journal article·2017-10

Anisotropic pitting of single-phase β-Zr alloy and isotropic pitting of α + β double-phase Zr alloy

Chaoqun Xia, Zhihao Feng, Shuguang Liu, Xing Zhang, Bing Zhang, Bo Pan, Xinyu Zhang, Mingzhen Ma, Riping Liu

Corrosion Science· Volume 127
Publisher page

Abstract

Abstract Pitting corrosion behaviour of Zr-40Ti-5Al–4 V alloys with different phase composition was investigated. Pitting of the single-phase β-Zr alloy is crystallographic and the corrosion pits exhibit different orientation, which is mainly attributed to the favored dissolution kinetics of the {001} plane in body-centered cubic β grains. In contrast, isotropic and circular shaped pitting, due to the evenly distributed α and β phases, was observed in Zr alloy containing α + β double-phase. In addition, weight loss and electrochemical experiments reveal that the double-phase alloy is more sensitive to pitting than the single-phase alloy.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Schemel · 1997
2. Effect of isothermal annealing on the corrosion behavior of Zr-xNb alloys10.1016/j.jnucmat.2004.01.015 ↗
3. The influence of alloying elements on the corrosion of Zr alloys10.1016/j.corsci.2015.12.022 ↗
4. Microstructure and mechanical properties of as-cast Zr–Nb alloys10.1016/j.actbio.2011.07.005 ↗
5. Effects of Al content on structure and mechanical properties of hot-rolled ZrTiAlV alloys10.1016/j.matdes.2013.05.065 ↗
6. Cox · 2011 · 893
7. Pitting corrosion of bulk glass-forming zirconium-based alloys10.1016/j.jallcom.2004.01.043 ↗
8. Relationship between amorphous structure and corrosion behaviour in a Zr-Ni metallic glass10.1016/j.corsci.2012.02.017 ↗
9. The corrosion behaviour of Zr-based bulk metallic glasses in 0.5 M NaCl solution10.1016/j.corsci.2011.05.014 ↗
10. Electrochemical behavior of multicomponent amorphous and nanocrystalline Zr-based alloys in different environments10.1016/j.corsci.2005.09.001 ↗
11. The effect of oxidation on the corrosion resistance and mechanical properties of a Zr-based metallic glass10.1016/j.corsci.2011.06.032 ↗
12. Corrosion behavior of Ti-6Al-4 V with different thermomechanical treatments and microstructures
13. An image analysis study of pit formation on Ti-6Al-4V10.1016/S0921-5093(02)00218-6 ↗
14. Effect of the accumulated annealing parameter on the corrosion characteristics of a Zr-0. 5Nb-1. 0Sn-0. 5Fe-0. 25Cr alloy10.1016/S0022-3115(99)00288-3 ↗
15. Preparation of the ZrTiAlV alloy with ultra-high strength and good ductility10.1016/j.msea.2012.01.022 ↗
16. Pitting corrosion on zirconium—a review10.5006/1.3579296 ↗
17. Passivity breakdown, pit initiation and propagation of pits in metallic materials—review10.1016/j.corsci.2014.10.006 ↗
18. Pitting corrosion of Al and Al-Cu single crystals10.1149/1.2086291 ↗
19. Pitting corrosion of zirconium and hafnium10.1016/0013-4686(88)80016-1 ↗
20. The effect of crystallographic orientation on the active corrosion of pure magnesium10.1016/j.scriptamat.2007.10.027 ↗
21. The Chemical Physics of Solid Surfaces and Heterogeneous Catalysis
22. Corrosion and passivation of annealed Ti-20Zr-6.5Al-4 V alloy10.1016/j.corsci.2015.08.038 ↗
23. Nucleation of corrosion pits in Ringer's solution containing bovine serum10.1016/j.corsci.2007.05.018 ↗
24. The effect of temperature on the nucleation of corrosion pits on titanium in Ringer's physiological solution10.1016/j.biomaterials.2004.02.023 ↗
25. Depassivation current transients measured between identical twin microelectrodes in open circuit10.1016/j.corsci.2006.06.036 ↗