Microstructure and chemical composition of the oxide scale formed on the sanicro 25 steel tubes after fireside corrosion
Source abstract
Abstract
Abstract The Sanicro 25 austenitic steel is foreseen as a potential material for steam superheaters and reheaters in ultra-supercritical power plants. The aim of investigation was to characterize in detail an oxide scale grown on the Sanicro 25 tube after fireside oxidation at 650 °C. The morphology of the oxide scale and the microstructure of the bulk material were investigated using advanced electron microscopy methods. A multilayered and multicomponent oxide scale containing mainly Cr2O3 was found on the surface exposed to combustion gases. Directly under the oxide scale, a chromium-depleted zone with no M23C6 carbides was observed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. U.S. Program on materials technology for ultra-supercritical coal power plants10.1007/s11665-013-0717-6 ↗
2. Alloy for ultrasupercritical coal fired boilers
3. Creep behavior and microstructure evolution at 750°C in a new precipitation-strengthened heat-resistant austenitic stainless steel10.1016/j.msea.2012.07.090 ↗
4. WB 559/2, Hochwarmfeste Nickelbasislegierung HR6W Nahtloses Rohr, VdTÜV Merkblätter. (2012).
5. SANDVIK, (2015). http://www.smt.sandvik.com.
6. WB 555, Warmfester austenitischer Stahl, Sanicro® 25, VdTÜV Merkblätter. (2008).
7. Oxidation behaviour of Sanicro 25 (42Fe22Cr25NiWCuNbN) in O2/H2O mixture at 600°C10.1007/s11085-011-9281-3 ↗
8. Microstructural stability and oxidation behavior of Sanicro 25 during long-term steam exposure in the temperature range 600–750°C10.1002/maco.201407901 ↗
9. Enhanced oxidation of the 9% Cr steel P91 in water vapour containing environments10.1016/j.corsci.2006.02.002 ↗
10. Performance of chromia- and alumina-forming Fe- and Ni-base alloys exposed to metal dusting environments: the effect of water vapor and temperature10.1016/j.corsci.2014.11.022 ↗
11. Corrosion of Fe–9Cr–(Mn, Si) alloys in CO2–H2O–SO2 gases10.1016/j.corsci.2015.05.040 ↗
12. Effects of cerium and manganese on corrosion of Fe–Cr and Fe–Cr–Ni alloys in Ar–20CO2 and Ar–20CO2–20H2O gases at 650°C10.1016/j.corsci.2015.08.012 ↗
13. Surface phase transformation in austenitic stainless steel induced by cyclic oxidation in humidified air10.1016/j.corsci.2015.08.030 ↗
14. Advanced STEM/EDX investigation on an oxide scale thermally grown on a high-chromium iron-nickel alloy under very low oxygen partial pressure10.1016/j.corsci.2015.09.021 ↗
15. Hot corrosion of materials: fundamental studies10.1007/BF03222665 ↗
16. Hot corrosion of metals and alloys10.1007/s11085-011-9254-6 ↗
17. Investigation of the mechanisms of Type-II hot corrosion of superalloy CMSX-410.1016/j.corsci.2013.11.048 ↗
18. Effect of temperature on coal ash hot corrosion resistance of Inconel 740 superalloy10.1016/j.corsci.2014.01.020 ↗
19. Role of tantalum in the hot corrosion of a Ni-base single crystal superalloy10.1016/j.corsci.2015.05.066 ↗
20. Corrosion of metals and alloys in mixed gas environments at elevated temperatures10.1007/BF00603609 ↗
21. Kinetics of breakaway oxidation of Fe–Cr and Fe–Cr–Ni alloys in dry and wet carbon dioxide10.1016/j.corsci.2013.08.008 ↗
22. L. Intiso i O. Tassa, Corrosion of superheater materials—full scale test loops, in: ISHOC-2014, Int. Symp. High-Temperature Oxid. Corros., 2014: pp. 87–89.
23. The fireside corrosion of HR6W and Sanicro 25 austenitic alloys
24. P. Stadelmann, JEMS Java Electron Microscopy Software, (2015). http://cime.epfl.ch/.
25. Precipitation in creep resistant austenitic stainless steels10.1179/026708301101508972 ↗
26. Influence of high temperature on a microstructure of HR6W alloy for advanced steam power plants
27. Numerical simulation of long-term precipitate evolution in austenitic heat-resistant steels10.1016/j.calphad.2010.01.001 ↗
28. Development of high strength interstitial free steel by copper precipitation hardening10.1016/j.matlet.2006.10.037 ↗
29. Effect of Cu content on aging precipitation behaviors of Cu-rich phase in Fe–Cr–Ni alloy10.1016/S1006-706X(10)60101-X ↗
30. Evaluation of welded joints properties and microstructure of new austhenitic steels Sanicro 25 and HR6W
31. Antibacterial properties, corrosion resistance and mechanical properties of Cu-modified SUS 304 stainless steel10.1016/j.msea.2004.10.032 ↗
32. Effect of aging on antibacterial performance of Cu-bearing martensitic stainless steel10.1179/1753555714Y.0000000156 ↗
33. Study of copper precipitation behavior in a Cu-bearing austenitic antibacterial stainless steel10.1016/j.matdes.2010.11.030 ↗
34. Analysis of iron oxidation at high temperatures10.1021/ie00037a028 ↗
35. Review of the high-temperature oxidation of iron and carbon steels in air or oxygen10.1023/A:1023685905159 ↗
36. On the high-temperature oxidation of nickel10.1016/S0010-938X(02)00085-9 ↗
37. Effect of oxide grain structure on the high-temperature oxidation of Cr10.1007/BF00611694 ↗
38. S. Mrowec, T. Weber, Gas Corrosion of Metals, Warsaw, Poland, 1978 Published for The National Bureau of Standards and The National Science Foundation, Washington, DC, by Foreign Scientific Publications Department of the National Center for Science Technical and Economical Information, Original book: Korozja gazowa metali, Wydawnictwo “Śląsk” 1975.
39. Chromia scale growth in alloy oxidation and the reactive element effect10.1149/1.2220920 ↗
40. The reactive element effect in high-temperature corrosion10.1016/0921-5093(89)90730-2 ↗
41. Oxygen and silicon diffusion-controlled processes in vitreous silica10.1016/0022-3093(80)90493-7 ↗
42. The mechanism of oxygen diffusion in vitreous SiO210.1149/1.2123847 ↗