Monitoring of atmospheric corrosion and dewing process by interlacing copper electrode sensor
Source abstract
Abstract
Abstract A novel dewing sensor consisting of two interlacing (comb-like) copper electrodes was fabricated by photolithography to monitor the formation and evaporation process of thin electrolyte layer (TEL), as well as atmospheric corrosion of copper during wetting-drying and high-low temperature cyclic tests. Thanks to the ultra-narrow space between the comb-like electrodes, the sensor can probe earlier dew condensation on Cu even at low relative humidity. Moreover, the thickness of TEL can be easily calculated based on high-frequency impedance during the drying process of TEL.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Analytical Chemistry and Sensors · Gas Sensing Nanomaterials and Sensors · Acoustic Wave Resonator Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. The effects of Cl− ion concentration and relative humidity on atmospheric corrosion behaviour of Pcb-Cu under adsorbed thin electrolyte layer10.1016/j.corsci.2010.12.018 ↗
2. Effect of direct current electric field on atmospheric corrosion behavior of copper under thin electrolyte layer10.1016/j.corsci.2011.04.017 ↗
3. Eis study on aerobic corrosion of copper in ground water: influence of micro-organisms10.1016/j.electacta.2017.04.073 ↗
4. Electrochemical aspects of copper atmospheric corrosion in the presence of sodium chloride10.1016/j.electacta.2018.04.184 ↗
5. The effects of temperature and electric field on atmospheric corrosion behaviour of Pcb-Cu under absorbed thin electrolyte layer10.1016/j.corsci.2011.01.031 ↗
6. Effect of an alternating electric field on the atmospheric corrosion behaviour of copper under a thin electrolyte layer10.1016/j.corsci.2013.05.019 ↗
7. Electrochemical corrosion behaviour of copper under periodic wet–dry cycle condition10.1016/j.microrel.2013.05.002 ↗
8. Atmospheric corrosion monitoring of a weathering steel under an electrolyte film in cyclic wet–dry condition10.1016/j.corsci.2013.09.008 ↗
9. Electrochemical impedance study on galvanized steel corrosion under cyclic wet–dry conditions––influence of time of wetness10.1016/S0010-938X(03)00130-6 ↗
10. Corrosion monitoring
11. Application of Fe-C coated Lpfg sensor for early stage corrosion monitoring of steel bar in Rc structures10.1016/j.conbuildmat.2018.04.187 ↗
12. Data mining to online galvanic current of zinc/copper internet atmospheric corrosion monitor10.1016/j.corsci.2018.02.005 ↗
13. Electrochemical monitoring of atmospheric corrosion phenomena10.1016/0010-938X(76)90052-4 ↗
14. Laboratory studies of atmospheric corrosion—I. Weight loss and electrochemical measurements10.1016/0010-938X(80)90119-5 ↗
15. Corrosion monitoring and materials selection for automotive environments by using atmospheric corrosion monitor (Acm) sensor10.1016/j.corsci.2014.02.020 ↗
16. Schindelholz · 2012 · 135
17. Time of wetness in tropical climate: considerations on the estimation of tow according to Iso 9223 standard10.1016/j.corsci.2007.06.012 ↗
18. Electrochemical measurements of time-of-Wetness and atmospheric corrosion rates10.5006/0010-9312-33.1.13 ↗
19. Long-term corrosion of rebars embedded in aerial and hydraulic binders mechanisms and crucial physico-chemical parameters10.1016/j.corsci.2008.03.017 ↗
20. Comparability and accuracy of time of wetness sensing methods relevant for atmospheric corrosion10.1016/j.corsci.2012.10.026 ↗
21. Potential distribution measurement in galvanic corrosion of Zn/Fe couple by means of kelvin probe10.1016/S0010-938X(99)00074-8 ↗
22. Scanning kelvin probe for detection of the hydrogen induced by atmospheric corrosion of ultra-high strength steel10.1016/j.electacta.2016.08.122 ↗
23. Potentiometric measurement with a kelvin probe: contactless measurement of chloride ions in aqueous electrolyte10.1016/j.snb.2016.06.150 ↗
