Effects of ZrB2 and SiC dual addition on the oxidation resistance of graphite at 1600–2000°C
Source abstract
Abstract
Abstract The effects of ZrB2 and ZrB2 + SiC additions on the oxidation kinetics of graphite at 1600–2000 °C in air were investigated. The ZrB2 + SiC dual addition improves the oxidation resistance of graphite more effectively than the ZrB2 single addition, because the oxide scale formed on C–ZrB2–SiC is denser and thinner due to the existence of glassy SiO2. As the oxidation temperature increases, the oxidation rate of C–ZrB2–SiC gradually increases and oxide scales with layered microstructures form on its surface due to the greatly enhanced active oxidation of SiC at higher temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Materials for ultrahigh temperature structural applications
2. Oxidation-based materials selection for 2000°C+hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
3. W.G. Fahrenholtz, G.E. Hilmas, NSF–AFOSR joint workshop on future ultra-high temperature materials, Arlington VA, DMR-0403004, 2004.
4. The future of carbon–carbon composites10.1016/0008-6223(87)90116-3 ↗
5. Carbon–carbon, an overview
6. The influence of oxidation on the structure and strength of graphite-I: materials of different structure10.1016/0008-6223(82)90081-1 ↗
7. Oxidation behavior and protection of carbon/carbon composites10.1016/0008-6223(87)90197-7 ↗
8. Carbon–carbon composites: oxidation behavior and coatings protection
9. Resistance to ablation of pitch-derived ZrC/C composites10.1016/j.carbon.2004.05.006 ↗
10. Fabrication and oxidation behavior of a reaction derived graphite–ZrC composite for ultrahigh temperature applications10.1016/j.matlet.2009.07.022 ↗
11. The effect of zirconium carbide on ablation of carbon/carbon composite under an oxyacetylene flame10.1016/j.corsci.2010.09.028 ↗
12. Ultra-high temperature oxidation behavior of graphite-based composites reinforced by ZrC and ZrC–TaC
13. Effect of ZrB2 on the ablation properties of carbon composites10.1016/j.matlet.2005.10.040 ↗
14. Improved oxidation resistance of C–C composites using zirconium diboride and boron carbide10.1016/j.jeurceramsoc.2010.02.025 ↗
15. Oxidation of ZrB2-based ceramics in dry air10.1149/1.1618226 ↗
16. The ZrB2 volatility diagram10.1111/j.1551-2916.2005.00599.x ↗
17. Effect of an SiC addition on the oxidation of ZrB2
18. Oxidation of ZrB2–SiC ceramics under atmospheric and reentry conditions
19. Thermodynamic analysis of ZrB2–SiC oxidation: formation of a SiC-depleted region10.1111/j.1551-2916.2006.01329.x ↗
20. Zirconia transport by liquid convection during oxidation of zirconium diboride–silicon carbide10.1111/j.1551-2916.2007.02142.x ↗
21. Toward oxidation-resistant ZrB2–SiC ultra high temperature ceramics10.1007/s11661-010-0540-8 ↗
22. Oxidation-resistant ZrB2–SiC composites at 2200°C10.1016/j.compscitech.2007.08.017 ↗
23. Oxidation mechanism and resistance of ZrB2–SiC composite10.1016/j.corsci.2009.07.005 ↗
24. Oxidation of ZrB2–SiC ultra-high temperature ceramics over a wide range of SiC content10.1016/j.jeurceramsoc.2012.05.021 ↗
25. ZrB2–SiC leading edges in high enthalpy supersonic flows10.1111/j.1551-2916.2012.05226.x ↗
26. Ablation in different heat fluxes of C/C composites modified by ZrB2–ZrC and ZrB2–ZrC–SiC particles10.1016/j.corsci.2013.04.038 ↗
27. Effect of heat flux on ablation behaviour and mechanism of C/C–ZrB2–SiC composite under oxyacetylene torch flame10.1016/j.corsci.2013.04.052 ↗
28. Plasma wind tunnel testing of ultra-high temperature ZrB2–SiC composites under hypersonic re-entry conditions10.1016/j.jeurceramsoc.2010.01.029 ↗
29. Ultrahigh-temperature oxidation of Zr2Al3C4 via rapid induction heating10.1016/j.scriptamat.2008.12.002 ↗
30. Oxidation of carbon between 1000 and 2400°C10.1016/0008-6223(64)90288-X ↗
31. A theoretical and experimental study of carbon combustion in stagnation flow10.1016/0010-2180(90)90062-V ↗
32. Ablation behaviors of ultra-high temperature ceramic composites10.1016/j.msea.2007.02.040 ↗
33. Oxidation mechanism of a ZrB2–SiC–ZrC ceramic heated through high frequency induction at 1600°C10.1016/j.corsci.2011.03.024 ↗
34. NIST–JANAF Thermochemical Tables, .
35. Reactions between carbon and oxygen10.1039/tf9514700164 ↗
36. Mass transfer related to heterogeneous combustion of solid carbon in the forward stagnation region
37. Effect of temperature on graphite oxidation behavior10.1016/j.nucengdes.2003.11.004 ↗
38. Oxidation behaviour of zirconium diboride–silicon carbide ceramic composites under low oxygen partial pressure10.1016/j.corsci.2011.07.020 ↗
39. Modeling oxidation kinetics of SiC-containing refractory diborides10.1111/j.1551-2916.2011.04927.x ↗
40. The effect of a graphite addition on oxidation of ZrB2–SiC in air at 1500°C10.1016/j.jeurceramsoc.2012.09.016 ↗
41. Thermogravimetric study of the oxidation of ZrB2 in the temperature range of 800–1500°C10.1149/1.2408279 ↗
42. Evolution of structure during the oxidation of zirconium diboride–silicon carbide in air up to 1500°C10.1016/j.jeurceramsoc.2006.10.012 ↗
43. Effects of oxygen partial pressure and atomic oxygen on the microstructure of oxide scale of ZrB2–SiC composites at 1500°C10.1016/j.corsci.2013.03.023 ↗
44. Thermochemical and mechanical stabilities of the oxide scale of ZrB2+SiC and oxygen transport mechanisms10.1111/j.1551-2916.2008.02319.x ↗