journal article·2010-04

Evaluation of hydrogen absorption behaviour during acid etching for surface modification of commercial pure Ti, Ti–6Al–4V and Ni–Ti superelastic alloys

Akira Nagaoka, Ken’ichi Yokoyama, Jun’ichi Sakai

Corrosion Science· Volume 52· Issue 4
Publisher page

Abstract

Abstract The hydrogen absorption behaviour during acid etching for the surface modification of commercial pure Ti, Ti–6Al–4V and Ni–Ti superelastic alloys has been investigated on the basis of the surface morphology, electrochemical behaviour and hydrogen thermal desorption analysis. To simulate the conventional acid etching for the improvement of the biocompatibility of Ti alloys, the specimens are immersed in 1 M HCl, 1 M H2SO4 or 0.5 M HCl + 0.5 M H2SO4 aqueous solution at 60 °C. Upon immersion, commercial pure Ti absorbs substantial amounts of hydrogen irrespective of the type of solution. In H2SO4 or HCl + H2SO4 solutions, the hydrogen absorption occurs for a short time (10 min). For Ti–6Al–4V alloy, no hydrogen absorption is observed in HCl solution, whereas hydrogen absorption occurs in other solutions. For Ni–Ti superelastic alloy, the amount of absorbed hydrogen is large, resulting in the pronounced degradation of the mechanical properties of the alloy even for an immersion time of 10 min, irrespective of the type of solution. The hydrogen absorption behaviour is not necessarily consistent with the morphologies of the surface subjected to corrosion and the shift of the corrosion potential. The hydrogen thermal desorption behaviour of commercial pure Ti and Ni–Ti superelastic alloy are sensitively changed by acid etching conditions. The present results suggest that the evaluation of hydrogen absorption is needed for each condition of acid etching, and that the conventional acid etching often leads to hydrogen embrittlement.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (65)

