Role of chlorides on pitting and hydrogen embrittlement of Mg–Mn wrought alloy
Source abstract
Abstract
Abstract The role of chlorides on stress corrosion cracking behavior of Mg–Mn hot rolled alloy was studied in Mg(OH) 2 saturated, 0.01 M and 0.1 M NaCl solutions. The alloy was found to fail by hydrogen embrittlement mechanism both in presence and absence of chlorides. However, the role of chloride has been found to be to damage the passive film, cause pitting and increasing hydrogen embrittlement tendency of the alloy. Crack initiation occurred through pitting and grew in a transgranular manner involving hydrogen.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Winzer · Adv. Eng. Mater. · 2005 · 7 · 65910.1002/adem.200500071 ↗
2. Padekar · Corros. Sci. · 2013 · 71 · 110.1016/j.corsci.2013.01.001 ↗
3. Chakrapani · Metall. Trans. · 1976 · A7 · 17310.1007/BF02644454 ↗
4. Winzer · Mater. Sci. Eng. A · 2008 · 472 · 9710.1016/j.msea.2007.03.021 ↗
5. Song · Mater. Sci. Eng. A · 2005 · 399 · 30810.1016/j.msea.2005.04.003 ↗
6. Winzer · Mater. Sci. Eng. A · 2007 · 466 · 1810.1016/j.msea.2007.03.020 ↗
7. Padekar · Mater. Sci. Forum · 2011 · 690 · 36110.4028/www.scientific.net/MSF.690.361 ↗
8. M.A. Timonova, In: I.A. Levin (Ed.), Intercrystalline corrosion and corrosion of metals under stress, Great Britain, 1962.
9. Stampella · Corros. Sci. · 1984 · 24 · 32510.1016/0010-938X(84)90017-9 ↗
10. Winzer · Mater. Sci. Eng. A · 2008 · 488 · 33910.1016/j.msea.2007.11.064 ↗
11. Kannan · Mater. Des. · 2012 · 42 · 32110.1016/j.matdes.2012.06.007 ↗
12. Ben-Hamu · Corros. Sci. · 2008 · 50 · 150510.1016/j.corsci.2008.02.012 ↗
13. Winzer · Corros. Sci. · 2009 · 51 · 195010.1016/j.corsci.2009.05.037 ↗
14. Marker · Corros. Sci. · 1993 · 34 · 131110.1016/0010-938X(93)90090-4 ↗
15. In Stress Corrosion Cracking Theory and Practice
16. Standard test method for determining average grain size, ASTM E 112-10.
17. Zhang · J. Alloy Compd. · 2008
18. Padekar · Eng. Fract. Mech. · 2013 · 102 · 18010.1016/j.engfracmech.2013.02.018 ↗
19. Birbilis · Corros. Sci. · 2009 · 51 · 68310.1016/j.corsci.2008.12.012 ↗
20. Coy · Corros. Sci. · 2010 · 52 · 389610.1016/j.corsci.2010.08.006 ↗
21. Neil · Corros. Sci. · 2009 · 51 · 38710.1016/j.corsci.2008.11.005 ↗
22. Neil · Corros. Sci. · 2011 · 53 · 329910.1016/j.corsci.2011.06.005 ↗
23. Pan · Mater. Sci. Eng. A · 2011 · 528 · 497310.1016/j.msea.2011.02.095 ↗
24. Friedrich · 2006
25. Wang · Mater. Sci. Eng. A · 2003 · 355 · 20110.1016/S0921-5093(03)00065-0 ↗
26. Logan · J. Res. Natl. Bur. Stand. · 1958 · 61 · 50310.6028/jres.061.043 ↗
27. Perryman · J. Inst. Met. · 1951 · 78 · 621
28. N.D. Tomashov, V.N. Modestova, in: I.A. Levin (Ed.), Intercrystalline Corrosion and Corrosion of Metals under Stress, Great Britain, 1962.
29. Fairman · Corros. Sci. · 1965 · 5 · 71110.1016/S0010-938X(65)80027-0 ↗
30. Fairman · Corros. Sci. · 1971 · 11 · 53310.1016/S0010-938X(71)80020-3 ↗
31. Fairman · Brit. Corros. J. · 1971 · 6 · 17010.1179/000705971798323829 ↗
32. Wearmouth · Corrosion · 1973 · 29 · 25110.5006/0010-9312-29.6.251 ↗
33. Meletis · Corros. Sci. · 1986 · 26 · 6310.1016/0010-938X(86)90124-1 ↗
34. Song · Corros. Sci. · 1998 · 40 · 176910.1016/S0010-938X(98)00078-X ↗
35. Song · Corros. Sci. · 1999 · 41 · 24910.1016/S0010-938X(98)00121-8 ↗
36. Song · J. Wuhan Univ. Technol. – Mater. Sci. Ed. · 2009 · 11110.1007/s11595-009-1111-y ↗
37. Kannan · Metall. Mater. Trans. · 2007 · 38A · 284310.1007/s11661-007-9303-6 ↗
38. Venugopal · Corrosion · 1996 · 52 · 13810.5006/1.3292104 ↗
39. Shi · Corros. Sci. · 2011 · 53 · 22610.1016/j.corsci.2010.09.016 ↗
40. Shi · Corros. Sci. · 2010 · 52 · 57910.1016/j.corsci.2009.10.016 ↗
41. Liu · Corros. Sci. · 2009 · 51 · 60210.1016/j.corsci.2008.12.015 ↗