journal article·2015-09

Effect of thermal cycling on protective properties of alumina scale grown on thin Haynes 214 foil

A. Chyrkin, N. Mortazavi, M. Halvarsson, D. Grüner, W.J. Quadakkers

Corrosion Science· Volume 98
Publisher page

Abstract

The isothermal and cyclic oxidation of a thin alloy 214 foil (130μm thick) has been studied in air at 1200°C for up to 720 h. Haynes 214 forms a duplex oxide scale consisting of pure, columnar alumina overlaid by mixed Ni(Al,Cr) 2 O 4 spinel with minor inclusions of (Al,Cr) 2 O 3 . A transition from external alumina to chromia scaling (abbreviated as TACS) occurs at the oxide-alloy interface after the Al reservoir of the foil is exhausted due to oxidation. The tensile cracking of the oxide scale upon thermal cycling is shown to promote the early transition from protective to accelerated breakaway oxidation. © 2015 Elsevier Ltd.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Catalytic Processes in Materials Science · Magnesium Oxide Properties and Applications · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Metallic interconnectors for solid oxide fuel cells – a review
2. Boyce · 2012
3. Hünecke · 1997
4. Fraas · 1989
5. Candidate materials for advanced power generating plants and high temperature heat exchangers
6. Jones · 1989
7. Young · 2008
8. A comparison of oxidation behavior of Fe–Cr–Al, Ni–Cr–Al, and Co–Cr–Al alloys10.1007/BF00603481 ↗
9. The mechanism of oxidation of Ni–Cr–Al alloys at 1000°–1200°C10.1016/S0010-938X(71)80044-6 ↗
10. Oxidation behavior of some Ni–Cr–Al alloys at hight temperatures10.1007/BF02643040 ↗
11. ThyssenKruppVDM, Nicrofer® 6025HT – alloy 602CA, Material data sheet No. 4137, 2007.
12. Haynes 214 – Data sheet, Haynes international, 2011.
13. Long-term cyclic oxidation behavior of selected high temperature alloys
14. High-temperature oxidation performance of a new alumina-forming Ni–Fe–Cr–Al alloy in flowing air10.1016/j.ijhydene.2010.04.099 ↗
15. D.J. Young, A. Chyrkin, J. He, D. Grüner, W.J. Quadakkers, Slow Transition from Protective to Breakaway Oxidation of Haynes 214 Foil at High Temperature Oxidation of Metals, (2013) 405–427.10.1007/s11085-013-9364-4 ↗
16. Silicon and chromium depletion during the long-term oxidation of thin-sectioned austenitic steel10.1023/A:1018808925756 ↗
17. Effect of component thickness on lifetime and oxidation rate of chromia forming ferritic steels in low and high pO2 environments10.1179/mht.2005.029 ↗
18. Chromium depletion at 2-dimensional features during the selective oxidation of a 20Cr–25Ni austenitic steel10.1007/s11085-006-9039-5 ↗
19. Aluminium depletion in FeCrAlY steel during transitional alumina formation10.3184/096034005782744218 ↗
20. Oxidation-induced lifetime limits of thin-walled iron-based, alumina forming, oxide dispersion-strengthened alloy components10.1179/mst.1994.10.2.126 ↗
21. Two calculations concerning the critical aluminium content in Fe20Cr5Al alloys10.1002/maco.200503878 ↗
22. Lifetime extension of FeCrAIRE alloys in air: potential roles of an enhanced Al-reservoir and surface pretreatment10.1002/maco.200503916 ↗
23. Factors governing breakaway oxidation of FeCrAl-based alloys10.1002/(SICI)1521-4176(200004)51:4<224::AID-MACO224>3.0.CO;2-B ↗
24. Oxidation limited life of FeCrAl based alloys during thermal cycling
25. The prediction of breakaway oxidation for alumina forming ODS alloys using oxidation diagrams10.1002/maco.19940450404 ↗
26. Oxidation behavior of Fe–25Cr–20Ni-2.8Si during isothermal oxidation at 1286K; life-time prediction10.1007/s11085-008-9097-y ↗
27. A simple expression for predicting the oxidation limited life of thin components manufactured from FCC high temperature alloys10.1007/s11085-012-9283-9 ↗
