journal article·2017-08

The effect of carbon on hydrogen embrittlement in stable Cr-Ni-Mn-N austenitic stainless steels

Han-Seop Noh, Jee-Hyun Kang, Kwang-Min Kim, Sung-Joon Kim

Corrosion Science· Volume 124
Publisher page

Abstract

Abstract The effect of carbon on hydrogen embrittlement in stable austenitic stainless steels is investigated by adding either 0.02 or 0.1 wt.% C. During deformation, planar slip is pronounced and fine dislocation structures develop, which is followed by mechanical twinning in both steels. After hydrogen pre-charging, the alloy with higher carbon is more susceptible to hydrogen embrittlement. Based on strain hardening behaviour, it is proposed that C enhances planar slip and refines mechanical twins. Therefore, a higher C concentration results in more sites available for stress concentration and hydrogen trapping, and accelerates the embrittlement.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Hydrogen transport in austenitic stainless steel10.1016/0010-938X(75)90022-0 ↗
2. Influence of plastic deformation on hydrogen diffusion and permeation in stainless steels10.1016/0001-6160(89)90211-3 ↗
3. Permeability, solubility and diffusivity of hydrogen isotopes in stainless steels at high gas pressures10.1016/j.ijhydene.2006.05.008 ↗
4. The effect of pre-straining and δ-ferrite on the embrittlement of 304L stainless steel by hydrogen10.1016/0010-938X(93)90261-E ↗
5. Hydrogen-assisted crack in 304L/308L and 21Cr–6Ni–9Mn/308L propagation in austenitic stainless steel fusion welds10.1016/j.corsci.2012.03.046 ↗
6. Effect of alloying elements on hydrogen environment embrittlement of AISI type 304 austenitic stainless steel10.1016/j.ijhydene.2011.09.013 ↗
7. Analysis of martensitic transformation in 304 type stainless steels tensile tested in high pressure hydrogen atmosphere by means of XRD and magnetic induction10.1016/j.ijhydene.2011.11.080 ↗
8. Dependence of hydrogen embrittlement on hydrogen in the surface layer in type 304 stainless steel10.1016/j.ijhydene.2014.03.254 ↗
9. Effects of delta ferrite on hydrogen embrittlement of austenitic stainless steel welds10.1016/S0010-938X(98)00083-3 ↗
10. A new aspect on intergranular hydrogen embrittlement mechanism of solution annealed types 304, 316 and 310 austenitic stainless steels10.1016/j.corsci.2009.01.031 ↗
11. Hydrogen uptake in 316L stainless steel: consequences on the tensile properties10.1016/j.corsci.2005.11.004 ↗
12. Hydrogen-assisted quasi-cleavage fracture in a single crystalline type 316 austenitic stainless steel10.1016/j.corsci.2013.06.018 ↗
13. Hydrogen environment embrittlement testing at low temperatures and high pressures10.1016/j.corsci.2008.09.025 ↗
14. Effect of nickel equivalent on hydrogen gas embrittlement of austenitic stainless steels based on type 316 at low temperatures10.1016/j.actamat.2008.03.022 ↗
15. Delayed static failure of twinning-induced plasticity steels10.1016/j.scriptamat.2012.02.038 ↗
16. Hydrogen and aluminium in high-manganese twinning-induced plasticity steel10.1016/j.scriptamat.2014.01.039 ↗
17. Effect of aluminium on hydrogen permeation of high-manganese twinning-induced plasticity steel10.1016/j.scriptamat.2014.11.023 ↗
18. Microband-induced plasticity in a high Mn-Al-C light steel10.1016/j.msea.2008.05.042 ↗
19. Influence of copper as an alloying element on hydrogen environment embrittlement of austenitic stainless steel10.1016/j.ijhydene.2012.06.058 ↗
20. The effect of Si on hydrogen embrittlement of Fe-18Mn-0.6C-xSi twinning-induced plasticity steels10.1016/j.actamat.2015.10.015 ↗
21. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
22. Hydrogen effects on the interaction between dislocations10.1016/S1359-6454(97)00349-2 ↗
23. Hydrogen effects on dislocation activity in austenitic stainless steel10.1016/j.actamat.2006.02.007 ↗
24. The role of localized deformation in hydrogen-assisted crack propagation in 21Cr–6Ni–9 Mn stainless steel10.1016/j.actamat.2009.04.027 ↗
