journal article·2020-05

Hot corrosion behavior of Pt+Hf co-modified NiAl coating in the mixed salt of Na2SO4-NaCl at 900 °C

Y.F. Yang, Z.L. Liu, P. Ren, Q.W. Wang, Z.B. Bao, S.L. Zhu, W. Li

Corrosion Science· Volume 167
Publisher page

Abstract

Abstract Hot corrosion behavior of Pt+Hf co-modified NiAl coating was evaluated in a salt mixture of Na2SO4/NaCl (75:25, wt./wt.) at 900 °C in comparing to Pt modified NiAl coating. Worm-like embossments appeared and developed in Pt+Hf co-modified NiAl coating due to the formation of slack Al2S3 and gaseous chloride bubbles. The fast dissolution of HfO2 during hot corrosion led to the disappearing of diffusion barrier effect of Hf-rich zone and elements like, Ni, Ti and Pt diffused into the oxide scale. The hot corrosion mechanism of Pt+Hf co-modified NiAl coating and the effects of Hf on this process were discussed in this work.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Surface and interface segregation in β-NiAl with and without Pt addition10.1016/j.scriptamat.2005.10.065 ↗
2. Interfacial Segregation, Pore Formation, and Scale Adhesion on NiAl Alloys10.1007/s11085-005-1954-3 ↗
3. Cyclic oxidation and rumpling behavior of single phase β-(Ni, Pt) Al coatings with different thickness of initial Pt plating10.1016/j.corsci.2016.05.011 ↗
4. Influence of sulfur, platinum, and hafnium on the oxidation behavior of CVD NiAl bond coatings10.1023/A:1020525123056 ↗
5. Effect of composition on the oxidation and hot corrosion resistance of NiAl doped with precious metals10.1016/S0257-8972(00)00878-1 ↗
6. Synthesis and cyclic oxidation behavior of a (Ni, Pt) Al coating on a desulfurized Ni-base superalloy10.1007/s11661-999-0308-1 ↗
7. Influence of Pt on the metal-oxide interface during high temperature oxidation of NiAl bulk materials10.1016/j.corsci.2008.12.016 ↗
8. On the initiation of cyclic oxidation-induced rumpling of platinum-modified nickel aluminide coatings10.1016/j.actamat.2008.12.015 ↗
9. Rumpling of CVD (Ni,Pt)Al diffusion coatings under intermediate temperature cycling10.1016/j.surfcoat.2009.04.016 ↗
10. Surface rumpling of a (Ni,Pt)Al bond coat induced by cyclic oxidation10.1016/S1359-6454(00)00156-7 ↗
11. Effect of Hf, Y and C in the underlying superalloy on the rumpling of diffusion aluminide coatings10.1016/j.actamat.2007.10.006 ↗
12. Improved alumina scale adhesion of electron beam physical vapor deposited Dy/Hf-doped β-NiAl coatings10.1016/j.apsusc.2013.06.137 ↗
13. Preparation and enhanced oxidation performance of a Hf-doped single-phase Pt-modified aluminide coating10.1016/j.corsci.2016.09.014 ↗
14. Identification of hot corrosion resistant MCrAlY based bond coatings for gas turbine engine applications10.1016/S0257-8972(00)01156-7 ↗
15. A Zr-doped single-phase Pt-modified aluminide coating and the enhanced hot corrosion resistance10.1016/j.corsci.2018.02.006 ↗
16. Oxidation behavior of Hf-modified platinum aluminide coatings during thermal cycling
17. Corrosion failures in gas turbine hot components10.1007/s11668-012-9571-3 ↗
18. Hot corrosion in gas turbine components10.1016/S1350-6307(00)00035-2 ↗
19. Synthesis of Hf-modified aluminide coatings on Ni-base superalloys10.1016/j.surfcoat.2011.08.031 ↗
20. Hot corrosion and oxidation behavior of a novel Pt plus Hf-modified γ’-Ni3Al +γ-Ni-based coating10.1016/j.surfcoat.2006.07.250 ↗
21. Effect of aluminisation characteristics on the microstructure of single phase β-(Ni,Pt)Al coating and the isothermal oxidation behaviour10.1016/j.corsci.2016.01.024 ↗
22. Preparation and hot corrosion behavior of an Al-gradient NiCoCrAlYSiB coating on a Ni-base superalloy10.1016/j.corsci.2009.01.003 ↗
23. Hot corrosion of arc ion plating NiCrAlY and sputtered nanocrystalline coatings on a nickel-based single-crystal superalloy10.1016/j.corsci.2017.04.004 ↗
24. High-temperature oxidation and hot-corrosion behavior of EB-PVD beta-NiAlDy coatings10.1016/j.corsci.2010.11.041 ↗
25. Effect of reactive element oxide coatings on the high temperature oxidation behavior of a FeCrAl alloy10.1149/1.2069350 ↗
26. Y.F. Yang, P. Ren, Z.B. Bao, S.L. Zhu, F.H. Wang, W. Li, Microstructure and cyclic oxidation of a Hf-doped (Ni,Pt)Al coating for single-crystal superalloys, unpublished work.
27. Identification of hot corrosion resistant MCrAlY based bond coatings for gas turbine engine applications10.1016/S0257-8972(00)01156-7 ↗
28. Hot corrosion behavior of single-phase platinum-modified aluminide coatings: effect of Pt content and pre-oxidation10.1016/j.corsci.2017.08.015 ↗
29. Early-stage oxidation behavior of Pt-Modified γ’-Ni3Al-Based alloys with and without Hf addition10.1007/s11085-008-9125-y ↗
30. Analysis of pore formation at oxide–alloy interfaces—I: experimental results on FeAl10.1023/A:1023013931251 ↗
31. Hot corrosion of Ti3SiC2-based ceramics coated with Na2SO4 at 900 and 1000 °C in air10.1016/S0010-938X(02)00211-1 ↗
32. Hot corrosion behavior of Ti3SiC2 in the mixture of Na2SO4–NaCl melts10.1016/j.jeurceramsoc.2004.04.013 ↗
33. High temperature sulfidation and oxidation of sputter-deposited Nb−Al−Si coatings10.1007/BF03027087 ↗
34. Effect of platinum on the oxide-to-metal adhesion in thermal barrier coating systems10.1007/s10853-007-2130-8 ↗
35. Microstructures and cyclic oxidation behaviour of Pt-free and low-Pt NiAl coatings on the Ni-base superalloy Rene-8010.1016/j.corsci.2011.10.037 ↗
36. Electrochemical characterization of cast Ti–Hf binary alloys10.1016/j.actbio.2005.02.006 ↗
37. The influence of platinum on the oxidation and sodium sulfate induced hot corrosion of NiAl diffusion coatings10.3184/096034011X13188762374132 ↗