journal article·2016-10

On-line monitoring of oxide formation and dissolution on alloy 800H in supercritical water

Kashif I. Choudhry, David A. Guzonas, Dimitrios T. Kallikragas, Igor M. Svishchev

Corrosion Science· Volume 111
Publisher page

Abstract

Concentrations of dissolved metals, oxygen and hydrogen at the exit of an Alloy 800H tube exposed to oxygenated supercritical water were monitored to study the initial stages of oxidation. Initially, both water and oxygen are oxidants, generating H2, releasing low concentrations of Fe, Al, Ni and Mn. All added oxygen is consumed during this period. No Cr release is observed during these initial stages, attributed to Mn incorporation in the oxide. Rapid reappearance of oxygen in the water is attributed to thickening of the surface oxide. Manganese dissolution results in Cr release and formation of an outer iron oxide layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Subcritical and Supercritical Water Processes · High-Temperature Coating Behaviors · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. World Nuclear Association · 2015
2. Supercritical water-cooled reactor (SCWR) development through GIF collaboration
3. Supercritical water-cooled reactor materials—summary of research and open issues10.1016/j.pnucene.2014.02.008 ↗
4. Water chemistry in a supercritical water-cooled pressure tube reactor10.13182/NT12-A14093 ↗
5. Corrosion and stress corrosion cracking of austenitic stainless steels
6. Corrosion and stress corrosion cracking of Ni-base alloys
7. Corrosion of zirconium alloys
8. Selection of fuel cladding material for nuclear fission reactors10.1016/j.engfailanal.2011.06.010 ↗
9. Materials assessment for the Canadian SCWR core concept10.1007/s11837-015-1758-0 ↗
10. Development of high-performance pressure tube material for the Canadian SCWR concept10.1007/s11837-015-1750-8 ↗
11. Corrosion behavior of stainless steel 316 in sub- and supercritical aqueous environments: effect of LiOH additions10.1016/j.corsci.2013.02.005 ↗
12. Hydrogen evolution rate during the corrosion of stainless steel in supercritical water10.1016/j.corsci.2014.02.019 ↗
13. Alloy 800H under supercritical water conditions: a flow reactor study of corrosion and hydrogen evolution10.1002/maco.201508315 ↗
14. Supercritical water convection loop for SCWR materials corrosion tests under electron irradiation: first results and lessons learned
15. Supercritical water convection loop (NSC KIPT) for materials assessment for the next generation reactors
16. A Strategy in developing heat-transfer correlation for fuel assembly of the Canadian super-critical water-cooled reactor
17. Assessment of candidate fuel cladding alloys for the Canadian supercritical water-cooled reactor concept
18. Development of kinetic models for the long-term corrosion behaviour of candidate alloys for the Canadian SCWR
19. A comparative study of oxide scales grown on stainless steel and nickel-based superalloys in ultra-high temperature supercritical water at 800°C10.1016/j.corsci.2016.02.004 ↗
20. Microstructure stability of candidate stainless steels for Gen-IV SCWR fuel cladding application10.1016/j.jnucmat.2014.06.043 ↗
21. Development of Al added high-Cr ODS steels for fuel cladding of next generation nuclear systems10.1016/j.jnucmat.2010.12.300 ↗
22. Corrosion behavior of alloy 800H (Fe–21Cr–32Ni) in supercritical water10.1016/j.corsci.2010.10.021 ↗
23. Thermodynamic assessment of high-temperature oxidation of Fe-Cr alloys in air10.1007/s10789-005-0087-z ↗
24. Pourbaix diagrams for chromium, aluminum and titanium extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2012.02.002 ↗
25. The reproducibility of corrosion testing in supercritical water—results of an international interlaboratory comparison exercise10.1016/j.corsci.2016.01.034 ↗
26. Corrosion of engineering materials in a supercritical water cooled reactor: characterization of oxide scales on alloy 800H and stainless steel 31610.1016/j.corsci.2015.07.035 ↗
27. Pourbaix diagrams for the iron–water system extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2011.10.034 ↗
28. Effect of Cr content on corrosion resistance of Fe-Cr-Ni alloys exposed in Supercritical Water (SCW)
29. The effects of water vapor and hydrogen on the high-temperature oxidation of alloys10.1007/s11085-012-9349-8 ↗
30. Hydrogen emission during the steam oxidation of ferritic steels: kinetics and mechanism10.1016/0010-938X(89)90086-3 ↗
31. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: a review10.1016/j.pmatsci.2007.11.001 ↗
32. Molecular dynamics simulations of supercritical water at the iron hydroxide surface10.1016/j.supflu.2013.03.016 ↗
33. Properties of aqueous systems relevant to the SCWR via molecular dynamics simulations10.12943/ANR.2015.00041 ↗
34. The physical chemistry of corrosion in a supercritical water-cooled reactor
35. Cycle chemistry and its effect on materials in a supercritical water-cooled reactor: a synthesis of current understanding10.1016/j.corsci.2012.08.006 ↗
36. Effect of Al and Ti addition on performance of stainless steel 310 in supercritical water10.1179/1743278214Y.0000000225 ↗
37. The effect of manganese additions on the reactive evaporation of chromium in Ni–Cr alloys10.1016/j.scriptamat.2006.01.026 ↗
38. Activity transport in a supercritical water-cooled reactor