25. A new concept of hydrogen embrittlement in steel
26. The diffusion and trapping of hydrogen in steel10.1016/0001-6160(70)90078-7 ↗
27. A classification of hydrogen traps in steel10.1007/BF02812023 ↗
28. Trap theory of Hydrogen embrittlement10.1016/0001-6160(80)90106-6 ↗
29. Hydrogen-induced cracking at grain and twin boundaries in an Fe–Mn–C austenitic steel10.1016/j.scriptamat.2011.12.015 ↗
30. Hydrogen embrittlement in a Fe–Mn–C ternary twinning-induced plasticity steel10.1016/j.corsci.2011.09.022 ↗
31. Effect of hydrogen content on the embrittlement in a Fe–Mn–C twinning-induced plasticity steel10.1016/j.corsci.2012.03.009 ↗
32. Hydrogen-induced delayed fracture of a Fe–22Mn–0.6C steel pre-strained at different strain rates10.1016/j.scriptamat.2012.02.040 ↗
33. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗
34. Hydrogen embrittlement associated with strain localization in a precipitation-hardened Fe–Mn–Al–C light weight austenitic steel10.1016/j.ijhydene.2013.12.171 ↗
35. The effect of Ti precipitates on hydrogen embrittlement of Fe–18Mn–0. 6C–2Al–xTi twinning-induced plasticity steel10.1016/j.corsci.2014.08.005 ↗
36. The strength of austenitic stainless steels
37. Effect of carbon fraction on stacking fault energy of austenitic stainless steels10.1007/s11661-012-1423-y ↗
38. Correlation between stacking fault energy and deformation microstructure in high-interstitial-alloyed austenitic steels10.1016/j.actamat.2010.01.056 ↗
39. Composition and grain size dependencies of strain-induced martensitic transformation in metastable austenitic stainless steels10.2355/tetsutohagane1955.63.5_772 ↗
40. Multistage strain hardening through dislocation substructure and twinning in a high strength and ductile weight-reduced Fe-Mn-Al-C steel10.1016/j.actamat.2012.07.018 ↗
41. Dislocation and twin substructure evolution during strain hardening of an Fe-22wt.% Mn-0.6wt.%C TWIP steel observed by electron channeling contrast imaging10.1016/j.actamat.2011.07.009 ↗
42. Strain hardening by dynamic slip band refinement in a high-Mn lightweight steel10.1016/j.actamat.2016.06.037 ↗
43. Origin of extended tensile ductility of a Fe-28Mn-10Al-1C steel10.1007/s11661-009-9862-9 ↗
44. Impact of short-range ordering on yield strength of high manganese austenitic steels10.1016/j.msea.2014.07.016 ↗
45. Derivation and variation in composition-dependent stacking fault energy maps based on subregular solution model in high-manganese steels10.1007/s11661-009-0050-8 ↗
46. On the origin of planar slip in f.c.c. alloys10.1016/0001-6160(89)90143-0 ↗
47. On the stress dependence of partial dislocation separation and deformation microstructure in austenitic stainless steels10.1016/S1359-6454(03)00117-4 ↗
48. On the correlation between electron structure and short range atomic order in iron-based alloys10.1016/S1359-6454(00)00192-0 ↗
49. Competing mechanisms and modeling of deformation in austenitic stainless steel single crystals with and without nitrogen10.1016/S1359-6454(01)00296-8 ↗
50. Nitrogen in chromium–manganese stainless steels: a review on the evaluation of stacking fault energy by computational thermodynamics10.1088/1468-6996/14/3/033001 ↗
51. A physical concept for alloying steels with carbon+nitrogen10.1016/j.msea.2006.11.186 ↗
52. On the more persistently-enhanced strain hardening in carbon-increased Fe–Mn–C twinning-induced plasticity steel10.1016/j.msea.2015.05.044 ↗
53. Cathodic hydrogen embrittlement in alloy 71810.1016/S0921-5093(99)00167-7 ↗
54. Effect of surface hydrogen concentration on hydrogen embrittlement properties of stainless steels and Ni based alloys10.2355/isijinternational.ISIJINT-2015-268 ↗
55. The effect of hydrogen on the yield and flow stress of an austenitic stainless steel10.1007/BF02669643 ↗
56. Hydrogen embrittlement understood10.1007/s11663-015-0325-y ↗
57. On the formation and nature of quasi-cleavage fracture surfaces in hydrogen embrittled steels10.1016/j.actamat.2010.11.024 ↗