journal article·2020-10

Achieving superior hot corrosion resistance by PVD/HVOF duplex design

Pengjun Tang, Dongqing He, Wensheng Li, Lunlin Shang, Haimin Zhai, Liping Wang, Guangan Zhang

Corrosion Science· Volume 175
Publisher page

Abstract

Abstract In this study, an optimized duplex coating, consisting of a thick Cr3C2-NiCr interlayer and a top CrN film, were designed and deposited by HVOF and PVD. And then hot corrosion behaviors were systematically investigated, and corresponding corrosion mechanisms are discussed in detailed. Results showed that the thickness of the oxide scale of duplex coating is approximately one-tenth that of the Cr3C2-NiCr coating. Due to the formation of Cr2O3 oxide film, the CrN/Cr3C2-NiCr duplex coating exhibits superior hot corrosion resistance. However, chlorine-induced corrosion in uncovered holes is the main cause of local failure of duplex coating.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. A comparative study to evaluate the corrosion performance of Zr incorporated Cr3C2-(NiCr) coating at 900 °C10.1016/j.ceramint.2018.01.047 ↗
2. Chlorine induced high-temperature corrosion mechanisms in HVOF and HVAF sprayed Cr3C2-based hardmetal coatings10.1016/j.corsci.2019.108166 ↗
3. Hot corrosion resistance of high-velocity oxyfuel sprayed coatings on a nickel-base superalloy in molten salt environment10.1361/105996306X124392 ↗
4. High temperature wear performance of HVOF-sprayed Cr3C2-WC-NiCoCrMo and Cr3C2-NiCr hardmetal coatings10.1016/j.apsusc.2017.04.132 ↗
5. The role of microstructure in the high temperature oxidation mechanism of Cr3C2-NiCr composite coatings10.1016/j.corsci.2009.02.027 ↗
6. High-temperature erosion of HVOF sprayed Cr3C2-NiCr coating and mild steel for boiler tubes10.1007/s11666-008-9222-0 ↗
7. Corrosive wear behavior of chromium carbide coatings deposited by air plasma spraying10.1016/j.ceramint.2015.02.131 ↗
8. Corrosion behavior of hvof sprayed hard face coatings in alkaline-sulfide solution10.1016/j.apsusc.2017.04.149 ↗
9. Structure and wear behavior of NiCr-Cr3C2 coatings sprayed by supersonic plasma spraying and high velocity oxy-fuel technologies10.1016/j.apsusc.2015.08.019 ↗
10. Comparison of dry sliding friction and wear of Ti6Al4V alloy treated by plasma electrolytic oxidation and PVD coating10.1016/j.wear.2007.01.045 ↗
11. The electrochemical behavior of thermally oxidized CrN coatings deposited on steel by cathodic arc plasma deposition10.1016/j.apsusc.2004.05.024 ↗
12. Industrial applications of CrN (PVD) coatings, deposited at high and low temperatures10.1016/S0257-8972(97)00393-9 ↗
13. Hard coatings on thermochemically pretreated soft steels: application potential for ball valves10.1016/S0257-8972(98)00809-3 ↗
14. Characterization of duplex coating system (HVOF+PVD) on light alloy substrates10.1016/j.surfcoat.2016.06.020 ↗
15. An experimental method for evaluation of the load-carrying capacity of coated aluminium: the influence of coating stiffness, hardness and thickness10.1016/S0257-8972(00)00568-5 ↗
16. Production and characterization of duplex coating (HVOF and PVD) on Ti–6Al–4V substrate10.1016/j.tsf.2005.12.058 ↗
17. Thermal stability and mechanical properties of HVOF/PVD duplex ceramic coatings produced by HVOF and cathodic vacuum arc10.1016/j.ceramint.2017.02.151 ↗
18. High temperature oxidation of thin CrN coatings deposited on steel10.1116/1.580014 ↗
