journal article·2015-07

Stress corrosion cracking of several solution heat-treated Mg–X alloys

Fuyong Cao, Zhiming Shi, Guang-Ling Song, Ming Liu, Matthew S. Dargusch, Andrej Atrens

Corrosion Science· Volume 96
Publisher page

Abstract

The stress corrosion cracking (SCC) behaviour of solution heat-treated as-cast Mg0.1Zr, Mg1Mn, Mg0.1Sr, Mg0.3Si, Mg5Sn, Mg5Zn and Mg0.3Ca in distilled water (DW) was studied using the linearly increasing stress test (LIST). SCC susceptibility was related to the stress rate for all the Mg-X alloys except for Mg0.1Sr. At similar to 7.0 x 10(-4) MPa s(-1), Mg0.3Si and Mg5Sn were immune to SCC; Mg0.1Zr, Mg1Mn and Mg0.1Sr suffered medium SCC; Mg5Zn and Mg0.3Ca suffered relatively more serious SCC. At similar to 7.0 x 10(-5) MPa s(-1), Mg5Zn and Mg0.3Ca suffered the most serious transgranular SCC, whilst the other Mg-X alloys suffered medium SCC. (C) 2015 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Corrosion behaviour in salt spray and in 3.5% NaCl solution saturated with Mg(OH)2 of as-cast and solution heat-treated binary Mg–X alloys: X=Mn, Sn, Ca, Zn, Al, Zr, Si, Sr10.1016/j.corsci.2013.06.030 ↗
2. Understanding magnesium corrosion—a framework for improved alloy performance10.1002/adem.200310405 ↗
3. Review of recent developments in the field of magnesium corrosion10.1002/adem.201400434 ↗
4. Corrosion mechanisms of magnesium alloys10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
5. Influence of hot rolling on the corrosion behavior of several Mg–X alloys10.1016/j.corsci.2014.10.012 ↗
6. Corrosion behaviour in salt spray and in 3.5% NaCl solution saturated with Mg(OH)2 of as-cast and solution heat-treated binary Mg–RE alloys: RE=Ce, La, Nd, Y, Gd10.1016/j.corsci.2013.06.032 ↗
7. Corrosion of ultra-high-purity Mg in 3.5% NaCl solution saturated with Mg(OH)210.1016/j.corsci.2013.05.018 ↗
8. Stress corrosion cracking of a wrought Mg–Mn alloy under plane strain and plane stress conditions10.1016/j.engfracmech.2013.02.018 ↗
9. Stress corrosion cracking of a recent rare-earth containing magnesium alloy, EV31A, and a common Al-containing alloy, AZ91E10.1016/j.corsci.2013.01.001 ↗
10. Characterisation of stress corrosion cracking (SCC) of Mg–Al alloys10.1016/j.msea.2007.11.064 ↗
11. Evaluation of the delayed hydride cracking mechanism for transgranular stress corrosion cracking of magnesium alloys10.1016/j.msea.2007.03.020 ↗
12. Comparison of the linearly increasing stress test and the constant extension rate test in the evaluation of transgranular stress corrosion cracking of magnesium10.1016/j.msea.2007.03.021 ↗
13. Fractography of stress corrosion cracking of Mg–Al alloys10.1007/s11661-008-9475-8 ↗
14. Stress corrosion cracking (SCC) in Mg–Al alloys studied using compact specimens10.1002/adem.200700319 ↗
15. A critical review of the stress corrosion cracking (SCC) of magnesium alloys10.1002/adem.200500071 ↗
16. A study on stress corrosion cracking and hydrogen embrittlement of AZ31 magnesium alloy10.1016/j.msea.2005.04.003 ↗
17. Hydrogen embrittlement of magnesium and magnesium alloys: a review10.1149/2.023304jes ↗
18. Fracture toughness and hydrogen-assisted crack growth in engineering alloys
19. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
20. Milne · 2003
21. Mechanisms of hydrogen related fracture – a review
22. Study on the SCC susceptibility of friction stir welded AZ31 Mg sheet10.1016/j.msea.2007.01.065 ↗
23. Hydrogen behavior during stress-corrosion cracking of an AZ31 magnesium alloy10.2464/jilm.51.397 ↗
24. Stress corrosion cracking and liquid metal embrittlement in pure magnesium10.5006/1.3583907 ↗
25. Stress corrosion cracking of rare-earth containing magnesium alloys ZE41, QE22 and Elektron 21 (EV31A) compared with AZ8010.1016/j.msea.2007.07.070 ↗
26. Stress corrosion cracking of new Mg–Zn–Mn wrought alloys containing Si10.1016/j.corsci.2008.02.012 ↗
27. Stress-corrosion cracking of magnesium alloys
28. Transgranular SCC in Mg–Al alloys10.1016/S0010-938X(71)80020-3 ↗
29. Levin · 1962
30. Busk · 1987
31. ASM Specialty Handbook: Magnesium and Magnesium Alloys, ASM International, Metals Park, Ohio, 1999, p. 211.
32. Production of high purity magnesium alloys by melt purification with Zr10.1002/adem.201200054 ↗
33. Linearly increasing stress test (LIST) for SCC research10.1088/0957-0233/4/11/017 ↗
34. Room temperature creep of high strength steels10.1016/0956-7151(94)90360-3 ↗
35. The initiation and propagation of stress corrosion cracking in AISI 4340 and 3.5 NiCrMoV rotor steel in constant load tests10.1016/0010-938X(96)00010-8 ↗
36. Environmental assisted fracture for 4340 steel in water and air of various humidities10.1023/A:1018659226945 ↗
37. Stress corrosion crack propagation in AerMet 10010.1023/A:1004362400904 ↗
38. The stress corrosion cracking of as-quenched 4340 and 3.5 NiCrMoV steels under stress rate control in distilled water at 90° C10.1016/0010-938X(93)90235-9 ↗
39. Initiation of stress corrosion cracking for pipeline steels in a carbonate–bicarbonate solution10.1007/BF02652362 ↗
40. The influence of hydrogen on 3.5NiCrMoV steel studied using the linearly increasing stress test10.1016/j.corsci.2012.10.019 ↗
41. Environmentally induced cracking of magnesium10.1016/0010-938X(84)90017-9 ↗