The effect of relative humidity change on atmospheric pitting corrosion of stainless steel 304L
Source abstract
Abstract
Abstract Relative humidity fluctuations tend to influence atmospheric corrosion under natural exposure conditions. In this study, the effect of change in relative humidity on pitting corrosion of stainless steel under MgCl2 droplets is investigated with in situ X-ray microtomography and optical microscopy. Relative humidity fluctuations (between 33% RH and 85% RH or between 33% RH and 12% RH) tend to lead to nucleation of many small pits whereas continuous exposure at constant 33% RH leads to growth of a single pit. This indicates that natural fluctuations in relative humidity might be beneficial for preventing the growth of a large penetrating pit.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Winsley · 2011
2. Effect of nitrate and sulfate on atmospheric corrosion of 304L and 316L stainless steels10.1149/2.0921704jes ↗
3. ACSIS - a model to assess the potential for atmospheric corrosion of stainless steel ILW containers during interim storage and the operational phase of a UK geological disposal facility
4. Overview of UK research on the durability of container materials for radioactive wastes10.1179/1743278214Y.0000000190 ↗
5. Corrosion control of stainless steels in indoor atmospheres-practical experience (Part 2)10.5006/1438 ↗
6. Assessing the risk of under-deposit chloride-induced stress corrosion cracking in austenitic stainless steel nuclear waste containers10.1179/1743278214Y.0000000204 ↗
7. Pitting corrosion of sensitised type 304 stainless steel under wet-dry cycling condition10.1016/j.corsci.2017.02.010 ↗
8. The effect of deposition conditions on atmospheric pitting corrosion location under evans droplets on type 304L stainless steel10.5006/2614 ↗
9. Pitting corrosion mechanism of Type 304 stainless steel under a droplet of chloride solutions10.1016/j.corsci.2006.08.016 ↗
10. Pitting corrosion of bare stainless steel 304 under chloride solution droplets10.1149/1.3467850 ↗
11. Use of inkjet printing to deposit magnesium chloride salt patterns for investigation of atmospheric corrosion of 304 stainless steel10.1016/j.corsci.2011.05.055 ↗
12. Effects of particulate silica coatings on localized corrosion behavior of AISI 304SS under atmospheric corrosion conditions10.1149/1.2722535 ↗
13. Atmospheric pitting corrosion of 304L stainless steel: the role of highly concentrated chloride solutions10.1039/C4FD00246F ↗
14. Relative humidity for onsets of pitting corrosion and repassivation of stainless steels under wet-dry cyclic conditions containing chloride
15. Comparison of influences of NaCl and CaCl2 on the corrosion of 11% and 17% Cr ferritic stainless steels during cyclic corrosion test10.1016/j.corsci.2009.10.033 ↗
16. An electrochemical impedance study on atmospheric corrosion of steels in a cyclic wet-dry condition10.1016/0010-938X(95)00104-R ↗
17. AC impedance monitoring of pitting corrosion of stainless steel under a wet-dry cyclic condition in chloride-containing environment10.1016/0010-938X(96)00028-5 ↗
18. Pitting corrosion mechanism of stainless steels under wet-dry exposure in chloride-containing environments10.1016/S0010-938X(97)00124-8 ↗
19. Pit initiation and repassivation of stainless steels exposed to cyclic relative humidity changes10.1149/2.0151509jes ↗
20. Mechanistic studies of atmospheric pitting corrosion of stainless steel for ILW containers10.1179/1743278214Y.0000000183 ↗
21. Effect of relative humidity on corrosion of steel under sea salt aerosol proxies10.1149/2.0221410jes ↗
22. Effect of relative humidity on corrosion of steel under sea salt aerosol proxies10.1149/2.0231410jes ↗
23. Atmospheric pitting corrosion of stainless steel
24. ASTM, E104-02, 1951 · 2012
25. Guo · 2015
26. I12: the joint engineering, environment and processing (JEEP) beamline at diamond light source10.1107/S1600577515003513 ↗
27. Fiji: an open-source platform for biological-image analysis10.1038/nmeth.2019 ↗
28. Mi · 2013
29. Radiolytic effects on the in-situ investigation of buried interfaces with synchrotron X-RAY techniques10.1016/0022-0728(94)03772-U ↗
30. Xu · 2014
31. Computational modeling of bounding conditions for pit size on stainless steel in atmospheric environments10.1149/1.3261803 ↗
32. Ghahari · 2012
33. systems · 2014
34. Initial stage of pitting corrosion of type 304 stainless steel under thin electrolyte layers containing chloride ions10.1149/1.1992470 ↗
35. Mass-transfer and electrochemical kinetic interactions in localized pitting corrosion10.1002/aic.690320605 ↗
36. Dissolution and repassivation kinetics of FE-CR alloys in pit solutions .1. Effect of the surface salt layer10.1149/1.2056137 ↗
37. Dissolution and repassivation kinetics of a 12.3Cr-2.6Mo-6.5Ni super martensitic stainless steel - a comparative study10.1149/1.1474429 ↗
38. Effect of microstructure on the morphology of atmospheric corrosion pits in type 304L stainless steel10.5006/2935 ↗
39. Infrared observations of the response of NaCl, MgCl2, NH4HSO4, and NH4NO3 aerosols to changes in relative humidity from 298 to 238 K10.1021/jp9931408 ↗
40. Hygroscopic particle behavior studied by interdigitated array microelectrode impedance sensors10.1021/jp4098149 ↗
41. Infrared spectroscopy of model tropospheric aerosols as a function of relative humidity: observation of deliquescence and crystallization10.1029/97JD01361 ↗
42. Efflorescence relative humidity of airborne sodium chloride particles: a theoretical investigation10.1016/j.atmosenv.2006.12.014 ↗
43. Aerosol growth studies—II. Preparation and growth measurements of monodisperse salt aerosols10.1016/0021-8502(77)90002-7 ↗
44. Water content and morphology of sodium chloride aerosol particles10.1029/1999JD900286 ↗
45. Phase transitions of single salt particles studied using a transmission electron microscope with an environmental cell10.1080/02786820500295263 ↗
46. Transport processes and mechanism of pitting of Metals10.1149/1.2132857 ↗
47. Metastable pitting of stainless steel10.5006/1.3583880 ↗
48. Metastable pitting corrosion of stainless-steel and the transition to stability10.1098/rsta.1992.0114 ↗
49. The nucleation, growth and stability of micropits in stainless-steel10.1016/0010-938X(94)90145-7 ↗
50. The mechanism of lacy cover formation in pitting10.1016/S0010-938X(97)00043-7 ↗
51. Pit growth studies in stainless steel foils. I. Introduction and pit growth kinetics10.1016/S0010-938X(01)00133-0 ↗
52. Perforated covers for propagating pits10.1149/1.1838423 ↗
53. Synchrotron X-ray radiography studies of pitting corrosion of stainless steel: extraction of pit propagation parameters10.1016/j.corsci.2015.06.023 ↗
54. Computer simulation of single pit propagation in stainless steel under potentiostatic control10.1149/1.1376119 ↗
55. Pit growth studies in stainless steel foils. II. Effect of temperature, chloride concentration and sulphate addition10.1016/S0010-938X(01)00134-2 ↗
56. Localised dissolution kinetics, salt films and pitting potentials10.1016/S0010-938X(97)00049-8 ↗
57. An experimental confirmation of the pitting potential model of Galvele10.1016/0010-938X(88)90069-8 ↗