Cr diffusion coatings on a ferritic-martensitic steel for corrosion protection in KCl-rich biomass co-firing environments
Source abstract
Abstract
Abstract Three diffusion coatings (Cr, Ni + Cr, Ni-P + Cr) on a ferritic-martensitic X20CrMoV12-1 steel were investigated in a biomass-co-firing atmosphere in comparison to uncoated austenitic DMV 310 N. Exposures were conducted at 650 °C for up to 300 h with pure sulphates as well as a mixture of sulphates and KCl. These aggressive testing conditions were chosen to accelerate degradation of the specimens allowing for an efficient ranking between them. Beneath the deposit of Na2SO4-K2SO4 the coatings proved to be highly resistant whereas addition of KCl drastically accelerated the corrosive attack. This is discussed within the frame of different synergistic high temperature corrosion mechanisms.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Nag · 2008
2. High chromium martensitic steels - microstructure, properties and potential for further development
3. Development of seamless tubes for thermal and nuclear power plants10.2320/materia1962.22.389 ↗
4. Field test corrosion experiments in Denmark with biomass fuels. Part 1: straw-firing10.1002/1521-4176(200202)53:2<121::AID-MACO121>3.0.CO;2-R ↗
5. KCl-induced high temperature corrosion of selected commercial alloys - Part I: chromia-formers10.1002/maco.201408213 ↗
6. KCl-induced high temperature corrosion of selected commercial alloys - Part II: alumina and silica-formers10.1002/maco.201408215 ↗
7. Lab-scale investigations of high-temperature corrosion phenomena in straw-fired boilers10.1021/ef990001g ↗
8. Lab-Scale Investigation of Deposit-Induced Chlorine Corrosion of Superheater Materials under Simulated Biomass-firing Conditions. Part 1: Exposure at 560 °C10.1021/ef9000924 ↗
9. The influence of small amounts of KCl(s) on the high temperature corrosion of a Fe-2.25Cr-1Mo steel at 400 and 500°C10.1002/maco.201005942 ↗
10. Effect of flue gas composition on deposit induced high temperature corrosion under laboratory conditions mimicking biomass firing. Part I: exposures in oxidizing and chlorinating atmospheres
11. Effect of flue gas composition on deposit induced high temperature corrosion under laboratory conditions mimicking biomass firing. Part II: exposures in SO2 containing atmospheres10.1002/maco.201609174 ↗
12. Lehmusto · 2012
13. Comparison of potassium chloride and potassium carbonate with respect to their tendency to cause high temperature corrosion of stainless 304L steel10.1016/j.fuproc.2011.12.016 ↗
14. High temperature interaction of pure Cr with KCl10.4028/www.scientific.net/MSF.461-464.1047 ↗
15. The role of alloying elements in commercial alloys for corrosion resistance in oxidizing-chloridizing atmospheres Part I: literature evaluation and thermodynamic calculations on phase stabilities10.1002/maco.200390129 ↗
16. Role of alloying elements and carbides in the chlorine-induced corrosion of steels and alloys10.1590/S1516-14392004000100013 ↗
17. Acceleration of the High temperature oxidation of metals by chlorine
18. Modelling fireside corrosion of thermal sprayed coatings in co-firing of coal/biomass10.1002/maco.201307063 ↗
19. High temperature interaction of Al/Si-modified Fe–Cr alloys with KCl10.1016/j.corsci.2006.10.019 ↗
20. In-situ corrosion investigation at Masnedø CHP plant - a straw-fired power plant10.1002/(SICI)1521-4176(199910)50:10<579::AID-MACO579>3.0.CO;2-M ↗
21. The influence of copper in ash deposits on the corrosion of boiler tube alloys for waste-to-energy plants10.1002/maco.201206787 ↗
22. Senff-Wollenberg · 2009 · 501
23. Corrosion damage to the conveyor belt of a furnace for the removal of soil from organic chlorine compounds10.1002/maco.19970480307 ↗
24. Assessment of the degradation of metals and alloys in air-2 %chlorine at high temperature10.1080/02619180.1988.11753389 ↗
25. Chloridation-oxidation of nine commercial high-temperature alloys at 800°C10.1007/BF02153465 ↗
26. Fireside corrosion of chromium-and aluminum-coated ferritic-martensitic steels10.1007/s11085-016-9684-2 ↗
27. A calculation method of biomass slagging rate based on crystallization theory10.1002/apj.1775 ↗
28. An investigation of the embrittlement in X20CrMoV12.1 power plant steel after long-term service exposure at elevated temperature10.1016/j.msea.2004.05.080 ↗
29. The implication of chlorine-associated corrosion on the operation of biomass-fired boilers10.1016/S0360-1285(00)00003-4 ↗
30. ISO 21608: International Standard: Corrosion of metals and alloys - Test method for isothermal-exposure oxidation testing under high-temperature corrosion conditions for metallic materials. ISO 21608:2012. 2012. ISO TC156 WG 13 (High Temperature Corrosion). 19-12-2006.
