Abstract
Abstract S-phase was introduced on stainless steel surface by low-temperature liquid oxy-nitriding and its influence on the corrosion behavior has been explored through surface analysis and weight-loss method. The results indicated that the S-phase layer can significantly improve the corrosion resistance of austenitic stainless steels in H2S/CO2/Cl− simulated solutions, which was proved by lower corrosion rate, surface, and cross-sectional topography after corrosion. This improvement can be attributed to the fact that the Fe3O4 layer blocking the sulfur-containing medium and the consumption of H+ by the active nitrogen atoms, making it difficult for the corrosive medium to penetrate the steel.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (99)
Show source-provided references
1. Novel Cu-bearing high-strength pipeline steels with excellent resistance to hydrogen-induced cracking10.1016/j.matdes.2015.12.029 ↗
2. Non-isothermal prior austenite grain growth of a high-Nb X100 pipeline steel during a simulated welding heat cycle process10.1016/j.matdes.2015.09.039 ↗
3. Comparison of corrosion behaviour of low-alloy pipeline steel exposed to H2S/CO2-saturated brine and vapour-saturated H2S/CO2 environments10.1016/j.electacta.2017.02.114 ↗
4. The performance of Pd–Ag alloy membrane films under exposure to trace amounts of H2S10.1016/j.memsci.2015.10.031 ↗
5. Electrochemical characteristics of the early corrosion stages of API X52 steel exposed to H2S environments10.1016/j.matchemphys.2014.10.020 ↗
6. Electrochemical migration, whisker formation, and corrosion behavior of printed circuit board under wet H2S environment10.1016/j.electacta.2013.10.051 ↗
7. On the role of crystallographic texture in mitigating hydrogen-induced cracking in pipeline steels10.1016/j.corsci.2011.08.031 ↗
8. Pipeline failures in corrosive environments – a conceptual analysis of trends and effects10.1016/j.engfailanal.2015.03.004 ↗
9. Combined effect of pH and H2S on the structure of passive film formed on type 316L stainless steel10.1016/j.apsusc.2018.07.122 ↗
10. The electrochemical behaviour of 316L austenitic stainless steel in Cl− containing environment under different H2S partial pressures10.1016/j.apsusc.2013.10.080 ↗
11. Investigation of the deterioration of passive films in H2S-containing solutions10.1007/s12613-017-1482-6 ↗
12. Influence of H2S on the pitting corrosion of 316 L stainless steel in oilfield brine10.1016/j.corsci.2021.109265 ↗
13. The influence of microstructure on the protective properties of the corrosion product layer generated on the welded API X70 steel in chloride solution10.1016/j.corsci.2013.01.026 ↗
14. Effect of immersion time on the hydrogen content and tensile properties of A350LF2 steel exposed to hydrogen sulphide environments10.1016/j.corsci.2012.11.038 ↗
15. The effect of the partial pressure of H2S on the permeation of hydrogen in low carbon pipeline steel10.1016/j.corsci.2012.10.016 ↗
16. Untersuchungen zum Korrosionsmechanismus von unlegiertem Stahl in sauerstofffreien Kohlensäurelösungen. Teil I. Kinetik der Wasserstoffabscheidung10.1002/maco.19770281203 ↗
17. A new narrative for CO 2 corrosion of mild steel10.1149/2.0071911jes ↗
18. Key issues related to modelling of internal corrosion of oil and gas pipelines – a review10.1016/j.corsci.2007.06.006 ↗
19. Electrochemical growth of Iron sulfide films in H 2 S-Saturated chloride media10.5006/1.3299205 ↗
20. Corrosion and stress corrosion cracking behavior of 316L austenitic stainless steel in high H2S–CO2–Cl− environment10.1007/s10853-013-7168-1 ↗
21. Corrosion of stainless steel 316L in simulated formation water environment with CO2–H2S–Cl−10.1016/j.corsci.2009.08.010 ↗
22. Effect of CO2 and H2S on the composition and stability of passive film on iron alloy in geothermal water10.1016/j.electacta.2007.01.086 ↗
23. Detecting and monitoring erosion-corrosion using ring pair electrical resistance sensor in conjunction with electrochemical measurements10.1016/j.wear.2019.03.025 ↗
24. Understanding the influences of pre-corrosion on the erosion-corrosion performance of pipeline steel10.1016/j.wear.2019.203151 ↗
25. A study on corrosion behaviors of Ni–Cr–Mo laser coating, 316 stainless steel and X70 steel in simulated solutions with H2S and CO210.1016/j.surfcoat.2016.02.017 ↗
26. Exploring new W–B coating materials for the aqueous corrosion–wear protection of austenitic stainless steel10.1016/j.tsf.2013.09.035 ↗
