Failure mechanism transition of hydrogen embrittlement in AISI 304 K-TIG weld metal under tensile loading

Xiaogang Li, Baoming Gong, Caiyan Deng, Yizhe Li

Corrosion Science· Volume 130
Publisher page

Abstract

Abstract The effect of hydrogen on the tensile properties of AISI 304 K-TIG weld metal is investigated in this study. Fractographic analysis demonstrates a transition from quasi-cleavage/cleavage fracture to intergranular fracture in the brittle zone as the hydrogen-charging current density increases, which is attributed to the interplay of crystalline defect, hydrogen atoms, and α′ martensite transformation sites. It is believed that at low current density, α′ martensite nucleates and grows homogeneously in the interior of the grain. At high current density, the stress-induced α′ martensite forms preferentially at the grain boundary, which undergoes severe strain localisation and hydrogen atom segregation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Peckner · 1977
2. Caskey · 1983
3. A new aspect on intergranular hydrogen embrittlement mechanism of solution annealed types 304, 316 and 310 austenitic stainless steels10.1016/j.corsci.2009.01.031 ↗
4. Effect of austenite instability on the hydrogen-enhanced crack growth of austenitic stainless steels10.1016/j.corsci.2007.01.008 ↗
5. Effect of hydrogen on tensile behaviour of micrometre-sized specimen fabricated from a metastable austenitic stainless steel10.1016/j.corsci.2010.10.019 ↗
6. Hydrogen uptake in 316L stainless steel: consequenceson the tensile propertis10.1016/j.corsci.2005.11.004 ↗
7. Hydrogen-assisted fatigue crack growth of AISI 316L stainless steel weld10.1016/j.corsci.2008.08.016 ↗
8. Hydrogen-assisted quasi-cleavage fracture in a single cystalline type 316 austenitic stainless steel10.1016/j.corsci.2013.06.018 ↗
9. Effects of dissolved hydrogen and surface condition on the intergranular stress corrosion cracking initiation and short crack growth behavior of non-sensitized 316 stainless steel in simulated PWR primary water10.1016/j.corsci.2017.02.003 ↗
10. The influence of austenite stability on the hydrogen embrittlement and stress-corrosion cracking of stainless steel10.1007/BF02658313 ↗
11. On the physical differences between tensile testing of type 304 and 316 austenitic stainless steels with internal hydrogen and in external hydrogen10.1016/j.ijhydene.2010.06.018 ↗
12. Hydrogen environment embrittlement of austenitic stainless steels at low temperatures10.1016/j.ijhydene.2008.02.021 ↗
13. Effect of cold deformation on the corrosion behaviour of UNS S31803 duplex stainless steel in simulated concrete pore solution10.1016/j.corsci.2017.05.021 ↗
14. Plastic deformation and corrosion in austenitic stainless steel: a novel approach through microtexture and infrared spectroscopy10.1016/j.corsci.2016.05.027 ↗
15. Effect of surface nanocrystallization on the sensitization and desensitization behavior of Super304H stainless steel10.1016/j.corsci.2016.06.012 ↗
16. Influence of microstructure evolution on tribocorrosion of 304SS in artificial seawater10.1016/j.corsci.2014.07.062 ↗
17. Deformation behavior and micro structure/texture evolution of an annealed 304 AISI stainless steel sheet. Experimental and micromechanical modeling10.1016/j.ijplas.2006.07.002 ↗
18. Effect of strain-induced martensite on hydrogen environment embrittlement of sensitized austenitic stainless steels at low temperatures10.1016/S1359-6454(98)00136-0 ↗
19. Comparison of hydrogen gas embrittlement of austenitic and ferritic stainless steels10.1007/BF02646229 ↗
20. Internal reversible hydrogen embrittlement of austenitic stainless steels based on type 316 at low temperatures
21. Effects of hydrogen on metal fatigue
22. Influence of machining-induced martensite on hydrogen-assisted fracture of AISI type 304 austenitic stainless steel10.1016/j.ijhydene.2011.05.133 ↗
23. Effects of hydrogen on fatigue crack growth behavior of austenitic stainless steels10.1016/j.ijhydene.2008.02.067 ↗
24. Hydrogen-induced strain localization and failure of austenitic stainless steels at high hydrogen concentrations10.1016/0956-7151(91)90211-I ↗
25. The effect of carbon on hydrogen embrittlement in stable Cr-Ni-Mn-N austenitic stainless steels10.1016/j.corsci.2017.05.004 ↗
26. A TEM investigation of hydrogen-induced deformation twinning and associated martensitic phases in 304-type stainless-steel10.1007/BF00566284 ↗
27. Hydrogen-induced twinning in <0 0 1> Hadfield steel single crystals10.1016/j.scriptamat.2010.08.029 ↗
28. Solute segregation and hydrogen-induced intergranular fracture in an alloy steel10.1007/BF02644295 ↗
29. First-principles study on the grain boundary embrittlement of metals by solute segregation: part II. Metal (Fe, Al, Cu)-hydrogen (H) systems10.1007/s11661-010-0380-6 ↗
30. On the formation and nature of quasi-cleavage fracture surfaces in hydrogen embrittled steels10.1016/j.actamat.2010.11.024 ↗
31. The influence of calcareous deposits on hydrogen uptake and embrittlement of API 5CT P110 steel10.1016/j.corsci.2017.02.007 ↗
