposition of potassium salts on heat transfer surfaces in straw-fired boilers: A pilot-scale study10.1016/S0016-2361(99)00090-3 ↗
5. Utilizing biomass and waste for power production – A decade of contributing to the understanding, interpretation and analysis of deposits and corrosion products10.1016/j.fuel.2004.08.026 ↗
6. High temperature corrosion of superheater materials below deposited biomass ashes in biomass combusting atmospheres10.1179/174327807X159989 ↗
7. Corrosion of superheater steel materials under alkali salt deposits, Part 1: the effect of salt deposit composition and temperature10.1016/j.corsci.2008.01.010 ↗
8. Alkali induced corrosion of 304-type austenitic stainless steel at 600°C; Comparison between KCl, K2CO3 and K2SO410.4028/www.scientific.net/MSF.595-598.367 ↗
9. A thermodynamic study of the gaseous potassium chemistry in the convection sections of biomass fired boilers10.1002/maco.201005880 ↗
10. J. Lehmusto, B.-J. Skrifvars, P. Yrjas, M. Hupa, Comparison of potassium chloride and potassium carbonate with respect to their tendency to cause high temperature corrosion of stainless 304L steel, Fuel Process. Technol., doi:10.1016/j.fuproc.2011.12.016.10.1016/j.fuproc.2011.12.016 ↗
11. Accelerated oxidation rate of chromium induced by sodium chloride10.1007/BF00659274 ↗
12. Corrosion behavior of pure Cr with a solid NaCl deposit in O2 plus water vapor10.1023/A:1004690518225 ↗
13. High temperature interaction of pure Cr with KCl10.4028/www.scientific.net/MSF.461-464.1047 ↗
14. Local reactions of KCl particles with iron, nickel and chromium surfaces10.1002/maco.200503903 ↗
15. Salt melt induced corrosion of metallic materials in waste incineration plants10.1002/(SICI)1521-4176(199907)50:7<373::AID-MACO373>3.0.CO;2-T ↗
16. KCl induced corrosion of a 304-type austenitic stainless steel at 600°C; the role of potassium10.1007/s11085-005-5704-3 ↗
17. Fact sage thermochemical software and databases – recent developments10.1016/j.calphad.2008.09.009 ↗
18. High temperature corrosion of Cr with the presence of molten carbonate10.5796/kogyobutsurikagaku.64.464 ↗
19. Corrosion behavior of chromium in molten carbonate10.1149/1.1836388 ↗
20. The corrosion behaviour of iron and chromium in molten (Li0.62 K0.38)2CO310.1016/S0013-4686(97)10191-8 ↗
21. Tz. Tzvetkoff, J. Kolchakov, Mechanism of growth, composition and structure of oxide films formed on ferrous alloys in molten salt electrolytes – a review, Mater. Chem. Phys. 87 (2004) 201–211.10.1016/j.matchemphys.2004.05.039 ↗
22. Corrosion phenomena of alloys and electrode materials in molten carbonate fuel cells10.1002/(SICI)1521-4176(200005)51:5<287::AID-MACO287>3.0.CO;2-8 ↗
23. Hot corrosion of nickel and nickel-chromium alloys in molten carbonate mixtures
24. J. Lehmusto, D. Lindberg, P. Yrjas, B.-J. Skrifvars, M. Hupa, Studies on the partial reactions between potassium chloride and metallic chromium concerning corrosion at elevated temperatures, Oxid. Met., DOI 10.1007/s11085-011-9277-z.
25. Thermodynamic evaluation and optimization of the (Na2CO3+Na2SO4+Na2S+K2CO3+K2SO4+K2S) system10.1016/j.jct.2006.11.002 ↗
26. Thermodynamic evaluation and optimization of the (NaCl+Na2SO4+Na2CO3+KCl+K2SO4+K2CO3) system10.1016/j.jct.2006.12.018 ↗
27. S.D. Gromakov, Some rules pertaining to the determination of the type of phase diagrams of binary systems, Zh. Fiz. Khim+. 25 (1951) 1014–1025.
28. A.T. Dinsdale, CALPHAD: Comput. Coupling Phase Diagrams Thermochem. 15 (1991) 317–425.10.1016/0364-5916(91)90030-N ↗
29. Degterov · J. Phase Equilib. · 1996 · 17 · 47610.1007/BF02665994 ↗
30. I. Barin, O. Knacke, O. Kubaschewski, Thermochemical Properties of Inorganic Substances, Suppl., 1977.10.1007/978-3-662-02293-1 ↗
31. Nolte · Allg. Chem. · 1969 · 371 · 14910.1002/zaac.19693710306 ↗
32. http://www.hsc-chemistry.com/
33. D.D. Wagman, W.H. Evans, V.B. Parker, R.H. Schumm, I. Halow, S.M. Bailey, K.L. Churney, R.L. Nuttall, Journal of Physical and Chemical Reference Data, Vol. 11, Suppl. No. 2: The NBS Tables of Chemical Thermodynamic Properties. Selected Values for Inorganic and C1 and C2 Organic Substances in SI Units, Am. Inst. Phys., 1982.
34. M.W. Chase, Jr., (Ed.), NIST-JANAF Thermochemical Tables, Monograph No. 9, Parts I and II, American Chemical Society & American Institute of Physics, Woodbury, New York, USA, 1998.
35. Dessureault · J. Electrochem. Soc. · 1990 · 137 · 294110.1149/1.2087103 ↗
36. N. Saunders, A.P. Miodownik, CALPHAD (Calculation of Phase Diagrams): A Comprehensive Guide, Pergamon Materials Series in: R.W. Cahn, (Ed.), Vol. 1, Elsevier, Oxford, 1998, pp. 261–296.
37. The modified quasi-chemical model: part IV. two-sublattice quadruplet approximation10.1007/s11661-001-0230-7 ↗
38. Towards a comprehensive thermodynamic database for ash-forming elements in biomass and waste combustion – Current situation and future developments
39. An isotropic conductivity and phase transformation studies in potassium chromate crystals10.1139/v74-354 ↗
40. KCl-induced high temperature corrosion of the austenitic Fe–Cr–Ni alloys 304L and Sanicro 28 at 600°C10.1016/j.corsci.2005.05.018 ↗
41. The influence of small amounts of KCl(s) on the initial stages of the corrosion of alloy Sanicro 28 at 600°C10.1007/s11085-008-9118-x ↗
42. The chemistry of chromium and some resulting analytical problems10.1289/ehp.91927 ↗
43. Ion chromatography method for the determination of trace levels of chromium(VI) in water
44. Reaction of Cr and Cr oxide with NaCl at elevated temperature10.3323/jcorr.58.348 ↗
45. G.J. Janz, C.B. Allen, J.R. Downey Jr., R.P.T. Tamkins: Eutectic data; safety hazard, corrosion, melting points, compositions and bibliography. Troy, NY: Molten Salts Data Center, Rensselaer Polytechnic Institute, 1976.
46. Das Verhalten der Kaliumchromate bei höherer Temperatur10.1002/zaac.19080580111 ↗