19. Investigation of Fe3Al-based PVD/HVOF duplex coatings to protect stainless steel from sliding wear against alumina10.1016/j.surfcoat.2018.07.070 ↗
20. Tribological studies on PVD/HVOF duplex coating on Ti6Al4V substrate10.1016/j.surfcoat.2008.06.055 ↗
21. Designs and preparation of advanced HVOF-PVD duplex coating by combination of HVOF and arc ion plating10.1016/j.surfcoat.2016.06.017 ↗
22. Study of corrosion and tribocorrosion of Fe3Al-based duplex PVD/HVOF coatings against alumina in NaCl solution10.1016/j.surfcoat.2018.10.060 ↗
23. Tribological behaviors of CrN/Cr3C2-NiCr duplex coating at elevated temperatures10.1016/j.surfcoat.2019.124926 ↗
24. Oxidation resistance of CrN and CrAlN coating tools10.4028/www.scientific.net/AMR.189-193.137 ↗
25. Corrosion resistance of CrN thin films produced by dc magnetron sputtering10.1016/j.apsusc.2012.12.148 ↗
26. Improvement in corrosion resistance of CrN coatings10.1016/j.surfcoat.2018.07.018 ↗
27. High temperature oxidation of a CrN coating deposited on a steel substrate by ion plating10.1016/S0257-8972(01)01238-5 ↗
28. Hot corrosion behaviour of HVOF-sprayed Cr3C2-NiCrMoNbAl coating10.1016/j.surfcoat.2016.10.076 ↗
29. Hot corrosion behavior of HVOF-sprayed Cr3C2-WC-NiCoCrMo coating10.1016/j.ceramint.2017.04.109 ↗
30. Simultaneously achieving superior mechanical and tribological properties in WC/a-C nanomultilayers via structural design and interfacial optimization10.1016/j.jallcom.2016.12.173 ↗
31. Effect of surface roughness on early stages of pitting corrosion of type 301 stainless steel10.1016/S0010-938X(97)00072-3 ↗
32. The preparation and hot corrosion resistance of gradient NiCoCrAlYSiB coatings10.1016/j.surfcoat.2004.12.005 ↗
33. Chemisorption of oxygen on Ni (100) by SIMS and XPS10.1016/0039-6028(78)90216-9 ↗
34. Weak ferromagnetism at room temperature in Ti incorporated Cr2O3 thin film10.1016/j.physb.2019.06.031 ↗
35. One-step catalase controllable degradation of C3N4 for N-doped carbon dot green fabrication and their bioimaging applications10.1039/C4TB00772G ↗
36. Changes in the chemical state and composition of the clean surface of K2CrO4 and K2Cr2O7 due to air exposure and argon ion bombardment10.1002/(SICI)1096-9918(199703)25:3<161::AID-SIA223>3.0.CO;2-S ↗
37. Potassium chromate by XPS10.1116/1.1247820 ↗
38. Influence of Cr content on hot corrosion and a special tube sealing test of single crystal nickel base superalloy10.1016/j.corsci.2019.05.001 ↗
39. Barin · 1995
40. High-temperature corrosion performance of HVAF-sprayed NiCr, NiAl, and NiCrAlY coatings with alkali sulfate/chloride exposed to ambient air10.1016/j.corsci.2019.06.021 ↗
41. The implications of chlorine-associated corrosion on the operation of biomass-fired boilers10.1016/S0360-1285(00)00003-4 ↗
42. Chlorine-induced high temperature corrosion of HVAF-sprayed Ni-based alumina and chromia forming coatings10.1016/j.corsci.2017.12.033 ↗
43. Influence of the combined-effect of NaCl and Na2SO4 on the hot corrosion behaviour of aluminide coating on Ni-based alloys10.1016/j.jallcom.2019.03.165 ↗
44. Hot corrosion behaviour of Pt modified aluminized NiCrAlYSi coating on a Ni-based single crystal superalloy10.1016/j.corsci.2019.01.014 ↗
45. XPS in the study of high-temperature oxidation of CrN and TiN hard coatings10.1016/0257-8972(95)08360-X ↗
46. The effect of the Re-Ni diffusion barrier on the adhesion strength and thermal shock resistance of the NiCoCrAlY coating10.1016/j.surfcoat.2018.03.037 ↗