Effect of SiO2 barrier scale prepared by pre-oxidation on hot corrosion behavior of MoSi2-based coating on Nb alloy
Source abstract
Abstract
Abstract Using pre-oxidation at 1500 °C for 10 h, a continuous SiO2 barrier scale was fabricated on MoSi2-based/NbSi2 coating of Nb alloy expected to resist hot corrosion with Na2SO4 at 1000 °C. No obvious corrosion occurred for 2 h, while the corroded products including Na2Si2O5, Na2MoO4 and SiO2 deposits were generated respectively for 4 h and 8 h. The degradation of SiO2 scale triggered an evident increase in surface roughness. Due to a slow reaction rate, SiO2 scale can serve as a barrier isolating from Na2SO4 salt to alleviate the degradation of MoSi2-based coating effectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. The oxidation resistance of Nb-Si-based alloys at intermediate and high temperatures10.3390/ma13051229 ↗
2. A review of very-high-temperature Nb-silicide-based composites10.1007/s11661-003-0269-8 ↗
3. Oxidation behavior of the B-modified silicide coating on Nb-Si based alloy at intermediate temperatures10.1016/j.corsci.2017.12.016 ↗
4. Ultrahigh-temperature Nb-silicide-based composites10.1557/mrs2003.192 ↗
5. Isothermal oxidation mechanism of a newly developed Nb-Ti-V-Cr-Al-W-Mo-Hf alloy at 800-1200 °C10.1016/j.ijrmhm.2015.08.012 ↗
6. Reaction synthesis of spark plasma sintered MoSi2-B4C coatings for oxidation protection of Nb alloy10.1016/j.ceramint.2018.11.103 ↗
7. Oxidation behaviour of a Ge-modified silicide coating on an Nb-Si based alloy in the moderate temperature range10.1016/j.corsci.2019.108249 ↗
8. Isothermal oxidation and interdiffusion behavior of MoSi2/WSi2 compound coating on Nb-Ti-Si based alloy10.1016/j.apsusc.2019.144477 ↗
9. Hot corrosion mechanism in multi-Layer suspension plasma sprayed Gd2Zr2O7/YSZ thermal barrier coatings in the presence of V2O5 + Na2SO410.1007/s11666-016-0486-5 ↗
10. Hot corrosion behaviour of Nbss/Nb5Si3 in situ composites in the mixture of Na2SO4 and NaCl melts10.1016/j.corsci.2013.04.057 ↗
11. Hot corrosion behavior of silicide coating on an Nb-Ti-Si based ultrahigh temperature alloy10.1016/j.corsci.2014.10.053 ↗
12. Hot corrosion phenomena of Nb-Ti-Si based alloy and its silicide coating induced by different corrosive environments at 900 °C10.1016/j.ceramint.2018.01.238 ↗
13. Degradation of the plasma sprayed GdMgAl11O19 thermal barrier coating resistant to calcium-magnesium-aluminum-silicate attack at 1350 °C10.1016/j.corsci.2020.108593 ↗
14. A MoSi2-based composite coating by supersonic atmospheric plasma spraying to protect Nb alloy against oxidation at 1500 °C10.1016/j.surfcoat.2018.07.091 ↗
15. A long-term ultrahigh temperature application of layered silicide coated Nb alloy in air10.1016/j.apsusc.2018.01.114 ↗
16. Effect of mullite on the microstructure and oxidation behavior of thermal-sprayed MoSi2 coating at 1500 °C
17. Comparison investigation of hot corrosion exposed to Na2SO4 salt and oxidation of MoSi2-based coating on Nb alloy at 1000 °C10.1016/j.surfcoat.2020.125388 ↗
18. The solubility of SiO2 in fused Na2SO4 at 900 °C10.1149/1.2108692 ↗
19. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
20. Hot corrosion of silica10.1111/j.1151-2916.1990.tb05147.x ↗
21. Hot-corrosion behaviour of silica and silica-formers: external versus internal control10.1016/S0955-2219(98)00243-X ↗
22. Hot corrosion of Mo-Si-B coatings10.1007/s11085-017-9773-x ↗
23. Hot corrosion behavior of NbSi2/SiO2-Nb2O5 multilayer coating on Nb alloy10.1016/j.jallcom.2018.07.059 ↗
24. High-temperature oxidation of MoSi210.1007/s10853-009-4012-8 ↗
25. Effect of mullite on the microstructure and oxidation behavior of thermal-sprayed MoSi2 coating at 1500 °C10.1016/j.ceramint.2019.12.273 ↗
26. Silicide coating fabricated by HAPC/SAPS combination to protect Niobium alloy from oxidation10.1021/acsami.6b04599 ↗
27. Molten-salt corrosion of silicon-nitride: II, sodium sulfate10.1111/j.1151-2916.1988.tb05829.x ↗
28. Kinetics and mechanism of hot corrosion of γ-Y2Si2O7 in thin-film Na2SO4 molten salt10.1111/j.1551-2916.2008.02439.x ↗
29. Sodium sulfate: deposition and dissolution of silica10.1007/BF00665488 ↗
30. Corrosion of Si-based non-oxide ceramics by molten Na2SO410.4028/www.scientific.net/KEM.132-136.1588 ↗