In situ synchrotron X-ray tomography of 304 stainless steels undergoing chlorine-induced stress corrosion cracking
Source abstract
Abstract
Abstract To understand the mechanisms behind chlorine-induced stress corrosion cracking (CISCC) in 304 stainless steel, synchrotron high energy x-rays were used to perform in-situ x-ray microtomography on a pre-cracked sample under load in a corrosive simulated marine environment. The tomography scans showed the crack morphology evolving into a branching crack around the surface of the sample. Finite element analysis and stress intensity analysis are conducted to explain the observed crack branching.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. U.S. NRC · 2014
2. Stress corrosion cracking of stainless-steel canister for concrete cask storage of spent fuel10.1016/j.jnucmat.2008.06.005 ↗
3. Jones · 2017
4. Chloride-induced stress corrosion cracking of used nuclear fuel welded stainless steel canisters: a review10.1016/j.jnucmat.2015.07.043 ↗
5. Chloride induced stress corrosion cracking of candidate canister materials for dry storage of spent fuel10.1016/j.nucengdes.2007.03.038 ↗
6. Deformation induced martensitic transformation in 304 austenitic stainless steel: In-situ vs. Ex-situ transmission electron microscopy characterization10.1016/j.msea.2017.12.036 ↗
7. Microscopy study of intergranular stress corrosion cracking of X-52 line pipe steel10.5006/1.3280664 ↗
8. SKFM observation of SCC on SUS304 stainless steel10.1016/j.corsci.2006.05.014 ↗
9. Effect of loading history on stress corrosion cracking of 7075-T651 aluminum alloy in saline aqueous environment10.1007/s11661-010-0419-8 ↗
10. Discontinuous surface cracks during stress corrosion cracking of stainless steel single crystal10.1016/j.corsci.2011.06.019 ↗
11. In situ investigation of high humidity stress corrosion cracking of 7075 aluminum alloy by three-dimensional (3D) X-ray synchrotron tomography10.1080/21663831.2014.918907 ↗
12. Crack growth characterization in single-edge notched tension testing by means of direct current potential drop measurement10.1016/j.ijpvp.2017.06.009 ↗
13. In situ X-ray microtomography of stress corrosion cracking and corrosion fatigue in aluminum alloys10.1007/s11837-017-2413-8 ↗
14. Detecting and imaging stress corrosion cracking in stainless steel, with application to inspecting storage canisters for spent nuclear fuel10.1016/j.ndteint.2019.102180 ↗
15. Wu · 2017
16. Numerical simulation of temperature field and residual stress in multi-pass welds in stainless steel pipe and comparison with experimental measurements10.1016/j.commatsci.2005.07.007 ↗
17. Superior techniques for eliminating ring artifacts in X-ray micro-tomography10.1364/OE.26.028396 ↗
18. Fatigue voids and their significance10.1046/j.1460-2695.2002.00565.x ↗
19. Fracture mechanics by three-dimensional crack-tip synchrotron X-ray microscopy10.1098/rsta.2013.0157 ↗
20. Single edge-crack stress intensity factor solutions10.1016/j.engfracmech.2005.09.003 ↗
21. An efficient and accurate numerical method of stress intensity factors calculation of a branched crack10.1115/1.1796449 ↗
22. Studies of dynamic crack propagation and crack branching with peridynamics10.1007/s10704-010-9442-4 ↗
23. The role of crack branching in stress corrosion cracking of aluminium alloys10.1515/corrrev-2015-0050 ↗
24. Schijve · 2009
25. Bathias · 2010
26. Crack branching during stress corrosion cracking of high-strength materials10.1007/BF00716895 ↗
27. SCC growth behaviors of austenitic stainless steels in simulated PWR primary water10.1016/j.jnucmat.2012.03.013 ↗
28. Fatigue crack branching in laser melting deposited Ti–55511 alloy10.1016/j.ijfatigue.2019.03.006 ↗