27. Analysis of surface properties of tungsten carbide (WC) coating over austenitic stainless steel (SS316) using plasma spray process10.1016/j.matpr.2019.09.219 ↗
28. Compound layer growth and compound layer porosity of austenite plasma nitrocarburised non-alloyed steel10.1016/0257-8972(94)01009-8 ↗
29. Surface nitriding of SUS 304 austenitic stainless steel by a molten salt electrochemical process
30. Surface modification of 2205 duplex stainless steel by low temperature salt bath nitrocarburizing at 430 °C10.1016/j.apsusc.2013.01.111 ↗
31. Influence of the nitriding time in the wear behaviour of an AISI H13 steel during a crankshaft forging process10.1016/j.wear.2007.02.007 ↗
32. Zhang · Appl. Surf. Sci. · 2018 · 440 · 75510.1016/j.apsusc.2018.01.225 ↗
33. Thermal stability of low-temperature-carburized austenitic stainless steel10.1016/j.actamat.2017.02.018 ↗
34. Structure of the ion-nitrided layer of 18-8 stainless steel
35. Interstitial defects in 316L austenitic stainless steel containing “colossal” carbon concentrations: an internal friction study10.1016/j.scriptamat.2007.02.035 ↗
36. Gavriljuk · 1999 · 45
37. S-phase surface engineering of Fe-Cr, Co-Cr and Ni-Cr alloys10.1179/095066009X12572530170589 ↗
38. Corrosion properties of active screen plasma nitrided 316 austenitic stainless steel10.1016/j.corsci.2003.09.015 ↗
39. A comparative study of the tribocorrosion behaviour of low temperature nitrided austenitic and duplex stainless steels in NaCl solution10.1016/j.triboint.2020.106412 ↗
40. Plasma nitriding of 316L stainless steel in two different N2-H2 atmospheres - Influence on microstructure and corrosion resistance10.1016/j.surfcoat.2017.01.037 ↗
41. Erosion–corrosion resistance properties of 316L austenitic stainless steels after low-temperature liquid nitriding10.1016/j.apsusc.2018.01.225 ↗
42. Active screen plasma nitriding of 316 stainless steel for the application of bipolar plates in proton exchange membrane fuel cells10.1016/j.ijhydene.2014.04.102 ↗
43. Nitrogen significantly enhances corrosion resistance of 316L stainless steel in thiosulfate-chloride solution10.1016/j.corsci.2020.108792 ↗
44. A self-healing stainless steel: role of nitrogen in eliminating detrimental effect of cold working on pitting corrosion resistance10.1016/j.corsci.2018.09.013 ↗
45. 2003
46. The inhibition of CO2 corrosion of N80 mild steel in single liquid phase and liquid/particle two-phase flow by aminoethyl imidazoline derivatives10.1016/j.corsci.2008.12.024 ↗
47. Sour corrosion of C110 steel and its influence by galvanic couple and stress10.1021/ie2018492 ↗
48. Srinivasan · 1999 · 12
49. Corrosion of low alloy steel and stainless steel in supercritical CO2/H2O/H2S systems10.1016/j.corsci.2016.06.003 ↗
50. Comparison of the characteristics of corrosion scales covering 3Cr steel and X60 steel in CO2-H2S coexistence environment10.1016/j.jngse.2020.103371 ↗
51. The theory of stress corrosion cracking in alloys10.1108/eb006879 ↗
52. Effect of high temperature on the corrosion behavior and passive film composition of 316 L stainless steel in high H2S-containing environments10.1016/j.corsci.2020.108844 ↗
53. Influence of pH on the passivation behaviour of 904L stainless steel bipolar plates for proton exchange membrane fuel cells10.1016/j.jallcom.2016.06.013 ↗
54. Full depth profile of passive films on 316L stainless steel based on high resolution HAXPES in combination with ARXPS10.1016/j.apsusc.2012.02.099 ↗
55. Comparison study on the semiconductive and dissolution behaviour of 316L and alloy 625 in hydrochloric acid solution
56. The surface characterization and passive behavior of Type 316L stainless steel in H 2 S-containing conditions10.1016/j.apsusc.2017.06.214 ↗
57. A Round Robin on combined electrochemical and AES/ESCA characterization of the passive films on FeCr and FeCrMo alloys10.1016/0010-938X(88)90026-1 ↗
58. Low-temperature nitrocarburizing of austenitic stainless steel for combat corrosion in H2S environments
59. Effect of carbon and nitrogen on chemical homogeneity of Fcc iron-based alloys10.1007/s11661-997-0177-4 ↗
60. Electrochemical investigation of the influence of nitrogen alloying on pitting corrosion of austenitic stainless steels10.1016/S0010-938X(99)00013-X ↗
61. Corrosion of P235GH carbon steel in simulated Bure soil solution
62. Influence of cooling rate on the structure and formation of oxide scale in low carbon steel wire rods during hot rolling10.1016/j.surfcoat.2005.12.014 ↗
