Statistical study of the critical pitting temperature of 22-05 duplex stainless steel
Source abstract
Abstract
Abstract Using a multichannel electrochemical cell, critical potentials for passive film breakdown of a duplex stainless steel were measured at different temperatures in a 0.5 M NaCl aqueous solution. Statistical analysis shows that the transition between pitting and transpassivity does not occur at a well-defined “critical pitting temperature” (CPT) but takes place within a transition temperature interval (TTI), the width of which (∼10 to 1 °C) decreases as the size of the specimen increases. For practical purposes, the lower TTI bound appears to be the most reliable indicator of the CPT. Potentiostatic techniques were found to overestimate the CPT value compared to potentiodynamic estimations.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Shibata · Corrosion · 1977 · 33 · 24310.5006/0010-9312-33.7.243 ↗
2. Baroux · Corros. Sci. · 1988 · 28 · 96910.1016/0010-938X(88)90015-7 ↗
3. Brigham · Corrosion · 1972 · 28 · 17710.5006/0010-9312-28.5.177 ↗
4. Brigham · Corrosion · 1973 · 29 · 3310.5006/0010-9312-29.1.33 ↗
5. Qvarfort · Corros. Sci. · 1989 · 29 · 98710.1016/0010-938X(89)90088-7 ↗
6. Arnvig · ACOM · 1996 · 3 · 2
7. Brigham · Corrosion · 1974 · 30 · 16110.5006/0010-9312-30.5.161 ↗
8. Brigham · J. Electrochem. Soc. · 1974 · 121 · 119210.1149/1.2402009 ↗
9. Russel · Corrosion · 2001 · 57 · 36010.5006/1.3290360 ↗
10. ASTM G150 – 99 (2010) ISO 17864 (2005).
11. Moayed · Corros. Sci. · 1998 · 40 · 51910.1016/S0010-938X(97)00137-6 ↗
12. Laycock · Corrosion · 1999 · 55 · 59010.5006/1.3280500 ↗
13. Pardo · Corrosion · 2000 · 56 · 41110.5006/1.3280545 ↗
14. Liang · Corros. Sci. Protec. Technol. · 2005 · 17 · 392
15. Ernst · Corros. Sci. · 2007 · 49 · 370510.1016/j.corsci.2007.03.026 ↗
16. Moayed · Corros. Sci. · 2006 · 48 · 351310.1016/j.corsci.2006.02.010 ↗
17. Moayed · Corros. Sci. · 2003 · 45 · 120310.1016/S0010-938X(02)00215-9 ↗
18. R.F.A. Pettersson, in: Stainless Steel’08. Proceeding of the 6th European stainless steel conference, Helsinki, Finland, 2008, pp. 37–42.
19. Deng · Appl. Surf. Sci. · 2007 · 253 · 736910.1016/j.apsusc.2007.03.034 ↗
20. Schenk · Corrosion · 1964 · 20 · 12910.5006/0010-9312-20.4.129t ↗
21. Szklarska-Smialowska · Corros. Sci. · 1972 · 12 · 92510.1016/S0010-938X(72)80100-8 ↗
22. Ernst · Corros. Sci. · 1997 · 39 · 113310.1016/S0010-938X(97)00043-7 ↗
23. Moayed · Corros. Sci. · 2006 · 48 · 100410.1016/j.corsci.2005.03.002 ↗
24. Steinsmo · Corrosion · 1997 · 53 · 2610.5006/1.3280430 ↗
25. Jakobsen · Corros. Sci. · 2001 · 43 · 169310.1016/S0010-938X(00)00167-0 ↗
26. Dussart · ECS Trans. · 2009 · 16 · 29710.1149/1.3229978 ↗
27. Burstein · Corros. Sci. · 1996 · 38 · 225710.1016/S0010-938X(97)83146-0 ↗
28. Laycock · J. Electrochem. Soc. · 1998 · 145 · 262210.1149/1.1838691 ↗
29. Garfias-Mesias · Corros. Sci. · 1999 · 41 · 95910.1016/S0010-938X(98)00165-6 ↗
30. Webb · J. Electrochem. Soc. · 2001 · 148 · B18610.1149/1.1360205 ↗
31. B. Baroux, D. Gorse, R. Oltra. Critical Factors in Localized Corrosion IV, in: E.C.S. proceedings, vol. 2002–24, 2003, pp. 335–346.
32. Frankel · Corrosion · 1987 · 43 · 42910.5006/1.3583880 ↗
33. H.S. Isaacs, Y. Zhu, R.L. Sabatini, M.P. Ryan. Critical Factors in Localized Corrosion III, in: E.C.S. proceedings, vol. 98–17, 1999, pp. 376–382.
34. Alkire · J. Electrochem. Soc. · 1978 · 125 · 138210.1149/1.2131682 ↗
35. Newman · Corros. Sci. · 1986 · 26 · 105710.1016/0010-938X(86)90133-2 ↗