Studies on corrosion behavior of a single-crystal superalloy and its sputtered nanocrystalline coatings with solid NaCl deposit in O2 + 38 vol.% H2O environment at 700 °C

Wenyao Sun, Jinlong Wang, Lanlan Yang, Minghui Chen, Zebin Bao, Chengyue Zheng, Shenglong Zhu, Fuhui Wang

Corrosion Science· Volume 161
Publisher page

Abstract

Abstract Corrosion behavior of the N5 superalloy (Ni-7.0 Cr-6.2 Al-7.5 Co-5.0 W-1.5 Mo-6.5 Ta-3.0 Re) and two nanocrystalline coatings prepared by magnetron sputtering is investigated in chlorine and water vapor environment at 700 °C. The alloy shows low corrosion resistance. Its oxide scale spalls off readily and includes porous NiO outer layer and NiCr(Al)2O4 inner one. The nanocrystalline coating performs better. Its oxide scale consists of Al2O3, NiO and Ta2O5. Chlorination and/or oxidation of Ta ruined compactness of scale. The yttrium modified nanocrystalline coating provides the highest corrosion resistance. Its scale is exclusively alumina. Yttrium inhibits the outward diffusion of Ta.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · nanoparticles nucleation surface interactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. The high temperature behavior of superalloys exposed to sodium chloride: II. Corrosion10.1007/BF02649632 ↗
2. High temperature behavior of superalloys exposed to sodium chloride: I. Mechanical properties10.1007/BF02649631 ↗
3. Hot corrosion studies on Ni-base superalloy at 650 °C under marine-like environment conditions using three salt mixture (Na2SO4 + NaCl +NaVO3)10.1016/j.corsci.2016.01.008 ↗
4. High temperature corrosion of Fe-Cr-(Mn/Si) alloys in CO2-H2O-SO2 gases10.1016/j.corsci.2016.07.026 ↗
5. Benefits of Zr addition to oxidation resistance of a single-phase (Ni,Pt)Al coating at 1373 K10.1016/j.jmst.2019.03.013 ↗
6. Interaction of Ta and Cr on Type-I hot corrosion resistance of single crystal Ni-base superalloys10.1016/j.corsci.2017.01.011 ↗
7. Influence of Cr content on hot corrosion and a special tube sealing test of single crystal nickel base superalloy10.1016/j.corsci.2019.05.001 ↗
8. Solubilities of Cr2O3 in fused Na2SO4 at 1200 K10.1149/1.2108648 ↗
9. Preparation and hot corrosion behavior of a NiCrAlY + AlNiY composite coating10.1016/j.jmst.2016.04.017 ↗
10. Hot corrosion of YSZ/Al2O3 dispersed NiCrAlY plasma sprayed coatings in Na2SO4-10 wt.% NaCl melt10.1016/j.corsci.2010.04.007 ↗
11. The chemical composition of the passive film on Fe-24Cr and Fe-24Cr-11Mo studied by AES, XPS and SIMS10.1016/0010-938X(91)90013-F ↗
12. Semiconducting and passive film properties of nitrogen-containing type 316LN stainless steels10.1016/j.corsci.2006.05.041 ↗
13. Corrosion behavior of pure Cr with a solid NaCl deposit in O2 plus water vapor10.1023/A:1004690518225 ↗
14. Influence of Cr content on the corrosion of Fe-Cr alloys: the synergistic effect of NaCl and water vapor10.1023/A:1023083309041 ↗
15. Corrosion behavior of a sputtered K38G nanocrystalline coating with a solid NaCl deposit in wet oxygen at 600-700 °C10.1023/A:1016072726338 ↗
16. Oxidation of Fe-10Cr in O2 and in O2 + H2O environment at 600 °C: a microstructural investigation10.1016/j.corsci.2013.06.016 ↗
17. Oxidation of an austenitic stainless steel with or without alloyed aluminum in O2 + 10% H2O environment at 800 °C10.1016/j.corsci.2017.03.015 ↗
18. Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapor at 600 °C10.1016/j.corsci.2005.08.012 ↗
19. Studies on the corrosion behavior of Fe-20Cr alloy in NaCl solution spray at 600 °C10.1016/j.corsci.2018.01.033 ↗
20. A thermodynamic approach on vapor-condensation of corrosive salts from flue gas on boiler tubes in waste incinerators10.1016/j.corsci.2008.02.004 ↗
21. Effects of fuel impurities on the fireside corrosion of boiler tubes in advanced power generating systems-a thermodynamic calculation of deposit chemistry10.1016/S0010-938X(01)00060-9 ↗
22. Local reactions of KCl particles with iron, nickel and chromium surfaces10.1002/maco.200503903 ↗
23. The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
24. KCl-induced high temperature corrosion of the austenitic Fe–Cr–Ni alloys 304L and Sanicro 28 at 600 °C10.1016/j.corsci.2005.05.018 ↗
25. KCl-induced corrosion of an FeCrAl alloy at 600 °C in O2 + H2O environment: the effect of pre-oxidation10.1007/s11085-014-9507-2 ↗
26. High temperature interaction of Al/Si-modified Fe-Cr alloys with KCl10.1016/j.corsci.2006.10.019 ↗
27. Chlorine-induced high temperature corrosion of HVAF-sprayed Ni-based alumina and chromia forming coatings10.1016/j.corsci.2017.12.033 ↗
28. Experimental and thermodynamic investigations on the chlorine-induced corrosion of HVOF thermal sprayed NiAl coatings and 304 stainless steels at 700 °C10.1016/j.corsci.2018.02.047 ↗
29. Nickel base superalloys: current status and potential
30. Ta effect on oxidation of a nickel-based single-crystal superalloy and its sputtered nanocrystalline coating at 900-1100 °C10.1016/j.apsusc.2015.03.157 ↗
31. Effect of nickel base superalloy composition on oxidation resistance in SO2 containing, high pO2 environments10.1002/maco.201307299 ↗
32. High-temperature oxidation resistance of sputtered micro-grain superalloy K38G10.1007/BF00666917 ↗
33. Cross-sectional oxide distribution of cast IN738 and its sputtered coating at 1000 °C10.1016/S0257-8972(02)00909-X ↗
34. Oxidation and hot corrosion behavior of sputtered nanocrystalline coating of superalloy K5210.1016/j.tsf.2007.07.131 ↗
35. Hot corrosion of arc ion plating NiCrAlY and sputtered nanocrystalline coatings on a nickel-based single-crystal superalloy10.1016/j.corsci.2017.04.004 ↗
36. Solubility study on protective oxide films in molten chlorides created by refuse incineration environment10.1002/(SICI)1521-4176(200003)51:3<177::AID-MACO177>3.0.CO;2-O ↗
37. Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400-700 °C10.1016/S0010-938X(99)00142-0 ↗
38. Synergistic effect of NaCl and water vapor on the corrosion of Ti60 alloy at 500-700 °C10.1023/A:1018864216554 ↗
39. The effect of yttrium addition on oxidation of a sputtered nanocrystalline coating with moderate amount of tantalum in composition10.1016/j.apsusc.2016.01.088 ↗
40. Diffusion of Ta and its influence on oxidation behavior of nanocrystalline coatings with different Ta, Y and Al contents10.1016/j.corsci.2017.07.017 ↗