A study of the film formation kinetics on zinc in different acidic corrosion inhibitor solutions by quartz crystal microbalance
Source abstract
Abstract
Chromates conversion coatings provide very effective corrosion protection for many metals. However, the high toxicity of chromate leads to an increasing interest in using non-toxic alternatives such as molybdates, silicates, rare earth metal ions and etc. In this work, quartz crystal microbalance (QCM) was applied as an in-situ technique to follow the film formation process on zinc (plated on gold) in acidic solutions containing an inorganic inhibitor, i.e. potassium chromate, sodium silicate, sodium molybdate or cerium nitrate. Using an equation derived in this work, the interfacial mass change during the film formation process under different conditions was calculated, indicating three different film formation mechanisms. In the presence of K2CrO4 or Na2SiO3, the film growth follows a mix-parabolic law, showing a process controlled by both ion diffusion and surface reaction. The apparent kinetic equations are 0.4t = -17.4 + 20 Delta m(f) + (Delta m(f))(2) and 0.1t = 19.0 + 8.4 Delta m(f) + 10(Delta m(f))(2) respectively (t and Delta m are in seconds and mu g/cm(2)). In solutions containing Na2MoO4, a logarithmic law of Delta m(f) = -24.7 + 6.6 ln t was observed. Changing the inhibitor to Ce(NO3)(3), the film growth was found to obey an asymptote law that could be fit into the equation of Delta m(f) 55.1(1 - exp(-2.6 x 10(t)(-3))). (C) 2004 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Acoustic Wave Resonator Technologies · Corrosion Behavior and Inhibition · Ferroelectric and Piezoelectric Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Hinton · Metal Finish. · 1991 · 89 · 55
2. Hinton · Metal Finish. · 1991 · 89 · 15
3. Wilcox · Trans. IMF · 1997 · 75 · B140
4. Wilcox · Metal Finish. · 1988 · 86 · 71
5. Wilcox · Br. Corros. J. · 1987 · 22 · 25410.1179/000705987798271244 ↗
6. Wilcox · Trans. IMF · 1997 · 75 · B140
7. Hinton · J. Alloy Compd. · 1992 · 75 · 1510.1016/0925-8388(92)90359-H ↗
8. Bethencourt · Corros. Sci. · 1998 · 40 · 180310.1016/S0010-938X(98)00077-8 ↗
9. Wharton · Trans. IMF · 1999 · 77 · 15210.1080/00202967.1999.11871272 ↗
10. Aramaki · Corros. Sci. · 2001 · 43 · 59110.1016/S0010-938X(00)00085-8 ↗
11. Aramaki · Corros. Sci. · 2001 · 43 · 220110.1016/S0010-938X(00)00189-X ↗
12. Aramaki · Corros. Sci. · 2001 · 43 · 157310.1016/S0010-938X(00)00144-X ↗
13. Birks · 1983
14. Jones · 1992
15. Ward · Science · 1990 · 249 · 100010.1126/science.249.4972.1000 ↗
16. Forslund · J. Electrochem. Soc. · 1996 · 143 · 83910.1149/1.1836546 ↗
17. Forslund · J. Electrochem. Soc. · 1997 · 144 · 263710.1149/1.1837876 ↗
18. Yan · Electrochim. Acta · 2000 · 45 · 281510.1016/S0013-4686(00)00385-6 ↗
19. Buttry · Chem. Rev. · 1992 · 92 · 135510.1021/cr00014a006 ↗
20. Seo · Mater. Sci. Forum. · 1995 · 192–194 · 75510.4028/www.scientific.net/MSF.192-194.755 ↗
21. Chandler · Corrosion · 1991 · 47 · 17910.5006/1.3585241 ↗
22. Zucchi · J. Appl. Electrochem. · 1998 · 28 · 44110.1023/A:1003252824931 ↗
23. Szocs · J. Appl. Electrochem. · 1999 · 29 · 133910.1023/A:1003869715760 ↗
24. Gan · Corros. Sci. · 2000 · 42 · 137910.1016/S0010-938X(00)00007-X ↗
25. Wu · J. Electroanal. Chem. · 1994 · 374 · 9710.1016/0022-0728(94)03345-5 ↗
26. Bruckenstein · Electrochim. Acta · 1985 · 30 · 129510.1016/0013-4686(85)85005-2 ↗
27. Sauerbrey · Z. Phys. · 1959 · 155 · 20610.1007/BF01337937 ↗
28. Cai · J. Electrochem. Soc. · 1996 · 143 · 212510.1149/1.1836970 ↗
29. Song · Mater. Protect. · 1998 · 31 · 1
30. Evans · 1960
31. Han · Corros. Sci. Protect. Technol. · 1997 · 9 · 167
32. Zhang · 1986
33. Jones · Corrosion · 1965 · 21 · 29510.5006/0010-9312-21.9.295 ↗