journal article·2016-11

Role of irradiation-induced defects on SiC dissolution in hot water

Sosuke Kondo, Shinichiro Mouri, Yoshihiro Hyodo, Tatsuya Hinoki, Fumihisa Kano

Corrosion Science· Volume 112
Publisher page

Abstract

Abstract An enhancement of the dissolution of high-purity 3C-SiC in hot water (320 °C, 20 MPa: relevant to the light-water reactor coolant condition) is demonstrated after 5.1 MeV Si-ion irradiation. Optical spectrometry and Kelvin force microscopy revealed the creation of interband-defect localized states within the bandgap. The dissolution rate was found to be dependent on the irradiation fluence, irradiation-induced volume expansion, and the photoluminescence quenching. An annealing study showed prevention of irradiation-enhanced dissolution with the recovery of most defects. These results show that the dissolution rates of irradiated SiC are increased with the population of irradiation-induced defects.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon Carbide Semiconductor Technologies · Semiconductor materials and devices · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Dobisesky · 2011
2. Accident tolerant fuels for LWRs: a perspective10.1016/j.jnucmat.2013.12.005 ↗
3. Pitting corrosion in CVD SiC at 300°C in deoxygenated high-purity water10.1016/j.jnucmat.2008.03.025 ↗
4. Long-term corrosion behavior of CVD SiC in 360°C water and 400°C steam10.1016/j.jnucmat.2013.07.058 ↗
5. Radiation-induced material changes and susceptibility to intergranular failure of light-water-reactor core internals10.1016/S0022-3115(99)00075-6 ↗
6. Microstructural defects in SiC neutron irradiated at very high temperatures10.1016/j.jnucmat.2008.08.013 ↗
7. Effect of irradiation damage on hydrothermal corrosion of SiC10.1016/j.jnucmat.2015.04.034 ↗
8. Corrosion behavior of silicon carbide in 290°C water10.1111/j.1151-2916.1989.tb06029.x ↗
9. Low-temperature oxidation hydrothermal corrosion, and their effects on properties of SiC (Tyranno) fibers10.1111/j.1151-2916.1995.tb08835.x ↗
10. Hydrothermal corrosion of nitride and carbide of silicon10.1016/S0254-0584(00)00434-X ↗
11. Corrosion of silicon carbide ceramics and silicon nitride ceramics in high-temperature water
12. Thermodynamic potential for the anodic dissolution of n-type semiconductors10.1149/1.2133140 ↗
13. Electrolytic decomposition and photodecomposition of compound semiconductors in contact with electrolytes10.1116/1.569800 ↗
14. The role of energy levels in semiconductor-electrolyte solar cells10.1149/1.2131374 ↗
15. Broad area photoelectrochemical etching of n-type beta-SiC10.1149/1.2220722 ↗
16. A new multiple beams–material interaction research facility for radiation damage studies in fusion materials10.1016/S0920-3796(00)00181-2 ↗
17. Analysis of grain boundary sinks and interstitial diffusion in neutron-irradiated SiC10.1103/PhysRevB.83.075202 ↗
18. The influences of irradiation temperature and helium production on the dimensional stability of silicon carbide10.1016/S0022-3115(02)01062-0 ↗
19. Microstructural development in cubic silicon carbide during irradiation at elevated temperatures10.1016/j.jnucmat.2006.02.007 ↗
20. Annealing properties of defects in ion-implanted 3C-SiC studied using monoenergetic positron beams10.1143/JJAP.36.6650 ↗
21. Positron annihilation studies of defects in 3C-SiC hot-implanted with nitrogen and aluminum ions10.1007/s003390050585 ↗
22. Dominant recombination center in electron-irradiated 3C SiC10.1063/1.361214 ↗
23. Electron spin resonance in electron-irradiated 3C-SiC10.1063/1.343920 ↗
24. Electron spin resonance study of defects in CVD-grown 3C-SiC irradiated with 2MeV protons10.1007/BF02655600 ↗
25. Defects in neutron irradiated SiC10.1063/1.97941 ↗
26. Mean field rate theory and object kinetic Monte Carlo: a comparison of kinetic models10.1016/j.jnucmat.2008.08.047 ↗
27. Kelvin probe force microscopy10.1063/1.105227 ↗
28. High-resolution atomic force microscopy potentiometry10.1116/1.585423 ↗
29. Defects in cubic SiC on Si10.1080/10420159008213033 ↗
30. Mechanism of Fermi-level stabilization in semiconductors10.1103/PhysRevB.37.4760 ↗
31. Optical characterization of deep O implants in GaAs10.1063/1.323873 ↗
32. Optical properties of defects in ion implanted silicon carbide probed at λ=633nm10.1063/1.118142 ↗
33. Defect annealing in ion implanted silicon carbide10.1557/JMR.1997.0238 ↗
34. Low-temperature photoluminescence studies of chemical-vapor-deposition-grown 3C-SiC on Si10.1063/1.341532 ↗
35. Theoretical descriptions of porous silicon10.1016/0040-6090(94)05626-O ↗