Abstract
Abstract The effects of vacuum annealing and laser remelting on the microstructure and corrosion behaviour of plasma-sprayed Ni-coated WC coatings on steel substrate have been investigated. The laser remelting was operated in a continuous way while the vacuum annealing was operated with clamping the coating on the graphite face in order to avoid decarburization of WC. When compared with the as-sprayed coating, the microstructure of the post-heating treatment coatings has been found to consist of different phases. Moreover, the denser microstructure can be obtained after heating treatment, especially the laser remelting coating. Electron probe micro analyzer (EPMA) shows that the chemical composition remained largely unchanged except the “bumps” at the interface for as-sprayed and vacuum annealing coatings. The more uniform composition was obtained for laser remelting coating. The Vickers microhardness measurement shows a very slightly enhancement for post-heating treatment coatings, which may be duo to the lamellar structure, lower contemt and bulky of carbide for coatings. However, salt spray corrosion (SSC) show the laser remelting coating has the best corrosion resistance, which is due to its low number defects and uniform distribution of the phase and composition.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Mateos · Wear · 2000 · 239 · 27410.1016/S0043-1648(00)00325-2 ↗
2. Wännstrand · Surface & Coatings Technology · 1999 · 111 · 24710.1016/S0257-8972(98)00821-4 ↗
3. Vamsi Krishna · International Journal of Refractory Metals & Hard Materials · 2002 · 20 · 35510.1016/S0263-4368(02)00073-2 ↗
4. Roth · Surface & Coatings Technology · 1995 · 74–75 · 63710.1016/0257-8972(95)08338-3 ↗
5. Thermal Spray Coatings, Friction, Lubrication and Wear Technology
6. Protective coatings and their processing thermal spray
7. Hocking · 1989
8. McPherson · Surface & Coatings Technology · 1989 · 39/40 · 17310.1016/0257-8972(89)90052-2 ↗
9. Lim · Surface & Coatings Technology · 1996 · 79 · 15110.1016/0257-8972(95)02437-9 ↗
10. Guo · Surface & Coatings Technology · 1995 · 73 · 7310.1016/0257-8972(94)02364-6 ↗
11. Fernánder · Tribology International · 1996 · 29 · 47710.1016/0301-679X(95)00106-E ↗
12. Fu · Wear · 1997 · 210 · 15710.1016/S0043-1648(97)00058-6 ↗
13. Mateos · Wear · 2000 · 239 · 27410.1016/S0043-1648(00)00325-2 ↗
14. Yu · Surface & Coatings Technology · 2004 · 182 · 30810.1016/j.surfcoat.2003.08.065 ↗
15. Jiang · Materials Engineering · 1999 · 1 · 46
16. Razavy · Materials Science and Engineering · 2003 · A362 · 21310.1016/S0921-5093(03)00571-9 ↗
17. Hidouci · Surface & Coatings Technology · 2000 · 123 · 1710.1016/S0257-8972(99)00394-1 ↗
18. Wang · Wear · 1994 · 174 · 17710.1016/0043-1648(94)90105-8 ↗
19. Syewart · Surface & Coatings Technology · 1998 · 105 · 1310.1016/S0257-8972(98)00444-7 ↗
20. Zhao · Surface & Coatings Technology · 2005 · 190 · 29310.1016/j.surfcoat.2004.04.057 ↗
21. Oliveira · Corrosion Science · 2000 · 42 · 188110.1016/S0010-938X(00)00041-X ↗
22. Cavaleiro · 1998 · 233
23. Brett · Thin Solid Films · 1998 · 322 · 26310.1016/S0040-6090(97)00916-4 ↗
24. Toma · Surface & Coatings Technology · 2001 · 138 · 14910.1016/S0257-8972(00)01141-5 ↗