In situ monitoring of crevice corrosion morphology of Type 316L stainless steel and repassivation behavior induced by sulfate ions
Source abstract
Abstract
Abstract To analyze the repassivation mechanism induced by SO42− ions, in situ monitoring of the crevice corrosion morphology on Type 316L stainless steel was performed. The repassivation of the crevice corrosion was observed when the solution was changed from 1 M NaCl to 0.88 M Na2SO4 or to 1 M NaCl-0.88 M Na2SO4. The active dissolution of Type 316L stainless steel was suppressed by SO42− ions at pH 0.4 in anodic polarization measurements. The transition from active to passive states inside the crevice was likely promoted by SO42− ions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Anodic Oxide Films and Nanostructures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. On the roles of corrosion products in local cell processes10.5006/1.3584892 ↗
2. The significance of the local electrode potential within pits, crevices and cracks
3. Crevice corrosion of stainless steels. I. A mathematical model10.1179/000705978798358671 ↗
4. Visualization of pH and pCl distributions: initiation and propagation criteria for crevice corrosion of stainless steel10.1149/2.019207jes ↗
5. Simultaneous visualization of pH and Cl− distributions inside the crevice of stainless steel10.1016/j.corsci.2016.01.028 ↗
6. Application of chemical imaging sensor to in-situ pH imaging in the vicinity of a corroding metal surface10.1016/j.electacta.2015.07.184 ↗
7. Effect of ionic inter actions on the initiation of crevice corrosion in passive metals10.1149/1.1852433 ↗
8. A critical crevice solution and IR drop crevice corrosion model10.1016/j.corsci.2008.02.020 ↗
9. An arbitrary Lagrangian-Eulerian model for modelling the time-dependent evolution of crevice corrosion10.1016/j.corsci.2013.10.003 ↗
10. IR mechanism of crevice corrosion for Alloy T-2205 duplex stainless steel in acidic-chloride media10.1149/1.1380673 ↗
11. Important early developments and current understanding of the IR mechanism of localized corrosion10.1149/1.1565142 ↗
12. Behaviour of crevice corrosion in iron10.1016/j.corsci.2004.08.001 ↗
13. Measurement of pH gradients in the crevice corrosion of Iron using a Palladium Hydride microelectrode10.1149/1.1851053 ↗
14. IR voltage switch in delayed crevice corrosion and active peak formation detected using a repassivation-type scan10.1016/j.electacta.2004.12.017 ↗
15. Microprobe study of pH during the induction period preceding crevice corrosion10.1149/1.2139868 ↗
16. Pitting on the crevice wall prior to crevice corrosion: iron in sulfate/chromate solution10.1016/j.electacta.2010.10.013 ↗
17. Temperature and potential dependence of crevice corrosion of AISI 316 stainless steel10.1016/S0010-938X(00)00167-0 ↗
18. The determination of pH, potential and chloride concentration in corroding crevices on 304 stainless steel and 7475 aluminium alloy10.1016/0010-938X(87)90088-6 ↗
19. Effect of Applied potential on changes in solution chemistry inside crevices on Type 304L stainless steel and Alloy 82510.5006/1.3293476 ↗
20. Applicability of repassivation potential for long-Term prediction of localized corrosion of alloy 825 and type 316L stainless steel10.5006/1.3316014 ↗
21. Sedriks · 1996 · 180
22. Crevice corrosion of metallic materials
23. Cathodic protection to prevent crevice corrosion of stainless steels in halide media10.5006/0010-9312-29.1.28 ↗
24. Significance of protection potential in pitting and intergranular corrosion10.5006/0010-9312-26.10.431 ↗
25. A study on cathodic protection against crevice corrosion in dilute NaCl solutions10.1016/S0010-938X(01)00042-7 ↗
26. Pitting corrosion evaluation and inhibition of stainless steels: a review
27. Influence of alloy sulfur content and bulk electrolyte composition on crevice corrosion initiation of austenitic stainless steel10.5006/1.3284838 ↗
28. A competitive adsorption model for the inhibition of crevice corrosion and pitting10.1149/1.2086294 ↗
29. Growth of corrosion pits on stainless steel in chloride solution containing dilute sulphate10.1016/0010-938X(92)90191-5 ↗
30. The effects of some anions on metastable pitting of 316L stainless steel10.1016/S0010-938X(01)00031-2 ↗
31. Localized corrosion of passive metals
32. The initiation of crevice corrosion in stainless steels10.1016/S0010-938X(97)00050-4 ↗
33. Studies on accumulation of chloride ions in pits growing during anodic polarization
34. Studies on accumulation of chloride ions in pits growing during anodic polarization10.1016/0010-938X(75)90015-3 ↗
35. Composition of anolyte within pit anode of austenitic stainless steels in chloride solution10.5006/0010-9312-29.1.18 ↗
36. Effect of sulfate on the passive and crevice corrosion properties of Alloy 22 in 4M sodium chloride10.5006/1.3280666 ↗
37. Direct evidence of the potential distribution in crevices10.1016/0010-938X(92)90112-G ↗
38. In situ investigation of crevice corrosion on UNS S32101 duplex stainless steel in sodium chloride solution10.1016/j.corsci.2013.06.039 ↗
39. 2000 W.R. whitney award lecture: visualizing corrosion10.5006/1.3294386 ↗
40. Estimation of crevice corrosion life time for stainless steels in seawater environments
41. The evolution of crevice corrosion damage on the Ni-Cr-Mo-W alloy-22 determined by confocal laser scanning microscopy10.1016/j.corsci.2011.09.028 ↗
42. Influence of ultrasound on pitting corrosion and crevice corrosion of SUS304 stainless steel in chloride sodium aqueous solution10.1016/j.corsci.2007.11.001 ↗
43. The solution composition and electrode potential in pits, crevices and cracks10.1016/0010-938X(83)90014-8 ↗
44. Effects of Cl−, NO3− and SO42− anions on the anodic behavior of carbon steel in deaerated 0.50M NaHCO3 solutions10.1016/j.apsusc.2005.08.025 ↗
45. Szklarska-Smialowska · 1986 · 296
46. Electrochemical corrosion characteristics of type 316 stainless steel in simulated anode environment for PEMFC10.1016/S0013-4686(03)00113-0 ↗
47. Conductometry
48. The temperature coefficient of conductance for the alkali metal halide, tetraalkylammonium, halate, and perhalate ions in D2O10.1007/BF00650531 ↗