Show source-provided references
1. Effect of surface topology on the osseointegration of implant materials in trabecular bone10.1002/jbm.820291213 ↗
2. Fast precipitation of calcium phosphate layers on titanium induced by simple chemical treatments10.1016/S0142-9612(97)82297-1 ↗
3. Chemical modification of titanium surfaces for covalent attachment of biological molecules10.1002/(SICI)1097-4636(199805)40:2<324::AID-JBM18>3.0.CO;2-L ↗
4. Hydroxyapatite formation on alkali-treated titanium with different content of Na+ in the surface layer10.1016/S0142-9612(02)00043-1 ↗
5. Biomimetic apatite formation on chemically treated titanium10.1016/j.biomaterials.2003.08.009 ↗
6. Analysing the optimal value for titanium implant roughness in bone attachment using a tensile test10.1016/S0142-9612(03)00256-4 ↗
7. Surface treatments of titanium dental implants for rapid osseointegration10.1016/j.dental.2006.06.025 ↗
8. Acid pretreatment of titanium implants10.1016/S0142-9612(02)00576-8 ↗
9. Effect of surface pre-treatment on durability of resin-based cements bonded to titanium10.1016/j.dental.2005.08.002 ↗
10. Effect of surface treatment and sterilization processes on the corrosion behavior of NiTi shape memory alloy10.1002/1097-4636(20000915)51:4<685::AID-JBM17>3.0.CO;2-S ↗
11. Effect of surface treatment of NiTi alloy on its corrosion behavior in Hanks’ solution10.1002/jbm.10114 ↗
12. Influence of nitinol wire surface treatment on oxide thickness and composition and its subsequent effect on corrosion resistance and nickel ion release10.1002/jbm.a.30720 ↗
13. Surface modification of titanium by etching in concentrated sulfuric acid10.1016/j.dental.2005.09.007 ↗
14. Bioactive apatite coating on titanium using an alternate soaking process10.4012/dmj.26.186 ↗
15. Surface properties and biocompatibility of acid-etched titanium10.4012/dmj.27.415 ↗
16. Dissolution of Ti wires in sulphuric acid and hydrochloric acid solutions10.1016/j.corsci.2006.04.017 ↗
17. Hydrogen desorption from sand-blasted and acid-etched titanium surfaces after glow-discharge treatment10.1002/1097-4636(200101)54:1<20::AID-JBM3>3.0.CO;2-Z ↗
18. Hydride formation on titanium surfaces by cathodic polarization10.1016/j.apsusc.2008.08.090 ↗
19. Effects of potential on hydrogen absorption and desorption behaviors of titanium in neutral fluoride solutions10.1016/j.jallcom.2006.05.036 ↗
20. Susceptibility to hydrogen absorption and hydrogen thermal desorption of titanium alloys immersed in neutral fluoride solution under applied potential10.2320/matertrans.MRA2008083 ↗
21. Effects of potential, temperature and pH on hydrogen absorption and thermal desorption behaviors of Ni–Ti superelastic alloy in 0.9% NaCl solution10.1016/j.corsci.2008.04.022 ↗
22. Hydrogen absorption of titanium in acidic fluoride solutions10.1016/j.msea.2004.05.059 ↗
23. Susceptibility to delayed fracture of alpha–beta titanium alloy in fluoride solutions10.1016/j.corsci.2004.08.007 ↗
24. Relationship between hydrogen absorption and corrosion behavior of Ti–6Al–4V alloy immersed in acidic fluoride solutions10.2320/matertrans.MRA2008481 ↗
25. Hydride formation during cathodic polarization of Ti – I. Effect of current density on kinetics of growth and composition of hydride10.1016/S0010-938X(72)80014-3 ↗
26. Hydride formation during cathodic polarization of Ti – II. Effect of temperature and pH of solution on hydride growth10.1016/S0010-938X(74)80063-6 ↗
27. Hydrogen embrittlement of grade 2 and grade 3 titanium in 6% sodium chloride solution10.5006/1.3284883 ↗
28. Electrochemical, galvanic, and mechanical responses of grade 2 titanium in 6% sodium chloride solution10.5006/1.3283973 ↗
29. Distribution and thermal desorption behavior of hydrogen in titanium alloys immersed in acidic fluoride solutions10.1016/j.jallcom.2004.12.041 ↗
30. Hydrogen absorption into alpha titanium in acidic solutions10.1016/j.electacta.2006.07.017 ↗
31. Hydrogen embrittlement of Ni–Ti superelastic alloy in fluoride solution10.1002/jbm.a.10457 ↗
32. Degradation of tensile strength of Ni–Ti superelastic alloy due to hydrogen absorption in methanol solution containing hydrochloric acid10.1016/S0921-5093(03)00403-9 ↗
33. Hydrogen embrittlement of Ni–Ti superelastic alloy in ethanol solution containing hydrochloric acid10.1016/j.msea.2004.10.020 ↗
34. Effects of moisture and dissolved oxygen in methanol and ethanol solutions containing hydrochloric acid on hydrogen absorption and desorption behaviors of Ni–Ti superelastic alloy10.1016/j.msea.2006.02.005 ↗
35. Hydrogen absorption of titanium and nickel–titanium alloys during long-term immersion in neutral fluoride solution10.1002/jbm.b.30485 ↗
36. Thermal stability of titanium hydride thin films10.1063/1.111950 ↗
37. Hydride dissociation and hydrogen evolution behavior of electrochemically charged pure titanium10.1016/0925-8388(95)01565-5 ↗
38. Hydrogen desorption from pure titanium with different concentration levels of hydrogen10.1016/j.jallcom.2007.04.304 ↗
39. Th. Boellinghaus, Hydrogen absorption and desorption in a duplex-annealed Ti–6Al–4V alloy during exposure to different hydrogen-containing environments10.1016/j.msea.2006.06.088 ↗
40. Delayed fracture of Ni–Ti superelastic alloys in acidic and neutral fluoride solutions10.1002/jbm.a.20122 ↗
41. Susceptibility to delayed fracture of Ni–Ti superelastic alloy10.1016/S0921-5093(02)00201-0 ↗
42. Hydrogen detrapping from grain boundaries and dislocations in high purity iron10.1016/0956-7151(92)90436-I ↗
43. The identification of hydrogen trapping states in an Al–Li–Cu–Zr alloy using thermal desorption spectroscopy10.1007/s11661-000-0064-8 ↗
44. Hydrogen in trapping states innocuous to environmental degradation of high-strength steels10.2355/isijinternational.43.520 ↗
45. Hydrogen related failure of steels – a new aspect10.1179/026708304225019687 ↗
46. Lattice defects dominating hydrogen-related failure of metals10.1016/j.actamat.2008.06.031 ↗
47. The hydrogen embrittlement of titanium alloys
48. Hydrogen embrittlement of commercial purity titanium10.1016/S0010-938X(01)00159-7 ↗
49. An investigation on structure, deformation and fracture of hydrides in titanium with a large range of hydrogen contents10.1016/j.actamat.2004.04.024 ↗
50. Fracture associated with hydrogen absorption of sustained tensile-loaded titanium in acid and neutral fluoride solutions10.1002/jbm.a.20067 ↗
51. Fracture of sustained tensile-loaded Ti–0.2% Pd alloy in acid and neutral fluoride solutions10.1016/j.msea.2005.12.006 ↗
52. The effect of composition on the hydrogen embrittlement of alpha–beta titanium alloys
53. Environmental hydrogen embrittlement of an α–β titanium alloy: effect of microstructure10.1007/BF02642051 ↗
54. Hydrogen in β transformed Ti–6Al–4V10.1007/BF02652859 ↗
55. Effect of hydrogen on fracture and inert-environment sustained load cracking resistance of α–β titanium alloys10.1007/BF02644024 ↗
56. Effects of hydrogen in titanium alloys on subcritical crack growth under sustained load10.1016/0025-5416(76)90094-X ↗
57. A film-rupture model of hydrogen-induced, slow crack growth in acicular alpha–beta titanium10.1007/BF02646469 ↗
58. Effect of hydrogen on creep behavior of Ti–6Al–4V alloy at room temperature10.1007/BF02668562 ↗
59. Effect of hydrogen and strain rate upon the ductility of mill-annealed Ti6Al4V10.1016/S0010-938X(98)00109-7 ↗
60. Hydrogen embrittlement of Ni–Ti superelastic alloy aged at room temperature after hydrogen charging10.1016/j.msea.2007.02.102 ↗
61. Hydrogen thermal desorption behavior of Ni–Ti superelastic alloy subjected to tensile deformation after hydrogen charging10.1016/j.msea.2007.04.104 ↗
62. Hydrogen absorption and thermal desorption behaviors of Ni–Ti superelastic alloy subjected to sustained tensile-straining test with hydrogen charging10.1016/j.scriptamat.2007.05.002 ↗
63. Hydrogen solubility and diffusion in the shape-memory alloy NiTi10.1088/0953-8984/1/14/003 ↗
64. Hydrogen embrittlement behavior induced by dynamic martensite transformation of Ni–Ti superelastic alloy10.1016/j.actamat.2008.12.030 ↗
65. Effect of constituent phase of Ni–Ti shape memory alloy on susceptibility to hydrogen embrittlement10.1016/j.msea.2004.02.029 ↗