Effect of hypersonic flow chemical composition on the oxidation behavior of a super-strong UHTC
Source abstract
Abstract
A super-strong ZrB2 ceramic containing WC and SiC was tested in a supersonic arc-jet wind tunnel by exposure to flows with two chemical compositions, simulated air or pure nitrogen, at temperatures of 2650 and 2800 K. Temperature jumps of 500-600 K were observed in both environments at constant flow conditions. SEM analyses revealed that oxygen in the high-enthalpy flow retards the material consumption owing to the formation of partially protective glass. Then, it appears that even 5 vol% of W-compounds is sufficient to modify the subscale oxide configuration and form a cell-like multi-layered architecture typical of tungsten, rather than that typical of ZrB2.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. 2014
2. Aero-thermo-chemical characterization of ultra-high-temperature ceramics for aerospace applications10.1016/j.jeurceramsoc.2017.12.043 ↗
3. Formation of tough interlocking microstructure in ZrB2–SiC based ultra high temperature ceramics by pressureless sintering10.1557/jmr.2009.0274 ↗
4. Chemical Reactions, Anisotropic Grain Growth and Sintering Mechanisms of Self-Reinforced ZrB2–SiC Doped with WC10.1111/j.1551-2916.2010.04278.x ↗
5. Combined effects of WC and SiC on densification and thermo-mechanical stability of ZrB2 ceramics10.1016/j.matdes.2016.06.114 ↗
6. Microstructure evolution of a W-doped ZrB2 ceramic upon high-temperature oxidation10.1111/jace.14738 ↗
7. Thermoablative resistance of ZrB2-SiC-WC ceramics at 2400 °C10.1016/j.actamat.2017.05.033 ↗
8. Strong ZrB2-SiC-WC ceramics at 1600 °C10.1111/j.1551-2916.2011.05062.x ↗
9. Role of WC additive on reaction, solid-solution and densification in HfB2–SiC ceramics10.1016/j.jeurceramsoc.2013.10.007 ↗
10. Core-shell structure: an effective feature for strengthening ZrB2 ceramics10.1016/j.scriptamat.2018.09.024 ↗
11. Oxidation of ZrB2 and ZrB2-SiC ceramics with tungsten additions
12. Thermal and electrical transport in ZrB2-SiC-WC ceramics up to 1800 °C10.1016/j.actamat.2017.02.052 ↗
13. Segregation of tungsten atoms at ZrB2 grain boundaries in strong ZrB2-SiC-WC ceramics10.1016/j.scriptamat.2018.07.038 ↗
14. Thermoablative resistance of ZrB2–SiC–WC ceramics at 2400 °C10.1016/j.actamat.2017.05.033 ↗
15. Effect of an SiC addition on the oxidation of ZrB2
16. Oxidation of ZrB2-SiC: influence of SiC content on solid and liquid oxide phase formation10.1111/j.1551-2916.2008.02874.x ↗
17. Oxidation of ZrB2–SiC ultra-high temperature composites over a wide range of SiC content10.1016/j.jeurceramsoc.2012.05.021 ↗
18. Oxidation mechanism and resistance of ZrB2–SiC composites10.1016/j.corsci.2009.07.005 ↗
19. Effects of oxygen partial pressure and atomic oxygen on the microstructure of oxide scale of ZrB2–SiC composites at 1500 °C10.1016/j.corsci.2013.03.023 ↗
20. Effects of transition metals on the oxidation behavior of ZrB2 ceramics10.1016/j.corsci.2014.11.019 ↗
21. Super-strong materials for temperatures exceeding 2000 °C10.1038/srep40730 ↗
22. Microstructure evolution of a W-doped ZrB2 ceramic upon high-temperature oxidation10.1111/jace.14738 ↗
23. Modeling and evaluating the environmental degradation of UHTCs under hypersonic flow
24. Experimental and computational analysis of thermo‐oxidative‐structural stability of ZrB2–SiC–Ti during arc‐jet testing10.1111/jace.15001 ↗
25. Arc jet testing and evaluation of Mo–Si–B coated Mo and SiC–ZrB2 ceramics10.1016/j.jeurceramsoc.2014.06.011 ↗
26. Effects of LaB6 addition on arc-jet convectively heated SiC-containing ZrB2-based ultra-high temperature ceramics in high enthalpy supersonic airflows10.1016/j.corsci.2013.06.029 ↗
27. Testing ultra-high-temperature ceramics for thermal protection and rocket applications10.1080/17436753.2018.1509175 ↗
28. Characterization of carbon-fiber reinforced ultra-high-temperature ceramic matrix composites in arc-jet environment
29. Thermo-chemical surface instabilities of SiC-ZrB2 ceramics in high enthalpy dissociated supersonic air flows10.1016/j.jeurceramsoc.2017.01.018 ↗
30. Aerothermal behaviour of a SiC fibre-reinforced ZrB2 sharp component in supersonic regime10.1016/j.jeurceramsoc.2012.01.019 ↗
31. Dynamic oxidation of ultra-high temperature ZrB2–SiC under high enthalpy supersonic flows10.1016/j.corsci.2010.11.018 ↗
32. Arc-jet wind tunnel characterization of ultra-high-temperature ceramic matrix composites10.1016/j.corsci.2018.12.039 ↗
33. Gordon · 1994
34. Siegel · 1978
35. Temperature jump phenomenon during plasmatron testing of ZrB2-SiC ultrahigh-temperature ceramics10.2514/1.T3798 ↗
36. Weil · 2013 · 1
37. The O-W (Oxygen-Tungsten) system10.1007/BF02877593 ↗
38. Thermophysical properties of ZrB2 and ZrB2–SiC ceramics10.1111/j.1551-2916.2008.02268.x ↗
39. On the oxidation mechanism of pure tungsten in the temperature range 600–800 °C10.1016/j.corsci.2011.12.027 ↗
40. Kinetics of oxidation of pure tungsten, 1150°–1615 °C10.1149/1.2426043 ↗
41. Method to improve the oxidation resistance of ZrB2 -based ceramics for reusable space systems10.1016/j.jeurceramsoc.2018.01.025 ↗