Quasi-continuous-wave laser surface melting of aluminium alloy: Precipitate morphology, solute segregation and corrosion resistance
Source abstract
Abstract
Abstract A quasi-continuous-wave laser surface melting is performed on 2219 aluminium alloys to improve the corrosion resistance. The fast cooling rate and the multi-directional solidification behavior of the process transform large and long-chained constituent particles into fine and isolated circular precipitates with alleviated solute segregation. The improved corrosion resistance is due to the formation of low-flaw-density passive film, the reduction of the driving force for corrosion and the improvement of the re-passivation capability of the modified surface. The large and long-chained constituent particles are the preferred sites for corrosion initiation and propagation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Additive Manufacturing Materials and Processes · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Friction stir processing of aluminium alloy AA7075: microstructure, surface chemistry and corrosion resistance10.1016/j.corsci.2016.02.006 ↗
2. Localized corrosion of a 2219 aluminium alloy exposed to a 3.5% NaCl solution10.1016/j.corsci.2010.04.035 ↗
3. Establishing a correlation between interfacial microstructures and corrosion initiation sites in Al/Cu joints by SEM-EDS and AFM-SKPFM10.1016/j.corsci.2013.10.039 ↗
4. Pitting corrosion of rheocast A356 aluminium alloy in 3.5 wt.% NaCl solution10.1016/j.corsci.2013.04.023 ↗
5. SEM/EDS characterization of laser shock peening effect on localized corrosion of Al alloy in a near natural chloride environment10.1016/j.corsci.2014.01.032 ↗
6. Comparison of corrosion behaviour of friction stir processed and laser melted AA 2219 aluminium alloy10.1016/j.matdes.2011.03.033 ↗
7. Relationship between microstructure and corrosion performance of AA2050-T8 aluminium alloy after excimer laser surface melting10.1016/j.corsci.2010.03.003 ↗
8. Microstructure and corrosion properties of diode laser melted friction stir weld of aluminum alloy 2024 T35110.1016/j.apsusc.2010.11.163 ↗
9. Enhanced performance of the AA2050-T8 aluminium alloy following excimer laser surface melting and anodising processes10.1016/j.tsf.2009.09.121 ↗
10. Excimer laser surface treatment of aluminum alloy AA7075 to improve corrosion resistance10.1016/S0257-8972(03)00850-8 ↗
11. Grain structure and homogeneity of pulsed laser treated surfaces on Al-aerospace alloys and FSWs10.1016/j.msea.2007.06.029 ↗
12. Effect of excimer laser surface melting on the microstructure and corrosion performance of the die cast AZ91D magnesium alloy10.1016/j.corsci.2009.09.025 ↗
13. Corrosion mechanism of laser-melted AA 2014 and AA 2024 alloys10.1016/j.apsusc.2005.01.067 ↗
14. Fundamental understanding of the corrosion performance of laser-melted metallic alloys10.1016/j.surfcoat.2005.07.108 ↗
15. Influence of laser surface treated on the characterization and corrosion behavior of Al-Fe aerospace alloys10.1016/j.apsusc.2013.03.025 ↗
16. Yb-fiber laser beam effects on the surface modification of Al-Fe aerospace alloy obtaining weld filet structures, low fine porosity and corrosion resistance10.1016/j.surfcoat.2011.10.007 ↗
17. Nd : YAG laser surface melting of aluminium alloy 6013 for improving pitting corrosion fatigue resistance10.1007/s10853-007-2208-3 ↗
18. The effect of excimer laser surface treatment on the pitting corrosion fatigue behaviour of aluminium alloy 707510.1023/A:1024498922104 ↗
19. Corrosion protection of AA2024-T351 friction stir welds by laser surface melting with Excimer laser10.1179/1743278211Y.0000000020 ↗
20. Effects of laser modes on Nb segregation and Laves phase formation during laser additive manufacturing of nickel-based superalloy10.1016/j.matlet.2016.10.118 ↗
21. Laves phase control of Inconel 718 alloy using quasi-continuous-wave laser additive manufacturing10.1016/j.matdes.2017.03.004 ↗
22. Melt-pool motion, temperature variation and dendritic morphology of Inconel 718 during pulsed-and continuous-wave laser additive manufacturing: a comparative study10.1016/j.matdes.2017.01.065 ↗
23. Investigation on the manufacture of a large-scale aluminum alloy ingot: microstructure and macrosegregation10.1002/adem.201600375 ↗
24. The effect of globular microstructure size on the mechanical properties in reheating process of aluminum alloys10.1361/10599490418451 ↗
25. Quantitative analysis of pitting corrosion behavior of thixoformed A356 alloy in chloride medium using electrochemical techniques10.1016/j.matdes.2008.10.003 ↗
26. Breakdown of passivity of aluminium alloys by intermetallic phases in neutral chloride solution10.1016/S0966-9795(99)00114-4 ↗
27. Corrosion behavior of laser melted AZ91HP magnesium alloy10.1002/maco.200604031 ↗
28. Statistical analysis of constituent particles in 7075-T6 aluminum alloy10.1007/BF02586171 ↗
29. Banded microstructure in AA2024-T351 and AA2524-T351 aluminum friction stir welds - part I. Metallurgical studies10.1016/S0921-5093(03)00532-X ↗