28. R. Brück, Metallic honeycomb body e.g. particle separator, manufacturing method for use in exhaust gas system of mobile internal combustion engine of motor vehicle, involves forming material-fit connection points at part of boundary points, Patent No.WO2010122006-A1, Emitec Emissionstechnologie GmbH, 2000.
29. O. Fourier, Producing metallic catalyst support used to purify exhaust gases, comprises preparing first and second metal foils and an external cylinder, rolling up the metal foils, fitting honeycomb body into external cylinder and applying pressure, Patent No.US2014000077-A1, Calsonic Kansei Corp, 2012.
30. Y. Okazaki, M. Kasuya, A. Suzuki, Y. Yamakawa, H. Tamura, Metallic carrier for exhaust gas purification catalyst, Patent No. WO200126808-A, Nippon Steel Corp; Fuji Jukogyo Kk; Fuji Heavy Ind Ltd, 2006.
31. Development of advanced metallic filters for hot gas cleaning
32. M. Schober, S. Sikorski, A. Werner, Abradable coating for arrangement at aircraft engine housing of e.g. high pressure gas turbine, has form-stabilizing honeycomb-shaped reinforcement element embedded in elastomer sealing body, where element comprises glass fibers, Patent No. DE102009034025-A1, MTU Aero Engines GmbH, 2009.
33. The capability of transmission Kikuchi diffraction technique for characterizing nano-grained oxide scales formed on a FeCrAl stainless steel10.1016/j.matlet.2015.02.008 ↗
34. A TEM study of the oxide scale development in Ni–Cr–Al alloys10.1016/S0010-938X(03)00100-8 ↗
35. Growth and microstructure of α-Al2O3 on Ni–Al alloys – internal precipitation and transition to external scale10.1149/1.2129964 ↗
36. The effect of water vapor on oxidation performance of alloys used in recuperators10.1115/GT2002-30543 ↗
37. Chromium volatilization rates from Cr2O3 scales into flowing gases containing water vapor10.1007/s11085-006-9030-1 ↗
38. Characterization of the breakaway Al content in alumina-forming alloys10.1179/mht.2004.021 ↗
39. Reaction mechanism in alumina/chromia (Al2O3–Cr2O3) solid solutions obtained by coprecipitation10.1111/j.1151-2916.2000.tb01508.x ↗
40. Electrochemical determination of activities in Cr2O3–Al2O3 solid-solution10.1149/1.2131408 ↗
41. Oxygen and aluminum diffusion in alpha-Al2O3: how much do we really understand?10.1016/j.jeurceramsoc.2007.12.020 ↗
42. Oxidation mechanism for nickel–aluminum alloys at temperatures between 900° and 1300°C
43. Oxidation of Ni–Cr–Al Alloys between 1000° and 1200°C10.1149/1.2407837 ↗
44. Transient oxidation of a gamma-Ni–28Cr–11Al Alloy10.1007/s11085-009-9179-5 ↗
45. Oxide phase development upon high temperature oxidation of gamma-NiCrAl alloys10.1002/maco.200503934 ↗
46. The third-element effect in the oxidation of Ni–xCr–7Al (x=0, 5, 10, 15at.%) alloys in 1atm O2 at 900–1000°C10.1016/j.corsci.2006.03.008 ↗
47. The Thermo-Calc database system
48. Cracking and spalling of protective oxides10.1016/0921-5093(89)90731-4 ↗
49. Stress effects in high-temperature oxidation of metals10.1179/imr.1995.40.1.1 ↗
50. The oxidation of metals at high temperatures
51. The healing behaviour of protective oxide scales on heat-resistant steels after cracking under tensile strain10.1007/BF01072918 ↗
52. Deformation and cracking behaviour of protective oxide scales on heat-resistant steels under tensile strain10.1007/BF00664232 ↗
53. Tensile cracking of a chromia layer on a stainless steel during thermal cycling with hold periods10.1016/j.msea.2005.08.193 ↗
54. Mechanisms of breakaway oxidation and application to a chromia-forming steel10.1023/A:1018855914737 ↗
55. The diffusion and solubility of oxygen in solid nickel10.1007/BF02646220 ↗
56. Effect of specimen thickness on the growth rate of chromia scales on Ni-base alloys in high- and low-pO2 gases10.1016/j.jallcom.2007.12.015 ↗
57. Thermodynamic modeling of oxidation of Al–Cr–Ni alloys10.1016/j.jallcom.2004.02.053 ↗
58. Metal–spinel–corundum three phase equilibria in the system Ni–Cr–Al–O at 1373K