24. Lateral resolution in scanning kelvin probe microscopy10.1016/j.corsci.2015.09.008 ↗
25. In situ Qcm and Tm-Afm investigations of the early stages of degradation of silver and copper surfaces10.1016/j.apsusc.2006.08.005 ↗
26. Corrosion monitoring in archives by the electrical resistance technique10.1016/j.culher.2013.04.002 ↗
27. Copper corrosion monitoring by electrical resistance probes in anoxic groundwater environment in the presence and absence of sulfate reducing bacteria10.1016/j.sna.2018.03.018 ↗
28. Investigation of atmospheric corrosion of Zn using Ac impedance and differential pressure meter10.1016/j.electacta.2004.01.033 ↗
29. Electrochemical corrosion monitoring of galvanized steel under cyclic wet–dry conditions10.1016/S0010-938X(99)00057-8 ↗
30. Ac impedance study on corrosion of 55%Al–Zn alloy-coated steel under thin electrolyte layers10.1016/S0010-938X(00)00009-3 ↗
31. Corrosion monitoring of nickel-containing steels in marine atmospheric environment10.1016/j.corsci.2004.10.009 ↗
32. Screen-printed atmospheric corrosion monitoring sensor based on electrochemical impedance spectroscopy10.1016/j.snb.2009.03.027 ↗
33. Eis monitoring study of atmospheric corrosion under variable relative humidity10.1016/j.corsci.2010.07.018 ↗
34. Late pleistocene loess-like deposits in the coastal area of South China10.1016/j.catena.2018.04.032 ↗
35. In-situ investigation of atmospheric corrosion behavior of bronze under thin electrolyte layers using electrochemical technique10.1016/S1003-6326(11)61311-3 ↗
36. Corrosion of pure magnesium under thin electrolyte layers10.1016/j.electacta.2008.05.074 ↗
37. Corrosion behaviour of copper under chloride-containing thin electrolyte layer10.1016/j.corsci.2011.06.004 ↗
38. The corrosion of tin under thin electrolyte layers containing chloride10.1016/j.corsci.2012.08.040 ↗
39. The atmospheric corrosion of zinc: the effects of salt concentration, droplet size and droplet shape10.1016/j.electacta.2010.09.099 ↗
40. Multiscale modelling of the corrosion of metals under atmospheric corrosion10.1016/j.electacta.2010.10.025 ↗
41. An integrated modeling approach for atmospheric corrosion in presence of a varying electrolyte film10.1016/j.electacta.2015.11.010 ↗
42. Influence of environmental factors on atmospheric corrosion in dynamic environment10.1016/j.corsci.2018.03.042 ↗
43. Atmospheric corrosion factors of printed circuit boards in a dry-heat desert environment: salty dust and diurnal temperature difference10.1016/j.cej.2017.11.017 ↗
44. The role of Uv illumination on the Nacl-induced atmospheric corrosion of Q235 carbon steel10.1016/j.corsci.2014.06.013 ↗
45. Advantage of super-hydrophobic surface as a barrier against atmospheric corrosion induced by salt deliquescence10.1016/j.corsci.2014.09.001 ↗
46. Atmospheric corrosion initiation on steel from predeposited Nacl salt particles in high humidity atmospheres, corrosion engineering
47. The role of electrochemical polarization in micro-droplets formation10.1016/j.elecom.2008.09.010 ↗
48. The effect of relative humidity on the atmospheric corrosion of defective organic coating materials: an Eis study with a new approach10.1016/S0010-938X(99)00126-2 ↗
49. The influence of relative humidity and temperature on the acetic acid vapour-induced atmospheric corrosion of lead10.1016/j.corsci.2008.08.009 ↗
50. Influence of relative humidity and ozone on atmospheric silver corrosion10.1016/j.corsci.2013.07.028 ↗
51. Formation and growth of micro-droplets during the initial stage of atmospheric corrosion10.1016/j.electacta.2004.01.032 ↗
52. An application of electrochemical impedance spectroscopy to atmospheric corrosion study10.1016/0010-938X(95)00002-2 ↗
53. Salt concentration dependence of ionic conductivity in ion exchange membranes10.1016/j.memsci.2017.10.024 ↗