32. Hydrogen-assisted crack propagation in 304L/308L and 21Cr-6Ni-9Mn/308L austenitic stainless steel fusion welds10.1016/j.corsci.2012.03.046 ↗
33. Fatigue crack growth of AISI 304 stainless steel welds in air and hydrogen10.1016/j.msea.2004.02.018 ↗
34. Hydrogen-assisted crack propagation in austenitic stainless steel fusion welds10.1007/s11661-009-9922-1 ↗
35. Hydrogen environment embrittlement of orbital welded austenitic stainless steels at −50°C10.1016/j.ijhydene.2009.05.081 ↗
36. Effect of weld composition and microstructure on hydrogen assisted fracture of austenitic stainless steels10.1007/BF02643740 ↗
37. Hydrogen absorption of different welded duplex steels10.1016/j.ijhydene.2010.01.148 ↗
38. Cold cracking of structural steel weldments as reversible hydrogen embrittlement effect10.1016/S0360-3199(99)00058-0 ↗
39. Environmentally assisted crack growth in 308L stainless steel weld metal in simulated primary water10.1016/j.corsci.2016.12.011 ↗
40. Hydrogen diffusion and hydrogen influenced critical stress intensity in an API X70 pipeline steel welded joint-Experiments and FE simulations10.1016/j.ijhydene.2012.05.005 ↗
41. Hydrogen effect on fracture toughness of pipeline steel welds, with in situ hydrogen charging10.1016/j.ijhydene.2011.06.140 ↗
42. Hydrogen interaction and stress-corrosion in hydrocarbon storage vessel and pipeline weldings10.1016/j.ijhydene.2005.05.011 ↗
43. Hydrogen permeation behavior in relation to microstructural evolution of low carbon bainitic steel weldments10.1016/j.corsci.2016.07.025 ↗
44. Hydrogen permeation and embrittlement susceptibility of X80 welded joint under high-pressure coal gas environment10.1016/j.corsci.2016.04.029 ↗
45. Influence of macro segregation on hydrogen environment embrittlement of SUS 316L stainless steel10.1016/j.ijhydene.2009.02.015 ↗
46. Influence of hydrogen content on the tensile properties and fracture of austenitic stainless steel welds10.1016/j.ijhydene.2012.11.016 ↗
47. Quantifying the hydrogen embrittlement of pipeline steels for safety considerations10.1016/j.ijhydene.2012.05.143 ↗
48. Toughness and hydrogen compatibility of austenitic stainless steel welds at cryogenic temperatures10.1016/j.ijhydene.2007.03.009 ↗
49. Keyhole gas tungsten arc welding of AISI 316L stainless steel10.1016/j.matdes.2015.07.011 ↗
50. Electrochemical method for studying hydrogen in iron, nickel and palladium10.1016/0360-3199(92)90051-W ↗
51. Effect of hydrogen on ductility of high strength 3Ni-Cr-Mo-V steels10.1016/j.msea.2013.11.058 ↗
52. Influence of hydrogen on the mechanical and fracture properties of some martensitic advanced high strength steels in simulated service conditions10.1016/j.corsci.2016.05.040 ↗
53. Effects of alloy composition and strain hardening on tensile fracture of hydrogen-precharged type 316 stainless steels10.1016/j.ijhydene.2007.10.046 ↗
54. Effect of hydrogen on work hardening of type 304L austenitic stainless steel10.1016/0036-9748(81)90294-5 ↗
55. Dieter · 1986
56. Electrochemical nanoindentation: a new approach to probe hydrogen/deformation interaction10.1016/j.scriptamat.2006.03.041 ↗
57. Kinetics of strain-induced martensite nucleation10.1007/BF02672301 ↗
58. Effect of hydrogen on martensite formation in austenitic stainless steels in high-pressure torsion10.1016/j.actamat.2009.03.006 ↗
59. A new model for hydrogen assisted cracking (hydrogen embrittlement)10.1007/BF02642048 ↗
60. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
61. Hydrogen embrittlement of ferritic steels: observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗
62. Mechanics of the hydrogen-dislocation-impurity interactions–I. Increasing shear modulus10.1016/0022-5096(94)00056-B ↗
63. Hydrogen effects on the character of dislocations in high-purity aluminum10.1016/S1359-6454(99)00156-1 ↗
64. Effects of delta ferrite on hydrogen embrittlement of austenitic stainless steel welds10.1016/S0010-938X(98)00083-3 ↗
65. Analysis of hydrogen atom transport in a two-phase alloy10.1016/0921-5093(94)90488-X ↗
66. Brittle fracture in austenitic steel10.1016/0956-7151(94)90300-X ↗
67. The role of localized deformation in hydrogen-assisted crack propagation in 21Cr-6Ni-9Mn stainless steel10.1016/j.actamat.2009.04.027 ↗
68. Investigation of the fracture mechanism of Ti-5Al-2.5Sn at cryogenic temperatures10.1007/BF02646411 ↗
69. Deformation behavior of age-hardened Ti-Mo alloys10.1016/0001-6160(74)90057-1 ↗
70. Modeling hydrogen transport by dislocations10.1016/j.jmps.2015.03.002 ↗
71. Reducing grain boundary, dislocation line and vacancy formation energies by solute segregation II. Experimental evidence and consequences10.1016/j.actamat.2007.05.033 ↗
72. First-principles study on the interaction of H interstitials with grain boundaries in alpha- and gamma-Fe10.1103/PhysRevB.84.144121 ↗
73. The effect of pre-straining and δ-ferrite on the embrittlement of 304L stainless steel by hydrogen10.1016/0010-938X(93)90261-E ↗