63. Formation of iron oxide and iron sulfide at high temperature and their effects on corrosion10.1016/j.corsci.2018.02.045 ↗
64. Unraveling the effects of CO2 and H2S on the corrosion behavior of electroless Ni-P coating in CO2/H2S/Cl– environments at high temperature and high pressure10.1016/j.corsci.2018.12.022 ↗
65. Mesh-capped probe design for direct pH measurements at an actively corroding metal surface10.1007/s10800-009-0043-8 ↗
66. Measuring the growth of oxide films on low carbon steel at 500°C by impedance spectroscopy10.1016/S0010-938X(99)00079-7 ↗
67. Chemical diffusion in non-stoichiometric metal sulphides10.1007/BF01154488 ↗
68. Transport properties of sulfide scales and sulfidation of metals and alloys10.1007/BF00659899 ↗
69. Krishnamoorthy · 2016
70. Herbert · 2015
71. Peering below the surface10.1038/nmat1226 ↗
72. A point defect model for anodic passive films: II. Chemical breakdown and pit initiation10.1149/1.2127592 ↗
73. Effect of nitrogen alloying on the semiconducting properties of passive films and metastable pitting susceptibility of 316L and 316LN stainless steels10.1016/j.matchemphys.2010.02.033 ↗
74. The effect of electrochemical nitridation on the corrosion resistance of the passive films formed on the 2205 duplex stainless steel10.1016/j.matlet.2019.126640 ↗
75. High corrosion resistance of austenitic stainless steel alloyed with nitrogen in an acid solution10.1016/j.corsci.2011.02.039 ↗
76. Srinivasan · 1996
77. Universalism of hydrogen sulfide and carbon dioxide corrosion inhibitors in conditions of oil production and processing10.1007/s10556-018-0464-5 ↗
78. Hydrogen trapping on non metallic inclusions in Cr-Mo low alloy steels10.1016/S0010-938X(98)00008-0 ↗
79. Hydrogen embrittlement understood10.1007/s11661-015-2836-1 ↗
80. The effect of absorbed hydrogen on the dissolution of steel10.1016/j.heliyon.2016.e00209 ↗
81. Effects of surface oxide films on hydrogen permeation and susceptibility to embrittlement of X80 steel under hydrogen atmosphere10.1016/j.ijhydene.2017.12.170 ↗
82. Entry, transport and absorption of hydrogen in low-temperature plasma nitrided austenitic stainless steel10.1016/S1359-6454(01)00112-4 ↗
83. Hydrogen absorption in plasma-nitrided iron10.1016/j.actamat.2005.11.018 ↗
84. Effect of strain-induced martensite on hydrogen embrittlement of austenitic stainless steels investigated by combined tension and hydrogen release methods10.1016/j.ijhydene.2013.01.198 ↗
85. Influence of nitrogen alloying on hydrogen embrittlement in AISI 304-type stainless steels10.1007/BF02647103 ↗
86. Effect of hydrogenation on mechanical properties and tensile fracture mechanism of a high-nitrogen austenitic steel10.1007/s10853-016-0676-z ↗
87. Nitrogen effect on hydrogen diffusivity and hydrogen embrittlement behavior in austenitic stainless steels10.1016/j.scriptamat.2020.03.038 ↗
88. Effect of S-phase on the hydrogen induced phase transition and hydrogen embrittlement susceptibility in AISI 304 stainless steel10.1016/j.matpr.2015.07.377 ↗
89. Stress corrosion behavior of low-temperature liquid-nitrided 316 austenitic stainless steel in a sour environment
90. A comprehensive review on internal corrosion and cracking of oil and gas pipelines10.1016/j.jngse.2019.102971 ↗
91. Galvanic corrosion of carbon steel in anoxic conditions at 80°C associated with a heterogeneous magnetite (Fe3O4)/mackinawite (FeS) layer10.1016/j.electacta.2017.09.183 ↗
92. Effect of H2S on the CO2 corrosion of carbon steel in acidic solutions10.1016/j.electacta.2010.08.049 ↗
93. Near-neutral pH corrosion of mill-scaled X-65 pipeline steel with paint primer10.1016/j.jmst.2020.01.016 ↗
94. Effect of residual dissolved oxygen on the corrosion behavior of low carbon steel in 0.1M NaHCO3 solution10.1016/j.jmst.2017.11.004 ↗
95. The effect of alloyed nitrogen or dissolved nitrate ions on the anodic behaviour of austenitic stainless steel in hydrochloric acid10.1016/0010-938X(87)90040-0 ↗
96. Role of nitrogen in improving resistance to localized corrosion in austenitic stainless steels. [22 Cr20 Ni6 Mo]
97. Surface composition of stainless steel during active dissolution and passivation10.2355/isijinternational.31.134 ↗
98. Electrochemical investigation of the influence of nitrogen alloying on pitting corrosion of austenitic stainless steels10.1016/S0010-938X(99)00013-X ↗
99. Microelectrodes for the study of localized corrosion