The influence of manufacturing processes on the microstructure and corrosion of the AZ91D magnesium alloy evaluated using a computational image analysis
Source abstract
Abstract
Abstract The influence of different manufacturing processes on the microstructure and corrosion of the AZ91D magnesium alloy was investigated. The twin-roll casting process was compared with an established high-pressure die casting process and the Thixomolding ® process. The best corrosion resistance was found in thixomolded specimens due to a continuous and small meshed β-phase network, a homogeneous and small grain size, a minimal extent of Al and Zn segregations and the highest amount of β-phase. Parabolic corrosion-time dependence was found for thixomolded AZ91D and attributed to microstructural features. A computational image analysis was adapted for AZ91D micrographs and utilised for microstructural quantification.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Ghali · 2010
2. Polmear · 1996
3. Ferry · 2006
4. Dworog · 2002
5. Czerwinski · 2008
6. Injection molding of magnesium alloys
7. Feasibility study of twin roll casting process for magnesium alloys10.1016/j.jmatprotec.2007.04.009 ↗
8. Twin roll casting and melt conditioned twin-roll casting of magnesium10.4028/www.scientific.net/SSP.141-143.195 ↗
9. Extremely fine and uniform microstructure of magnesium AZ91D alloy sheets produced by melt conditioned twin roll casting10.1179/174328408X326129 ↗
10. Magnesium alloy strip produced by a melt-conditioned twin roll casting process10.4028/www.scientific.net/MSF.690.129 ↗
11. The effect of crystallographic orientation on the active corrosion of pure magnesium10.1016/j.scriptamat.2007.10.027 ↗
12. Influence of hot rolling on the corrosion behavior of several Mg–X alloys10.1016/j.corsci.2014.10.012 ↗
13. Crystallographic orientation and electrochemical activity of AZ31 Mg alloy10.1016/j.elecom.2010.05.011 ↗
14. Quantifying texture evolution during hot rolling of magnesium Twin Roll Cast strip10.1016/j.msea.2014.02.057 ↗
15. Corrosion and oxidation of thixomolded magnesium alloys
16. Corrosion behaviour of high pressure die-cast and semi-solid cast AZ91D alloys10.1016/S0010-938X(02)00075-6 ↗
17. A corrosion study of the main constituent phases of AZ91 magnesium alloys10.1016/S0010-938X(03)00109-4 ↗
18. Influence of the casting method on microstructure and corrosion of AZ91 and AM50
19. Influence of microstructure on the corrosion of diecast AZ91D10.1016/S0010-938X(98)00121-8 ↗
20. Effect of Mg17Al12 precipitate on corrosion behavior of AZ91D magnesium alloy10.4028/www.scientific.net/MSF.419-422.851 ↗
21. Effect of Al content on the corrosion behavior of Mg–Al alloys in aqueous solutions of different pH10.1016/j.electacta.2010.06.007 ↗
22. About some corrosion mechanisms of AZ91D magnesium alloy10.1016/j.corsci.2004.09.018 ↗
23. Understanding magnesium corrosion – a framework for improved alloy performance10.1002/adem.200310405 ↗
24. Measurement of the corrosion rate of magnesium alloys using Tafel extrapolation10.1016/j.corsci.2009.10.016 ↗
25. Colour etching and coloured image analysis – a way of characterising the microstructures of innovative cast materials10.1515/pm-2000-370804 ↗
26. The development of an electrolytic etching process for examining the microstructure of thixocast magnesium alloy AZ91hp10.1515/pm-2000-370304 ↗
27. Grain size measurement
28. Solidifi cation of cast magnesium alloys
29. Development of the as-cast microstructure in magnesium–aluminium alloys10.1016/S1471-5317(00)00007-9 ↗
30. Jones · 1996
31. Corrosion mechanism and evaluation of anodized magnesium alloys10.1016/j.corsci.2014.04.008 ↗
32. An innovative specimen configuration for the study of Mg corrosion10.1016/j.corsci.2010.09.016 ↗
33. Corrosion of ultra-high-purity Mg in 3.5% NaCl solution saturated with Mg(OH)210.1016/j.corsci.2013.05.018 ↗
34. Advances in Mg corrosion and research suggestions10.1016/j.jma.2013.09.003 ↗
35. Low apparent valence of Mg during corrosion10.1016/j.corsci.2014.07.060 ↗
36. The effect of aluminium content on the eutectic morphology of high pressure die cast magnesium–aluminium alloys10.1016/j.jallcom.2009.11.199 ↗
37. Corrosion behaviour of AZ21, AZ501 and AZ91 in sodium chloride10.1016/S0010-938X(98)00078-X ↗
38. Effect of galvanic corrosion between precipitate and matrix on corrosion behavior of As-cast magnesium-aluminum alloys10.1007/BF03028082 ↗
39. Influence of microstructure and composition on the corrosion behaviour of Mg/Al alloys in chloride media10.1016/j.electacta.2008.06.001 ↗
40. Local electrochemical impedance spectroscopy applied to the corrosion behavior of an AZ91 magnesium alloy10.1149/1.1602080 ↗
41. Corrosion behaviour of magnesium/aluminium alloys in 3.5wt.% NaCl10.1016/j.corsci.2007.11.005 ↗
42. Nonstoichiometric precipitation in As-Cast Mg-xAl-lZn alloy10.1007/BF03028090 ↗
43. Divorced eutectic in a HPDC magnesium–aluminum alloy10.1016/j.jallcom.2003.11.174 ↗
44. Morphology and structure of oxide films formed on MgAl alloys by exposure to air and water10.1149/1.1837048 ↗
45. Morphology and structure of water-formed oxides on ternary MgAl alloys10.1149/1.1837432 ↗
46. Liquidus and solidus temperatures of Mg-rich Mg–Al–Mn–Zn alloys10.1016/j.actamat.2006.04.022 ↗