Abstract
Abstract Oxidation behavior in O2 + 10% H2O at 800 °C of an austenitic stainless steel with or without aluminum is investigated. The Al-free steel enters into breakaway oxidation stage after only 15 h exposure, while the one with 2.7 wt% aluminum shows high oxidation resistance. This minor amount of aluminum is lower than the critical content to form an intact alumina scale, but it promotes the formation of a thin Al-rich inner layer which is favor in prohibiting holes formation due to volatilization of CrO2(OH)2 and Kirkendall effect. A compact scale develops and protects the Al-containing steel very well.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. The oxidation behavior of metals and alloys at high temperatures in atmospheres containing water vapor: a review10.1016/j.pmatsci.2007.11.001 ↗
2. A review of the oxidation behavior of structural alloys in steam10.1179/095066010X12646898728165 ↗
3. Corrosion of engineering materials in a supercritical water cooled reactor: characterization of oxide scales on Alloy 800H and stainless steel 31610.1016/j.corsci.2015.07.035 ↗
4. Experimental and numerical investigation of stress corrosion cracking of sensitized type 304 stainless steel under high-temperature and high-purity water10.1016/j.corsci.2015.05.001 ↗
5. Effect of thermo-mechanical processing on oxidation of austenitic stainless steel 316L in supercritical water10.1016/j.corsci.2015.02.008 ↗
6. Surface phase transformation in austenitic stainless steel induced by cyclic oxidation in humidified air10.1016/j.corsci.2015.08.030 ↗
7. Enhanced oxidation of 9% Cr in water vapor containing environment10.1016/j.corsci.2006.02.002 ↗
8. Temperature and water vapour effects on the cyclic oxidation behavior of Fe–Cr alloys10.1016/j.corsci.2010.04.026 ↗
9. Evidence for chromium evaporation influencing the oxidation of 304L: the effect of temperature and flow rate10.1023/A:1014877600235 ↗
10. Comparison between the oxidation of iron in oxygen and in steam at 650–750°C10.1016/j.corsci.2013.06.014 ↗
11. Theoretical and experimental investigation of the thermochemistry of CrO2(OH)2(g)10.1021/jp0647380 ↗
12. Investigation into the failure mechanism of chromia scale thermally grown on an austenitic stainless steel in pure steam10.1016/j.corsci.2016.03.021 ↗
13. Oxidation of 310 steel in H2O/O2 mixtures at 600°C: the effect of water-vapour-enhanced chromium evaporation10.1016/S0010-938X(02)00056-2 ↗
14. High pressure steam oxidation of alloys for advanced ultra-supercritical conditions10.1007/s11085-014-9491-6 ↗
15. The mechanism of the high-temperature oxidation of iron-chromium alloys in water vapor10.1149/1.2425963 ↗
16. Chromium volatilization rates from Cr2O3 scales into flowing gases containing water vapor10.1007/s11085-006-9030-1 ↗
17. Oxidation of Fe–10Cr in O2 and in O2 + H2O environment at 600°C: A microstructural investigation10.1016/j.corsci.2013.06.016 ↗
18. High Temperature oxidation of Fe-Cr alloys in wet oxygen10.1007/BF01670507 ↗
19. Indication of chromium oxide hydroxide evaporation during oxidation of 304L at 873K in the presence of 10% water vapor10.1023/A:1018875024306 ↗
20. The effect of water vapor on the initial stages of oxidation of the FeCrAl Alloy Kanthal AF at 900°C10.1007/s11085-007-9055-0 ↗
21. A comparison of the oxidation behaviors of Al2O3 formers and Cr2O3 formers at 700°C − oxide solid solutions acting as a template for nucleation10.1016/j.corsci.2007.12.012 ↗
22. Temperature dependence of metastable alumina formation during thermal oxidation of FeCrAl foils10.1002/maco.200403851 ↗
23. Microstructure and mechanical properties of Al-alloyed Fe–Cr–Ni–Mn–C stainless steels10.1016/j.msea.2014.09.001 ↗
24. Creep-resistant, Al2O3-forming austenitic stainless steels10.1126/science.1137711 ↗
25. Development of L12-ordered Ni3(Al, Ti)-strengthened alumina-forming austenitic stainless steel alloys10.1016/j.scriptamat.2013.09.005 ↗
26. Effects of minor alloy additions and oxidation temperature on protective alumina scale formation in creep-resistant austenitic stainless steels10.1016/j.scriptamat.2007.08.032 ↗
27. Effects of silicon additions on the oxide scale formation of an alumina-forming austenitic alloy10.1016/j.corsci.2012.08.039 ↗
28. Young · 2008
29. Oxidation of binary FeCr alloys (Fe–2.25Cr, Fe–10Cr, Fe–18Cr and Fe–25Cr) in O2 and in O2 + H2O environment at 600°C10.1007/s11085-010-9229-z ↗
30. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
31. Improvement of high-temperature oxidation resistance and strength in alumina-forming austenitic stainless steels10.1016/j.matlet.2011.07.021 ↗
32. The effect of the oxidation atmosphere on the initial oxidation of type 430 stainless steel at 1273K10.1016/S0010-938X(97)00113-3 ↗
33. Growth and adherence of chromia based surface scales on Ni-base alloys in high- and low-pO2 gases10.1016/j.msea.2007.05.035 ↗
34. Passivity and inhibition during the oxidation of metals at elevated temperatures10.1016/S0010-938X(65)80003-8 ↗
35. Composition microstructure, and water vapor effects on internal/external oxidation of alumina-forming austenitic stainless steels10.1007/s11085-009-9161-2 ↗