Abstract

Abstract The spatial and crystallographic orientations of facets formed during stress corrosion cracking of Ti–8Al–1Mo–1V have been characterized using quantitative fractography and electron backscatter diffraction. The results indicate that most facets are formed nearly perpendicular to the loading direction on irrational { h k i l } planes. The facets were imaged with high resolution scanning electron microscopy and were found to contain evidence of localized plastic flow despite their “brittle” appearance at moderate magnification. Some fracture planes were related to titanium hydride habit planes, however, the mechanism of faceted growth does not appear to involve hydride nucleation, growth, and fracture, but rather hydrogen enhanced localized plasticity.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Fundamentals
2. Lütjering · 2003
3. Titanium alloys
4. Curtis · Trans. ASM · 1969 · 62 · 457
5. Metallurgical aspects of the stress corrosion cracking of titanium alloys
6. The influence of oxygen concentration on the internal stress and dislocation arrangements in α titanium10.1007/BF02652870 ↗
7. Deformation behavior of HCP Ti–Al alloy single crystals10.1007/s11661-002-0153-y ↗
8. An analysis of frequency and amplitude effects on corrosion fatigue crack propagation in Ti–8Al–1Mo–1V10.1007/BF02662746 ↗
9. The relationship between crystallographic texture and salt water cracking susceptibility in Ti–6Al–4V10.1016/0921-5093(95)09820-8 ↗
10. Strain rate dependent environment assisted cracking of α/β–Ti alloys in chloride solution
11. Electron fractography – a tool for the study of micromechanisms of fracturing processes
12. Stress corrosion cracking mechanism of Ti–6Al–4V in acidic methanol10.5006/1.3585078 ↗
13. Internal hydrogen-induced subcritical crack growth in Ti–6Al–4V10.1016/S1359-6462(97)00046-8 ↗
14. Hydrogen-induced subcritical crack growth in Ti–6Al–4V alloy10.1016/S0921-5093(97)00506-6 ↗
15. I.M. Robertson, H.K. Birnbaum, Dislocation mobility and hydrogen – a brief review, in: Proc. 11th International Conference on Fracture. , 2009 (accessed 19.12.09).
16. Shih · Acta Metall. · 1988 · 36 · 11110.1016/0001-6160(88)90032-6 ↗
17. Hydride formation
18. Crystallography of fatigue crack initiation and growth in fully lamellar Ti–6Al–4V10.1007/s11661-009-0064-2 ↗
19. Fractography and its role in fracture interpretation, fatigue and fracture of Egr.10.1111/j.1460-2695.1996.tb00168.x ↗
20. A Review of microstructure effects on hydrogen-induced sustained load cracking in structural titanium alloys
21. Environmental cracking behavior of Ti–6Al–6V–2Sn: influence of alloy chemistry
22. Relationship between composition, microstructure, and stress-corrosion cracking (in salt solution) in titanium alloys
23. A.L. Pilchak, Ph.D. Dissertation, The Ohio State University, Department of Materials Science and Engineering, 2009.
24. A.L. Pilchak, J.C. Williams, Observations on the role of hydrogen in facet formation in near-α titanium, Metall. Mater. Trans. A, in press.
25. Effect of hydrogen on fracture and inert-environment sustained load cracking resistance of α-β titanium alloys10.1007/BF02644024 ↗
26. Hydride habit planes in titanium–aluminum alloys10.1007/BF02817895 ↗
27. Determining fracture facet crystallography using backscatter patterns and quantitative tilt fractography10.1557/JMR.1993.2482 ↗
28. Crystallography of fracture facets in a near-alpha titanium alloy10.1007/s11661-006-0144-5 ↗
29. Determination of crystallographic orientation of dwell-fatigue facture facets in Ti-6242 alloy10.1007/s10853-006-0252-z ↗
30. Uncertainty in the determination of fatigue facet crystallography10.1016/j.scriptamat.2004.10.040 ↗
31. Observations on the faceted initiation site in the dwell-fatigue tested Ti-6242 alloy: crystallographic orientation and size effects10.1007/s11661-006-0095-x ↗
32. The origins of heterogeneous deformation during primary hot working of Ti–6Al–4V10.1016/S0749-6419(01)00057-2 ↗
33. Investigation of the fracture mechanism of Ti–5Al–2.5Sn at cryogenic temperatures10.1007/BF02646411 ↗
34. Crystallography of fluted fracture in near-α titanium alloys10.1007/s11661-009-0091-z ↗
35. Comments on the electron fractography of α-titanium10.1007/BF02661765 ↗
36. Chesnutt · 1976
37. Low ΔK faceted crack growth in titanium alloys10.1016/j.ijfatigue.2008.03.036 ↗
38. Deformation and creep modeling in polycrystalline Ti–6Al alloys10.1016/S1359-6454(03)00289-1 ↗
39. Suresh · 1998