journal article·2016-06

Corrosion mechanism of hydrogenated nitrile butadiene rubber O-ring under simulated wellbore conditions

Dezhi Zeng, Qiyao He, Tan Li, Junying Hu, Taihe Shi, Zhi Zhang, Zhiming Yu, Ruijia Liu

Corrosion Science· Volume 107
Publisher page

Abstract

Abstract Corrosion testing of hydrogenated nitrile butadiene rubber (HNBR) O-ring was conducted at 140 °C, 35 MPa containing 0.5 MPa CO 2 for 168 h in simulated wellbore conditions using self-designed compression simulator and autoclave. The mechanical properties, EDS and fracture morphology analyses were performed. The corrosion under the compression state was more serious than that under the free state. Moreover, liquid corrosion was more serious under the free state. The decrease of mechanical properties can be attributed to the penetration of corrosive media and chemical actions, which changed the structure of rubber chains, weakened the reinforcement role of carbon black (CB).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Drilling and Well Engineering · Corrosion Behavior and Inhibition · Asphalt Pavement Performance Evaluation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. RP90 · 2016
2. Failure behavior of rubber O-ring under cyclic exposure to high-pressure hydrogen gas10.1016/j.engfailanal.2013.01.034 ↗
3. NORSOK-M710, Qualification of non-metallic sealing materials and manufacturers, (2001).
4. Effect of carbon black loading on the swelling and compression set behavior of SBR and NBR rubber compounds10.1016/j.matdes.2008.07.043 ↗
5. Factors influencing hardness and compression set measurements on O-rings10.1080/03602559.2013.779710 ↗
6. Effect of fillers on natural rubber/high styrene rubber blends with nano silica: morphology and wear10.1016/j.matdes.2009.08.014 ↗
7. Mechanical and tribological properties of natural rubber reinforced with carbon blacks and Al2O3 nanoparticles10.1016/j.matdes.2013.01.033 ↗
8. Validation of improved methods for predicting long-term elastomeric seal lifetimes from compression stress–relaxation and oxygen consumption techniques10.1016/S0141-3910(03)00159-9 ↗
9. Prediting the lifetime of fluorosilicone o-rings10.1016/j.polymdegradstab.2009.10.005 ↗
10. Predicting and confirming the lifetime of o-rings10.1016/j.polymdegradstab.2004.07.019 ↗
11. Accelerated aging and lifetime prediction: review of non-Arrhenius behaviour due to two competing processes10.1016/j.polymdegradstab.2005.05.004 ↗
12. Influence of carbon black on crack damage and hydrogen permeation properties of filled EPDM rubbers exposed to high-pressure hydrogen gas10.1002/app.34344 ↗
13. Influence of fillers on hydrogen penetration properties and blister fracture of rubber composites for O-ring exposed to high-pressure hydrogen gas10.1016/j.ijhydene.2008.11.105 ↗
14. Yamabe · 2009
15. Application of acoustic emission method to detection of internal fracture of sealing rubber material by high-pressure hydrogen decompression10.1016/j.polymertesting.2010.11.002 ↗
16. NACE TM 0187, Evaluating elastomeric materials in sour gas environments, 2003
17. Accelerated thermal ageing studies on nitrile rubber O-rings10.1016/S0142-9418(02)00171-X ↗
18. Internal crack symmetry phenomena during gas-induced rupture of elastomers10.5254/1.3538617 ↗
19. High-pressure gas testing of elastomer seals and a practical approach to designing for explosive decompression service10.1016/S1350-4789(04)00231-4 ↗
20. Thermal ageing studies on room-temperature vulcanised polysiloxane rubbers10.1016/S0141-3910(01)00118-5 ↗
21. Storage life of silicone rubber sealing ring used in solid rocket motor10.1016/j.cja.2014.10.013 ↗
22. Fracture of elastomers by gas decompression10.5254/1.3538735 ↗
23. Verification properties of O-rings made from viton extreme with advanced polymer architecture used in pipeline valves containing very sour gas10.3923/jas.2010.2693.2696 ↗
24. I.S.O. 3601/1, Fluid power systems − O-rings − Part 1: Inside diameters, cross-sections tolerances and designation codes, (2013).
25. G.B./T. 5720, Test methods for rubber O-rings, (2008).
26. D1414 · 2008
27. Evaluation of percutaneous penetration of natural rubber latex proteins10.1093/toxsci/56.2.262 ↗
28. Investigation of the swelling response and quantitative prediction for hydrogenated nitrile rubber10.1016/j.polymertesting.2013.12.013 ↗
29. Yang · 1997
30. Enhancement of the chemical resistance of nitrile rubber by direct fluorination10.1002/app.12212 ↗
31. Acidic hydrolysis of polyacrylonitrile: effect of neighboring groups10.1021/ma010213o ↗
32. Investigation of corrosion behavior of aluminum flakes coated by polymeric nanolayer: effect of polymer type10.1016/j.corsci.2014.06.045 ↗
33. Degradation of hydrogenated nitrile-butadiene rubber in aqueous solutions of H2S or HCl10.1007/s40242-013-2401-7 ↗
34. Determination of dynamic mechanical properties of carbon black filled rubbers at wide frequency range using Havriliak–Negami model10.1016/j.euromechsol.2015.06.002 ↗