journal article·2015-12Open access

Reaction morphologies developed by nickel aluminides in type II hot corrosion conditions: The effect of chromium

Thomas Gheno, Maryam Zahiri Azar, Arthur H. Heuer, Brian Gleeson

Corrosion Science· Volume 101

Abstract

Abstract The short-term reaction of Ni–36Al (at. %) and Ni–36Al–5Cr alloys with Na 2 SO 4 in O 2 -0.1% SO 2 at 700 °C was studied by SEM and TEM. Local failure of the protective scale on NiAl led to nodule development via internal oxidation. Conversely, NiAlCr underwent a uniform attack involving internal sulfidation, porous scale growth, and NiO and Al 2 O 3 dissolution into the sulfate. The roles of gas and sulfate compositions were studied by comparing exposures to Na 2 SO 4 , Na 2 SO 4 –MgSO 4 and Na 2 SO 4 –Cr 2 O 3 deposits in air and O 2 -0.1% SO 2 . The effect of Cr in preventing passivation during early-stage exposure was associated with a coupled dissolution of NiO and Cr 2 O 3 .
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Formation and reactivity thermodynamics of sodium sulfate with gas turbine alloys10.5006/0010-9312-24.5.127 ↗
2. Mechanisms for hot corrosion of nickel-base alloys10.1007/BF02649626 ↗
3. Hot corrosion of high-temperature alloys10.1146/annurev.ms.07.080177.002401 ↗
4. Chemistry and electrochemistry of the hot corrosion of metals10.5006/1.3583026 ↗
5. Low-temperature hot corrosion in gas-turbines—a review of causes and coatings therefor10.1115/1.3239921 ↗
6. Birks · 2006
7. Hot corrosion of metals and alloys10.1007/s11085-011-9254-6 ↗
8. Mechanism of Na2SO4 induced corrosion at 600°C–900°C10.1149/1.2129375 ↗
9. Na2SO4-induced accelerated oxidation (hot corrosion) of nickel10.1007/BF02642794 ↗
10. Barin · 1993
11. Thermodynamic modeling of the Ni–S system10.3139/146.018005 ↗
12. Thermodynamic properties of double oxides of NaO with oxides of Cr, Ni and Fe10.1016/0022-3115(77)90157-X ↗
13. The solubilities of NiO, Co3O4, and ternary oxides in fused Na2SO4 at 1200 °K10.1149/1.2129374 ↗
14. The construction of isothermal quaternary phase-diagrams of the Na–M–O–S type for hot corrosion applications10.1007/BF00666383 ↗
15. Thermodynamics of molten sulfate mixtures10.1149/1.2124305 ↗
16. Synergistic dissolution of oxides in molten sodium sulfate10.1149/1.2086647 ↗
17. Hot corrosion of metals by molten salts
18. Low-temperature hot corrosion of cobalt-base alloys. 1. Morphology of the reaction product10.1007/BF02647841 ↗
19. Low-temperature hot corrosion of cobalt-base alloys. 2. Reaction mechanism10.1007/BF02647842 ↗
20. Sulfate-induced hot corrosion of nickel10.1007/BF00656835 ↗
21. The high temperature corrosion of metals in sulfidizing-oxidizing environments: a critical review10.1515/HTMP.1989.8.3.149 ↗
22. On the hot corrosion of nickel at 700°C10.1007/s11085-015-9588-6 ↗
23. Investigations of the mechanisms of Type-II hot corrosion of superalloy CMSX-410.1016/j.corsci.2013.11.048 ↗
24. Type II hot corrosion: kinetics studies of CMSX-410.1007/s11085-013-9395-x ↗
25. Type II hot corrosion: behavior of CMSX-4 and IN738LC as a function of corrosion environment10.1002/maco.201307425 ↗
26. Compositional factors affecting protective alumina formation under type II hot corrosion conditions10.1007/s11085-013-9410-2 ↗
27. Materials Preparation Center, Ames Laboratory USDOE, Ames IA, USA.
28. Phase transitions and ionic conductivity of the Na2SO4–MgSO4 system10.1016/0167-2738(90)90280-5 ↗
29. Microstructural study of the θ−α transformation in alumina scales formed on nickel aluminides10.1179/mht.2000.011 ↗
30. Thermodynamic re-assessment of the ternary system Al–Cr–Ni10.1016/S0364-5916(01)00049-9 ↗
31. γ-Al2O3 thin film formation via oxidation of β-NiAl(110)10.1016/j.actamat.2011.05.064 ↗
32. E.M. Levin, H.F. McMurdie, Phase diagrams for ceramists 1975 supplement, Am Ceram Soc, Westerville, OH, 1975.
33. The oxidation of NiAl. 3. Internal and intergranular oxidation10.1016/0010-938X(94)90107-4 ↗
34. Sulfidation behaviour of nickel aluminides10.1002/maco.19960471204 ↗
35. Accelerated oxidation, internal oxidation, intergranular oxidation, and pesting of intermetallic compounds10.1007/BF01046726 ↗
36. Influence of sulfides on oxidation behavior of nickel-base alloys10.1007/BF03037874 ↗
37. Non-protective alumina growth in sulfur-doped NiAl(Zr)10.1179/mht.2000.012 ↗
38. Hot corrosion of alumina10.1557/JMR.1993.1964 ↗
39. Solubility of α-Al2O3 in fused Na2SO4 at 1200K10.1149/1.2113944 ↗
40. The influence of electrode potential on the corrosion of gas-turbine alloys in sulfate melts10.1007/BF00662038 ↗
41. Inhibition of hot corrosion by MgSO4 and BaSO4 and its potential dependence10.1002/maco.19840350402 ↗
42. Solubilities of Cr2O3 in fused Na2SO4 at 1200K10.1149/1.2108648 ↗
43. Solubility of metal oxides under control of basicity by electrolysis in fused Na2SO410.2320/matertrans.45.2994 ↗
44. Protective coatings—purpose, role, and design10.1179/mst.1986.2.3.194 ↗
45. D.L. Ellis, Hot corrosion of the B2 nickel aluminides, CR191082, NASA (1993).
46. J.A. Nesbitt, Hot corrosion of single-crystal NiAl-X alloys, TM113128, NASA (1998).
47. Effect of composition on the oxidation and hot corrosion resistance of NiAl doped with precious metals10.1016/S0257-8972(00)00878-1 ↗
48. Hot corrosion resistance of nickel-chromium-aluminum alloys10.1149/1.2131427 ↗
49. Kinetics of the low-temperature hot corrosion of Co–Cr–Al alloys10.1149/1.2114105 ↗
50. Acidic and basic fluxing of Ni-base superalloys in a 90Na2SO4–10K2SO4 melt at 1173K10.1007/BF00666645 ↗
51. Kofstad · 1988 · 489