Al2O3–ZrO2 mixed oxide composite incorporated aluminium rich zinc coatings for high wear resistance
Source abstract
Abstract
Abstract Corrosion resistance and wear resistance are the two important parameters for high performance of zinc galvanic coating. In the present work, the improvement of these two characteristics was achieved by the incorporation of Al 2 O 3 –ZrO 2 mixed oxide composite in the coating. Al 2 O 3 –ZrO 2 mixed oxide composite was synthesized from ZrOCl 2 ·8H 2 O. Aluminium rich zinc coatings with high sliding wear resistance was developed from a galvanic bath containing the mixed oxide. Based on the performance of the coating during physicochemical and electrochemical characterization, the concentration of mixed oxide composite in the bath was optimized as 0.50 wt% Al 2 O 3 –0.50 wt% ZrO 2 . While rich in Al–metal content in the coating caused high corrosion resistance, the incorporation of the mixed oxide improved structural characteristics of the coating resulting in high wear resistance also. The coating was nonporous in nature and even the interior layers had high stability. The coatings have potential scope for high industrial utility.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Magnesium Oxide Properties and Applications · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Identification of coating damage processes in corroded galvanized steel by acoustic emission wavelet analysis10.1016/j.surfcoat.2006.10.018 ↗
2. Fe–Zn (iron–zinc)10.1361/105497103772084598 ↗
3. The effect of alloying elements on the crystallization behavior and on the properties of galvanized coatings10.1002/crat.200310144 ↗
4. Development of nano CeO2-incorporated high performance hot dip zinc coatings10.1016/j.surfcoat.2008.04.090 ↗
5. Studies on the influence of metal oxides on the galvanic characteristics of hot dip zinc coating10.1016/j.surfcoat.2007.07.033 ↗
6. Electrochemical and structural characterization of the mixed oxides-reinforced hot dip zinc coating10.1016/j.surfcoat.2007.02.028 ↗
7. Incorporation of TiO2 in hot dip zinc coating for efficient resistance to biogrowth10.1016/j.surfcoat.2005.04.058 ↗
8. Start up and steady state friction of alumina against alumina10.1016/S0043-1648(97)00041-0 ↗
9. P.J. Balu, ASM Hand Book, Friction, Lubrication and Wear Technology, vol. 18, ASM International, USA, 1992.
10. Tribological and micro structural analysis of Al2O3/TiO2 nano composites to use in the femoral head of hip replacement10.1016/S0043-1648(03)00099-1 ↗
11. New design concept of structural ceramics–ceramic nano composite10.2109/jcersj.99.974 ↗
12. Synthesis and micro structural characterization of α-Al2O3–t-ZrO2 composite powders prepared by combustion technique10.1016/j.msea.2007.02.078 ↗
13. Composite wear resistant material based on aluminium oxide10.1023/A:1011332732698 ↗
14. Corrosion resistance of zinc–aluminium coatings obtained by hot dip metallization
15. Co-inhibition characteristics of sodium tungstate with potassium iodate on mild steel corrosion10.1016/j.corsci.2004.09.012 ↗
16. Assessment of corrosion resistance of surface coated galvanized steel by analysis of the AC impedance spectra measured on the salt spray tested specimen10.1007/s10008-006-0229-5 ↗
17. Electrochemical corrosion behavior of nano crystalline zinc coatings in 3.5wt% NaCl solutions10.1007/s10008-007-0293-5 ↗
18. The cathodic mass transport process during zinc corrosion in neutral aerated sodium sulphate solutions10.1016/0368-1874(84)83624-2 ↗
19. On porous electrodes in electrolyte solutions: 1. Capacitance effects10.1016/0013-4686(63)80042-0 ↗
20. Impedance studies of the growth of porous magnetite films on carbon steel in high temperature aqueous systems10.1016/0010-938X(83)90063-X ↗
21. Electrochemical corrosion characteristics of type 316 stainless steel in simulated anode environment for PEMFC10.1016/S0013-4686(03)00113-0 ↗
22. Influence of particle content and porosity on the behavior of cast in situ Al (Mn)–Al2O3 (MnO2) composite10.1016/j.wear.2005.02.120 ↗
23. Prediction of wear coefficient of Al 6061–TiO2 composites10.1016/j.wear.2005.02.115 ↗
24. The effects of an Fe–Zn intermetallic containing coating on the stress corrosion cracking behavior of a hot dip galvanized steel10.1016/S0257-8972(01)01017-9 ↗
25. Iron–zinc phases important in hot galvanizing
26. Kubaschewski · 1982
27. Thermodynamic description of the iron–zinc system
28. Massalski · 1990
29. The origin of striations on the surface of iron–zinc coated steel sheet produced by hot-dip galvannealing10.1023/A:1018551011111 ↗
30. Characterization of intermediate layers in hot dip zinc coated steels10.1007/s002160050364 ↗
31. Lepretre · 1998 · 95
32. Studies of the morphology of the Al-rich interfacial layer formed during the hot dip galvanizing of steel sheet10.1007/s11661-999-1000-1 ↗
33. Surface chemistry of galvanized steel sheets relevant to adhesion performance10.1016/0300-9440(95)00610-9 ↗
34. Evaluation of the corrosion behavior of galvannealed steel in chloride aqueous solution in tropical marine environment10.1007/s10800-005-9083-x ↗
35. A.C. impedance measurement of cystine adsorption at mild steel/sulfuric acid interface as corrosion inhibitor10.1007/s10008-008-0551-1 ↗
36. Electrochemical impedance spectroscopy (EIS) of corrosion process on inhomogeneous surfaces10.1016/0013-4686(90)80004-8 ↗
37. A fitting procedure for impedance data of systems with very low corrosion rates10.1016/0010-938X(89)90070-X ↗