Probing corrosion initiation at interfacial nanostructures of AA2024-T3
Source abstract
Abstract
High-strength aluminium alloys such as AA2024-T3 are often developed by the introduction of plastic deformation to a precipitate containing microstructure. These alloys contain complex, near-surface nanostructures whose effects on localised corrosion processes have not been well understood due primarily to the difficulty of characterising these heterogeneous compositions and structures. In this work, we observed entangled oxide networks co-located with dislocation structures piled up at corroded intermetallic particles of an AA2024-T3 alloy. It was revealed that dislocation arrays act as pathways for corrosive species and promote structural degradation at interfacial regions, providing a new insight into corrosion initiation at the nano-scale.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Nanostructural hierarchy increases the strength of aluminium alloys10.1038/ncomms1062 ↗
2. Nanostructure of aluminium alloy 2024: segregation, clustering and precipitation processes10.1016/j.actamat.2010.11.033 ↗
3. Linear complexions: confined chemical and structural states at dislocations10.1126/science.aab2633 ↗
4. Passivity breakdown pit initiation and propagation of pits in metallic materials – review10.1016/j.corsci.2014.10.006 ↗
5. Understanding localized corrosion10.1016/S1369-7021(08)70206-2 ↗
6. Microstructure and corrosion of AA202410.1515/corrrev-2014-0039 ↗
7. Investigation of dealloying by ultra-high-resolution nanotomography10.1002/sia.5176 ↗
8. Passive films at the nanoscale10.1016/j.electacta.2012.03.158 ↗
9. Mechanism of localized breakdown of 7000 series aluminum alloys10.1149/2.080310jes ↗
10. Role of nanostructure in pitting of Al-Cu-Mg alloys10.1016/j.electacta.2010.02.001 ↗
11. Nano-scale dissolution phenomena in Al-Cu-Mg alloys10.1016/j.elecom.2007.10.032 ↗
12. Retrogression and reaging and the role of dislocations in the stress corrosion of 7000-type aluminum alloys10.1007/BF02650294 ↗
13. Observations of intergranular corrosion in AA2024-T351: the influence of grain stored energy10.1016/j.corsci.2012.04.005 ↗
14. Grain-stored energy and the propagation of intergranular corrosion in AA2xxx aluminium alloys10.1002/sia.5218 ↗
15. Defect density associated with constituent particles in AA2024-T3 and its role in corrosion
16. Multiple twins of a decagonal approximant embedded in S-Al2CuMg phase resulting in pitting initiation of a 2024 Al alloy10.1016/j.actamat.2014.09.001 ↗
17. Strain-induced preferential dissolution at the dislocation emergences in MnS: an atomic scale study10.1080/14786435.2015.1052030 ↗
18. Investigation of microstructure and corrosion behavior of burnished aluminum alloy by TEM, EWF, XPS and EIS techniques10.1016/j.materresbull.2016.05.013 ↗
19. Nano-scale dissolution phenomena in Al–Cu–Mg alloys10.1016/j.elecom.2007.10.032 ↗
20. Local dissolution phenomena associated with S Phase(Al2CuMg)Particles in aluminum alloy 2024-T310.1149/1.1837874 ↗
21. Early stages during localized corrosion of AA2024 TEM specimens in chloride environment10.1002/sia.5193 ↗
22. Quasi in situ analytical TEM to investigate electrochemically induced microstructural changes in alloys: AA2024-T3 as an example10.1016/j.corsci.2012.12.006 ↗
23. Ultramicrotomy—a route towards the enhanced understanding of the corrosion and filming behaviour of aluminium and its alloys10.1016/S0010-938X(98)00006-7 ↗
24. Study of localized corrosion in AA2024 aluminium alloy using electron tomography10.1016/j.corsci.2012.02.001 ↗
25. In situ scanning tunneling microscopy study of grain-dependent corrosion on microcrystalline copper10.1021/jp507089f ↗
26. Atom probe tomography study of the nanoscale heterostructure around an Al20Mn3Cu2 dispersoid in aluminum alloy 202410.1021/la503418u ↗
27. Miller · 2014
28. Atom probe study of chromium oxide spinels formed during intergranular corrosion10.1016/j.scriptamat.2014.09.028 ↗
29. Atom probe tomography of stress corrosion crack tips in SUS316 stainless steels10.1016/j.corsci.2015.06.008 ↗
30. How the crystallography and nanoscale chemistry of the metal/oxide interface develops during the aqueous oxidation of zirconium cladding alloys10.1016/j.actamat.2012.09.021 ↗
31. EELS and atom probe tomography study of the evolution of the metal/oxide interface during zirconium alloy oxidation10.1016/j.jnucmat.2015.03.043 ↗
32. A guide on FIB preparation of samples containing stress corrosion crack tips for TEM and atom-probe analysis10.1016/j.micron.2007.12.003 ↗
33. Chapter 9 – recrystallization of two-phase alloys
34. Effect of impurities on the recrystallization texture in commercially pure copper-ETP wires10.1016/j.msea.2006.11.137 ↗
35. Deformation induced grain boundaries in commercially pure aluminium10.1016/S1359-6454(00)00138-5 ↗
36. Gault · 2012
37. Analysis of three-dimensional atom-probe data by the proximity histogram10.1007/S100050010051 ↗
38. A filtering method to reveal crystalline patterns from atom probe microscopy desorption maps10.1016/j.mex.2016.03.012 ↗
39. Investigation of dealloying of S phase (Al2CuMg) in AA 2024-T3 aluminium alloy using high resolution 2D and 3D electron imaging10.1016/j.corsci.2015.11.013 ↗
40. Dealloying and corrosion of Al alloy 2024 - T 310.1149/1.1498258 ↗
41. Corrosion of AA2024-T3 part II: Co-operative corrosion10.1016/j.corsci.2010.09.030 ↗
42. HRTEM and HAADF-STEM tomography investigation of the heterogeneously formed S (Al2CuMg) precipitates in Al–Cu–Mg alloy10.1080/14786435.2012.762469 ↗
43. Dislocation core radii near elastic stability limits10.1103/PhysRevB.87.134106 ↗
44. The mechanism of water diffusion in narrow carbon nanotubes10.1021/nl052254u ↗
45. Generation of hydrogen from aluminum and water – effect of metal oxide nanocrystals and water quality10.1016/j.ijhydene.2011.08.077 ↗
46. Three-dimensional atomic-scale imaging of impurity segregation to line defects10.1126/science.286.5448.2317 ↗
47. Studies of dislocations by field ion microscopy and atom probe tomography10.1080/14786435.2013.818257 ↗