31. NACE International Publication - Electroless Nickel Coatings. 24089. 1997. NACE International Publication.
32. R. Parkinson, Properties and applications of electroless nickel. 1-33. 25-5-2011. Nickel Development Institute.
33. Deposition of manganese and cobalt on ferritic-martensitic steels via pack cementation process10.1007/s11085-012-9340-4 ↗
34. Order-disorder transitions and solid state reaction kinetics in Na2SO4-K2SO4 system10.1139/v83-107 ↗
35. ISO · 2015
36. Fireside corrosion degradation of 15Mo3, T22, T23 & T91 in simulated coal-biomass co-fired environment10.1002/maco.201407886 ↗
37. Water-free methods of preparation for the analysis of chlorides in the high temperature oxidation in chlorine containing atmospheres
38. Fähsing · 2016
39. Kinetics of HCl emission from inorganic chlorides in simulated municipal wastes incineration conditions10.1016/j.ces.2004.07.131 ↗
40. KCl induced corrosion of a 304-type austenitic stainless steel at 600°C; the role of potassium10.1007/s11085-005-5704-3 ↗
41. Bürgel · 2001
42. Combustion characteristics of different biomass fuels10.1016/j.pecs.2003.10.004 ↗
43. Chlorine attack of carbon steel between 350 and 500 °C and its importance regarding corrosion in waste incineration10.1007/s11085-017-9749-x ↗
44. Pasten · 2006
45. Determination of the initiation and propagation mechanism of fireside corrosion
46. The effect of K2SO4 additive in Na2SO4 deposits on low temperature hot corrosion of iron-aluminum alloys10.1007/BF00665661 ↗
47. High temperature corrosion of matallic materials in composed oxidizing environements10.1515/htmp-2012-0091 ↗
48. Hot corrosion Type II of FeCr-based model alloys for boiler and heat exchanger applications10.1002/maco.201810640 ↗
49. Schütze · 2011 · 573
50. Effect of microstructure on KCl corrosion attack of modified AISI 310 steel10.1080/09603409.2017.1389381 ↗
51. Role of carbides in the high temperature corrosion of steels in HCl-containing atmospheres
52. Oxidation resistance of carbides in chlorine-containing atmospheres10.1515/HTMP.2002.21.5.307 ↗
53. Corrosion behaviour of austenitic stainless steels in the high chloride-containing environment10.1016/0921-5093(89)90754-5 ↗
54. Alkali induced corrosion of 304-type austenitic stainless steel at 600°C; comparison between KCl, K2CO3 and K2SO410.4028/www.scientific.net/MSF.595-598.367 ↗
55. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
56. The effects of KCl, K2SO4 and K2CO3 on the high temperature corrosion of a 304-Type austenitic stainless steel10.1007/s11085-011-9240-z ↗
57. The oxidation of alloys10.1088/0034-4885/39/5/001 ↗
58. On the hot corrosion of nickel at 700° C10.1007/s11085-015-9588-6 ↗
59. Electroless deposition of nickel