Effects of microtexture and Ti3Al (α2) precipitates on stress-corrosion cracking properties of a Ti-8Al-1Mo-1V alloy

Sheng Cao, Chao Voon Samuel Lim, Bruce Hinton, Xinhua Wu

Corrosion Science· Volume 116

Abstract

Abstract Effects of microtexture and Ti3Al (α2) precipitates on the Stress-Corrosion Cracking (SCC) properties of Ti-8Al-1Mo-1V (Ti-811) have been investigated using a constant displacement SCC test in 0.1 M aqueous sodium chloride (NaCl) solution. SEM, TEM, and EBSD were employed to characterize microstructure and microtexture. Results reveal that both microtexture and α2 precipitates increase the SCC susceptibility of Ti-811. The SCC propagation direction aligns with microtextured regions, and most α grains were preferentially orientated for basal slip along the SCC crack. SCC susceptibility was eliminated by implementing hot isostatic pressing (HIPping) and post heat-treatment processes through eliminating both crystallographic microtexture and α2 precipitates. Fractography showed that the formation mechanism of the propagation facets could be attributed to Hydrogen Enhanced Localized Plasticity (HELP).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Titanium Alloys Microstructure and Properties · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Titanium in the family automobile: the cost challenge10.1007/s11837-004-0144-0 ↗
2. Magnesium alloy applications in automotive structures10.1007/s11837-008-0150-8 ↗
3. Progress in structural materials for aerospace systems110.1016/j.actamat.2003.08.023 ↗
4. Titanium alloys for aerospace applications10.1002/adem.200310095 ↗
5. New trends in the development of mechanical engineering materials10.1016/S0924-0136(00)00619-1 ↗
6. Leyens · 2003
7. Advanced metals for aerospace and automotive use10.1016/0921-5093(94)91026-X ↗
8. Donachie · 2000
9. Boyer · 1994
10. Lutjering · 2007
11. Stress corrosion cracking facet crystallography of Ti-8Al-1Mo-1V10.1016/j.corsci.2010.05.046 ↗
12. The role of hydrogen in the stress corrosion cracking of titanium alloys10.1016/0010-938X(74)90005-5 ↗
13. Corrosion behavior of Ti–8Al–1Mo–1V alloy compared to Ti–6Al–4V10.1016/j.matdes.2010.09.009 ↗
14. Corrosion and passivity of Ti-13%Nb-13%Zr in comparison to other biomedical implant alloys10.5006/1.3290281 ↗
15. Electrochemical stability of anodic titanium oxide films grown at potentials higher than 3V in a simulated physiological solution10.1016/j.corsci.2006.08.010 ↗
16. Stress corrosion cracking (SCC) and hydrogen-assisted cracking in titanium alloys
17. Metallurgical aspects of the stress corrosion cracking of titanium alloys
18. Microstructure and slip character in titanium alloys10.14429/dsj.36.5971 ↗
19. Joshi · 2006
20. The effect of aluminium on twinning in binary alpha-titanium10.1016/j.actamat.2015.09.048 ↗
21. Some Characteristics of Aqueous Stress Corrosion in Titanium Allloys
22. Stress-corrosion Cracking in High Strength Steels and in Titanium and Aluminum Alloys
23. Ordering, stacking faults and stress corrosion cracking in austenitic alloys10.5006/0010-9312-20.1.15t ↗
24. Aqueous stress corrosion in titanium alloys10.1179/000705975798320783 ↗
25. Stress-corrosion cracking of titanium alloys
26. The relationship between crystallographic texture and salt water cracking susceptibility in Ti-6Al-4V10.1016/0921-5093(95)09820-8 ↗
27. Local texture and fatigue crack initiation in a Ti-6Al-4V titanium alloy10.1046/j.1460-2695.2002.00480.x ↗
28. The role of microtexture on the faceted fracture morphology in Ti-6Al-4V subjected to high-cycle fatigue10.1016/j.actamat.2010.03.036 ↗
29. A simple model to account for the role of microtexture on fatigue and dwell fatigue lifetimes of titanium alloys10.1016/j.scriptamat.2013.10.024 ↗
30. Texture heterogeneities in αp/αs titanium forging analysed by EBSD-relation to fatigue crack propagation10.1111/j.1365-2818.2009.03141.x ↗
31. Effect of microtexture on fatigue cracking in Ti–6Al–4V10.1016/j.actamat.2007.06.034 ↗
32. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
33. Dwell and normal cyclic fatigue behaviours of Ti60 alloy10.1016/j.jmst.2013.10.010 ↗
34. Development of microstructure and texture heterogeneities during static annealing of Ti–6.5Al–3.5Mo–1.5Zr–0.3Si alloy preformed by hot working10.1016/S1005-0302(12)60167-4 ↗
35. Macroscopic and microscopic aspects of the deformation and fracture mechanisms of ultrafine-grained aluminum processed by hot pressing10.1016/j.actamat.2005.09.012 ↗
36. Densification behaviour of titanium alloy powder under hot isostatic pressing10.1179/003258901666158 ↗
37. Powder metallurgy of titanium alloys10.1179/095066090790323984 ↗
38. The technologies of titanium powder metallurgy10.1007/s11837-004-0252-x ↗
39. Stress corrosion cracking of titanium alloys10.2514/3.4497 ↗
40. ASTM International · 2000
41. On the physics of moisture-induced cracking in metal-glass (copper-silica) interfaces10.1063/1.2775998 ↗
42. ASTM International · 2011
43. Observations of facet formation in near-α titanium and comments on the role of hydrogen10.1007/s11661-010-0507-9 ↗
44. Deformation behavior of HCP Ti-Al alloy single crystals10.1007/s11661-002-0153-y ↗
45. The influence of oxygen concentration on the internal stress and dislocation arrangements in α titanium10.1007/BF02652870 ↗
46. Cyclic deformation behaviour of an α/β titanium alloy – I. Micromechanisms of plasticity under various loading paths10.1016/S1359-6454(96)00406-5 ↗
47. Near threshold fatigue crack growth behavior of a titanium alloy: Ti-6Al-4V10.1016/0956-7151(91)90319-V ↗
48. Texture heterogeneities induced by subtransus processing of near α titanium alloys10.1016/j.actamat.2008.04.065 ↗
49. An analysis of frequency and amplitude effects on corrosion fatigue crack propagation in Ti-8Al-1Mo-1V10.1007/BF02662746 ↗
50. Hydrogen embrittlement and stress corrosion cracking in Ti-Al binary alloys10.5006/0010-9312-29.6.241 ↗
51. Hydrogen embrittlement of α titanium: in situ TEM studies10.1016/0001-6160(88)90032-6 ↗
52. The stress-corrosion cracking susceptibility of near-α titanium alloy IMI 834 in presence of hot salt10.1016/j.corsci.2014.01.013 ↗
53. Mechanistic and fractographic aspects of stress-corrosion cracking (SCC)
54. Hydrogen embrittlement (HE) phenomena and mechanisms
55. Stress corrosion cracking
56. Hydrogen embrittlement understood10.1007/s11663-015-0325-y ↗
57. Hydrogen-induced modification in the deformation and fracture of a precipitation-hardened Fe–Ni based austenitic alloy10.1016/j.jmst.2014.03.017 ↗
58. Microelectrode monitoring the crevice corrosion of titanium10.5006/1.3585272 ↗