journal article·2020-04

Liquid metal embrittlement of an Fe10Cr4Al ferritic alloy exposed to oxygen-depleted and -saturated lead-bismuth eutectic at 350°C

Xing Gong, Jiajun Chen, Feiyu Hu, Congying Xiang, Zhiyang Yu, Jun Xiao, Hui Wang, Haoran Gong, Hao Wang, Chaohong Liu, Yangbin Deng, Bo Pang, Xi Huang, Yongchun Li, Yuan Yin

Corrosion Science· Volume 165
Publisher page

Abstract

Abstract Liquid metal embrittlement (LME) of an Fe10Cr4Al (wt%) ferritic alloy was tested in lead-bismuth eutectic (LBE) at 350 °C using slow strain rate tensile tests. The results show that this alloy is highly susceptible to LME. The strong LME effect is manifested by a substantial reduction in ductility and completely cleaved fracture surfaces. Transgranular cleavage and intergranular cracking are the major fracture modes. The LME susceptibility is slightly weaker in oxygen-saturated LBE than oxygen-depleted LBE due to the presence of a double-layer scale consisting of magnetite and Al-rich spinel. The oxide scale is fragmented, indicative of a brittle nature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. OECD/NEA · 2015
2. Opportunities for the LWR ATF materials development program to contribute to the LBE-cooled ADS materials qualification program10.1016/j.jnucmat.2016.10.012 ↗
3. Oxide scale formation on 316L and FeCrAl steels exposed to oxygen controlled static LBE at temperatures up to 800 °C10.1016/j.solmat.2015.09.007 ↗
4. Oxidative passivation of Fe–Cr–Al steels in lead-bismuth eutectic under oxygen-controlled static conditions at 700 and 800 °C10.1016/j.jnucmat.2019.06.004 ↗
5. Liquid Pb-Bi embrittlement effects on the T91 steel after different heat treatments10.1016/j.jnucmat.2008.02.050 ↗
6. Slow strain rate tensile tests on T91 in static lead-bismuth eutectic10.1016/j.jnucmat.2006.05.039 ↗
7. Influence of LBE long term exposure and simultaneous fast neutron irradiation on the mechanical properties of T91 and 316L10.1016/j.jnucmat.2016.02.008 ↗
8. Low cycle fatigue behavior of a modified 9Cr-1Mo ferritic-martensitic steel in lead-bismuth eutectic at 350°C - Effects of oxygen concentration in the liquid metal and strain rate10.1016/j.corsci.2015.02.022 ↗
9. Low cycle fatigue behaviour of T91 martensitic steel at 300°C in air and in liquid lead bismuth eutectic10.1016/j.ijfatigue.2005.11.003 ↗
10. Characteristics and liquid metal embrittlement of the steel T91 in contact with lead–Bismuth eutectic10.1016/j.jnucmat.2015.08.048 ↗
11. Creep-to-rupture tests of T91 steel in flowing Pb-Bi eutectic melt at 550 °C10.1016/j.jnucmat.2009.08.013 ↗
12. The role of oxide films in preventing liquid metal embrittlement of T91 steel exposed to liquid lead-bismuth eutectic10.1016/j.jnucmat.2018.07.018 ↗
13. Temperature dependence of liquid metal embrittlement susceptibility of a modified 9Cr-1Mo steel under low cycle fatigue in lead-bismuth eutectic at 160 to 450°C10.1016/j.jnucmat.2015.06.021 ↗
14. Influence of liquid lead and lead-bismuth eutectic on tensile, fatigue and creep properties of ferritic/martensitic and austenitic steels for transmutation systems10.1016/j.jnucmat.2011.04.047 ↗
15. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500°C10.1016/j.jnucmat.2017.04.004 ↗
16. Transmission electron microscopy study of complex oxide scales on DIN 1.4970 steel exposed to liquid Pb-Bi eutectic10.1016/j.corsci.2018.10.018 ↗
17. Multiscale investigation of crack path and microstructural changes during liquid metal embrittlement of 304L austenitic steel in liquid sodium10.1016/j.corsci.2017.08.009 ↗
