journal article·2016-01

Effects of pre-formed nanostructured surface layer on oxidation behaviour of 9Cr2WVTa steel in air and liquid Pb–Bi eutectic alloy

Y.H. Lu, Z.B. Wang, Y.Y. Song, L.J. Rong

Corrosion Science· Volume 102
Publisher page

Abstract

Abstract A nanostructured surface layer was pre-formed on a 9Cr2WVTa reduced activation ferritic/martensitic steel sample by means of surface mechanical rolling treatment (SMRT). In comparison with the initial sample, oxidation experiments at 600 °C in air showed that the oxidation resistance of the SMRT sample is markedly enhanced, due to the formation of a more continuous, homogenous, and compact oxide scale enriched with Mn. Furthermore, oxidation experiments at 550 °C in oxygen-saturated liquid Pb–Bi eutectic alloy showed that the oxidation resistance is improved on the SMRT sample after pre-oxidation in air, due to depressed diffusivities in the pre-formed oxide scale.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ion-surface interactions and analysis · High-Temperature Coating Behaviors · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Ferritic/martensitic steels for next-generation reactors10.1016/j.jnucmat.2007.05.005 ↗
2. Technical issues related to the development of reduced-activation ferritic/martensitic steels as structural materials for a fusion blanket system10.1016/j.fusengdes.2011.04.047 ↗
3. Elevated temperature ferritic and martensitic steels and their application to future nuclear reactors10.1179/174328005X41140 ↗
4. Control of precipitation behaviour in reduced activation steels by intermediate heat treatment10.1016/j.msea.2011.05.084 ↗
5. MYRRHA: a multipurpose accelerator driven system for research & development10.1016/S0168-9002(01)00164-4 ↗
6. OECD/NEA Nuclear Science Committee · 2007
7. Oxidation mechanism of an Fe-9Cr-1Mo steel by liquid Pb–Bi eutectic alloy at 470°C (Part II)10.1016/j.corsci.2008.06.051 ↗
8. Liquid metal corrosion of T91 and A316L materials in Pb–Bi eutectic at temperatures 400–600°C10.1016/j.corsci.2005.04.001 ↗
9. A review of steel corrosion by liquid lead–bismuth10.1016/j.corsci.2009.03.013 ↗
10. Investigation on oxygen controlled liquid lead corrosion of surface treated steels10.1016/S0022-3115(99)00211-1 ↗
11. Influence of temperature on the interaction mode of T91 and AISI 316L steels with Pb–Bi melt saturated by oxygen10.1016/j.corsci.2008.02.006 ↗
12. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb–Bi eutectic alloy (Part III)10.1016/j.corsci.2008.06.049 ↗
13. Nanoscale assembly of high-temperature oxidation-resistant nanocomposites10.1039/B9NR00118B ↗
14. The effect of nanocrystallization on the selective oxidation and adhesion of Al2O3 scales10.1007/BF01670500 ↗
15. Diffusion of chromium in nanocrystalline iron produced by means of surface mechanical attrition treatment10.1016/S1359-6454(03)00260-X ↗
16. Surface nanocrystallization (SNC) of metallic materials-presentation of the concept behind a new approach
17. Nanostructured surface layer on metallic materials induced by surface mechanical attrition treatment10.1016/j.msea.2003.10.261 ↗
18. Revealing extraordinary intrinsic tensile plasticity in gradient nano-grained copper10.1126/science.1200177 ↗
19. Fatigue behaviour of AISI 316L stainless steel with a gradient nanostructured surface layer10.1016/j.actamat.2014.12.057 ↗
20. Enhancing torsion fatigue behaviour of a martensitic stainless steel by generating gradient nanograined layer via surface mechanical grinding treatment10.1179/1743284712Y.0000000192 ↗
21. Nitriding iron at lower temperatures10.1126/science.1080216 ↗
22. Enhanced reactive diffusion of Zn in a nanostructured Fe produced by means of surface mechanical attrition treatment10.1016/j.actamat.2011.12.016 ↗
23. Grain size effects on the austenitization process in a nanostructured ferritic steel10.1016/j.actamat.2011.03.006 ↗
24. Chang · 2010
25. Diffusion of Mn54 in iron and iron–manganese alloys
26. Relation entre les Phenomenes de diffusion du Fer et du chrome radioactifs dans les alliages Fer-Chrome de 0 a 15% de Chrome et leur transformation α=(α+γ)
27. The effect of manganese additions on the reactive evaporation of chromium in Ni–Cr alloys10.1016/j.scriptamat.2006.01.026 ↗
28. Effect of component thickness on lifetime and oxidation rate of chromia forming ferritic steels in low and high pO2 environments10.1179/mht.2005.029 ↗
29. Thermal stability and the structure of vacancy–solute clusters in iron alloys10.1016/j.actamat.2014.11.026 ↗
30. Effects of dilute substitutional solutes on interstitial carbon in α-Fe: interactions and associated carbon diffusion from first-principles calculations
31. Grain boundary excess volume and defect annealing of copper after high-pressure torsion10.1016/j.actamat.2013.12.036 ↗
32. Deformation induced percolating porosity in high pressure torsioned (HPT) copper
33. Diffusion of Cr in nanostructured Fe and low carbon steel produced by means of surface mechanical attrition treatment10.4028/www.scientific.net/DDF.249.147 ↗
34. Kofstad · 1988
35. Oxide growth and spalling on Fe–Cr alloys studied by hot stage microscopy10.1016/S0010-938X(68)80130-1 ↗
36. Oxidation resistance of nanocrystalline alloys
37. The high-temperature oxidation of cobalt-21wt.% chromium-3vol.% Y2O3 alloys10.1007/BF00614619 ↗
38. Wagner · Z. Elektrochem. · 1959 · 63 · 772
39. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb–Bi eutectic alloy (Part I)10.1016/j.corsci.2008.06.050 ↗
40. M. Caro, T. Zalesky, P. Hosemann, B.S. El-dasher, W.G. Halsey, B. Stuart, Thermal effects on thin laser-peened ferritic-martensitic samples, Laser Science and Technology Program, UCRL-TR-231687, Lawrence Livermore National Laboratory, Livermore, CA,
41. Influence of the surface mechanical pulsed treatment on the oxidation of Fe-0.2C-13Cr-0.3Si steel in lead melts10.1007/s11003-010-9236-x ↗
42. Some observations on the compatibility ofstructural materials with molten lead10.1016/S0010-938X(77)80001-2 ↗