18. Review of the studies on fundamental issues in LBE corrosion10.1016/j.jnucmat.2007.06.019 ↗
19. Corrosion behavior of austenitic steels 1.4970, 316L and 1.4571 in flowing LBE at 450 and 550°C with 10−7 mass% dissolved oxygen10.1016/j.jnucmat.2014.08.024 ↗
20. Long-term corrosion of austenitic steels in flowing LBE at 400°C and 10−7 mass% dissolved oxygen in comparison with 450 and 550°C10.1016/j.jnucmat.2015.09.027 ↗
21. Corrosion scales on various steels after exposure to liquid lead–bismuth eutectic10.1016/j.jnucmat.2013.09.034 ↗
22. Oxide scales formed on Fe–Cr–Al-based model alloys exposed to oxygen containing molten lead10.1016/j.jnucmat.2013.02.044 ↗
23. Influence of composition and microstructure on the corrosion behavior of different Fe-Cr-Al alloys in molten LBE10.1016/j.jnucmat.2011.11.049 ↗
24. Corrosion resistance of Si- and Al-rich steels in flowing lead-bismuth10.1016/j.jnucmat.2006.05.019 ↗
25. Design of alumina forming FeCrAl steels for lead or lead–bismuth cooled fast reactors10.1016/j.jnucmat.2012.04.006 ↗
26. Corrosion and radiation resistant nanoceramic coatings for lead fast reactors10.1016/j.corsci.2017.05.011 ↗
27. Weisenburger · 2017
28. T91 cladding tubes with and without modified FeCrAlY coatings exposed in LBE at different flow, stress and temperature conditions10.1016/j.jnucmat.2008.02.026 ↗
29. 400 °C aging embrittlement of FeCrAl alloys: microstructure and fracture behavior10.1016/j.msea.2018.11.084 ↗
30. Oxidation studies of Fe10CrAl-RE alloys exposed to Pb at 550°C for 10000h10.1016/j.jnucmat.2013.07.023 ↗
31. Microstructural stability of Fe–Cr–Al alloys at 450–550 °C10.1016/j.jnucmat.2014.11.101 ↗
32. Liquid metal embrittlement susceptibility of a high-entropy alloy exposed to oxygen-depleted liquid lead-bismuth eutectic at 250 and 350°C10.1016/j.jnucmat.2019.151859 ↗
33. Schroer · 2007
34. Accuracy of potentiometric oxygen sensors with Bi/Bi2O3 reference electrode for use in liquid LBE10.1016/j.jnucmat.2012.06.011 ↗
35. Experimental analysis of the dynamic strain ageing for a modified T91 martensitic steel10.1016/j.msea.2011.12.031 ↗
36. Mechanism of dynamic strain aging and characterization of its effect on the low-cycle fatigue behavior in type 316L stainless steel10.1016/j.jnucmat.2004.12.012 ↗
37. Behaviour of pre-stressed T91 and ODS steels exposed to liquid lead-bismuth eutectic10.1016/j.corsci.2017.12.005 ↗
38. Segregation-induced ordered superstructures at general grain boundaries in a nickel-bismuth alloy10.1126/science.aam8256 ↗
39. Tensile fracture behavior of notched 9Cr-1Mo ferritic-martensitic steel specimens in contact with liquid lead-bismuth eutectic at 350°C10.1016/j.msea.2017.03.067 ↗
40. Mechanical properties of the steel T91 in contact with lead10.1016/j.nucengdes.2014.10.004 ↗
41. Behaviour of the steel T91 under uniaxial and multiaxial slow loading in contact with liquid lead10.1016/j.jnucmat.2015.05.041 ↗
42. Mechanisms and kinetics of environmentally assisted cracking: current status, issues, and suggestions for further work10.1007/s11661-012-1359-2 ↗
43. Multiscale investigation of quasi-brittle fracture characteristics in a 9Cr-1Mo ferritic-martensitic steel embrittled by liquid lead-bismuth under low cycle fatigue10.1016/j.corsci.2015.10.003 ↗
44. The kinetics of gallium penetration into aluminum grain boundaries—in situ TEM observations and atomistic models10.1016/S1359-6454(99)00463-2 ↗
45. Crack propagation in a liquid metal environment10.1016/0001-6160(63)90180-9 ↗
46. Concerning liquid metal embrittlement, particularly of zinc monocrystals by mercury10.1080/14786436308213836 ↗