journal article·2021-01

Segregating the homogeneous passive film and understanding the passivation mechanism of Ti-based metallic glasses

Jia-Lun Gu, Si-Yuan Lu, Yang Shao, Ke-Fu Yao

Corrosion Science· Volume 178
Publisher page

Abstract

Abstract Resolving structural and componential characteristics of passive film is a long-standing challenge in corrosion science since it’s difficult to separate extremely thin passive films. In this work, the passive films are successfully separated from Ti-Zr-Be-Al/Ni/Fe glassy substrates as large-area thin membranes by the designed “Ribbon-Penetration” method. The homogeneous and continuous passive films are identified as a single-layer amorphous structure, whose primary components are TiO2, ZrO2 and BeO. Alloying Ni or Fe element could induce the enrichment of TiO2 in the passive films and improve the structural compactness, resulting in the superior corrosion resistance in 3.5 wt.% NaCl solution.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Multi-element-resolved electrochemical corrosion analysis. Part I. Dissolution behavior and passivity of amorphous Fe50Cr15Mo14C15B610.1016/j.corsci.2014.08.002 ↗
2. Corrosion behavior of glassy Ni55Co5Nb20Ti10Zr10 alloy in 1 N HCl solution studied by potentiostatic polarization and XPS10.1016/j.corsci.2005.02.013 ↗
3. Effects of Cr addition on thermal stability, soft magnetic properties and corrosion resistance of FeSiB amorphous alloys10.1016/j.corsci.2018.04.006 ↗
4. The novel Ti-based metallic glass with excellent glass forming ability and an elastic constant dependent glass forming criterion10.1016/j.mtla.2019.100433 ↗
5. An abnormal correlation between electron work function and corrosion resistance in Ti-Zr-Be-(Ni/Fe) metallic glasses10.1016/j.corsci.2019.108392 ↗
6. The corrosion behaviour of Zr-based bulk metallic glasses in 0.5 M NaCl solution10.1016/j.corsci.2011.05.014 ↗
7. Effects of Cu addition on the glass forming ability and corrosion resistance of Ti-Zr-Be-Ni alloys10.1016/j.jallcom.2017.07.165 ↗
8. Electrochemical corrosion resistance of the amorphous and crystalline Pd-based alloys in simulated seawater
9. Bulk glassy Fe-Cr-Mo-C-B alloys with high corrosion resistance10.1016/S0010-938X(02)00002-1 ↗
10. Effect of thermally induced relaxation on passivity and corrosion of an amorphous Al–Co–Ce alloy10.1016/j.corsci.2012.03.012 ↗
11. Metastable pitting corrosion of stainless-steel and the transition to stability
12. Nucleation of corrosion pits on stainless-steel10.1080/09500839208229274 ↗
13. W.R. Whitney award lecture: in pursuit of new corrosion-resistant alloys10.5006/1.3277653 ↗
14. Novel corrosion behaviours of the annealing and cryogenic thermal cycling treated Ti-based metallic glasses10.1016/j.intermet.2019.04.010 ↗
15. Effect of surface finishing of a Zr-based bulk metallic glass on its corrosion behaviour10.1016/j.corsci.2010.01.027 ↗
16. Element-resolved corrosion analysis of stainless-type glass-forming steels10.1126/science.1230081 ↗
17. Relationship between amorphous structure and corrosion behaviour in a Zr–Ni metallic glass10.1016/j.corsci.2012.02.017 ↗
18. Influence of yttrium on surface chemistry and stability of passive film in Al-based binary metallic glasses10.1016/j.apsusc.2018.06.306 ↗
19. Phase diagram of the system: Al2O3-ZrO210.1016/S0272-8842(00)00023-7 ↗
20. Corrosion pits in thin films of stainless steel10.1149/1.1391569 ↗
21. Direct observation of thinmembrane passive filmover the growing pit on sputtered nanocrystalline austenitic stainless steel film10.1016/j.elecom.2015.01.013 ↗
22. An investigation on the continuous and uniform thin membrane passive film formed on sputtered nanocrystalline stainless steel10.1016/j.corsci.2015.11.031 ↗
23. A highly processable metallic glass: Zr41.2Ti13.8Cu12.5Ni10.0Be22.510.1063/1.110520 ↗
24. Comparing the pitting corrosion behavior of prominent Zr-based bulk metallic glasses10.1557/jmr.2014.371 ↗
25. Dependence of the pitting potential of al-alloys on solubility of alloying element oxides10.1016/0010-938X(93)90282-L ↗
26. The generation of surface roughness during slurry erosion-corrosion and its effect on the pitting potential10.1016/S0010-938X(96)00066-2 ↗
27. Centimeter-sized Ti-rich bulk metallic glasses with superior specific strength and corrosion resistance10.1016/j.jnoncrysol.2018.10.034 ↗
28. Metal dusting corrosion of austenitic alloys at low and high pressure with the effects of Cr, Al, Nb and Cu10.1016/j.corsci.2017.04.015 ↗
29. A corrosion-resistance superhydrophobic TiO2 film10.1016/j.apsusc.2012.04.061 ↗
30. Constant-phase-element behavior caused by coupled resistivity and permittivity distributions in films10.1149/2.039112jes ↗
31. Electrochemical behaviour of high nitrogen stainless steel in acidic solutions10.1016/j.corsci.2009.02.026 ↗
32. Effect of annealing below the crystallization temperature on the corrosion behavior of Al-Ni-Y metallic glasses10.1016/j.corsci.2014.03.015 ↗
33. Determination of effective capacitance and film thickness from constant-phase-element parameters10.1016/j.electacta.2009.10.065 ↗
34. Impedance characterization of anodic barrier Al oxide film beneath porous oxide layer10.1149/1.2208737 ↗
35. Niobium addition enhancing the corrosion resistance of nanocrystalline Ti5Si3 coating in H2SO4 solution10.1016/j.actamat.2013.10.040 ↗
36. The analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
37. Pit growth studies in stainless steel foils. I. Introduction and pit growth kinetics10.1016/S0010-938X(01)00133-0 ↗
38. Growth of single corrosion pit in sputtered nanocrystalline stainless steel film10.1016/j.corsci.2016.05.007 ↗
39. Impedance spectroscopy as a technique for studying the spontaneous passivation of metals in electrolytes10.1016/0013-4686(95)00464-5 ↗
40. Atomistic free-volume zones and inelastic deformation of metallic glasses10.1038/nmat2802 ↗
41. Tuning order in disorder10.1038/nmat4300 ↗
42. Corrosion behavior of bulk (Zr58Nb3Cu16Ni13Al10)(100-x)Yx (x=0, 0.5, 2.5 at. %) metallic glasses in sulfuric acid10.1016/j.corsci.2019.01.016 ↗
43. Atlas of electrochemical equilibria in aqueous solutions
44. Role of late transition metals on pitting resistance of Zr-Ti-(Cu, Ni, Co)-Al bulk metallic glasses in 0.6 M NaCl aqueous solution10.1016/j.jmst.2017.04.010 ↗
45. Stabilization treatment of cultural heritage artefacts: in situ monitoring of marine iron objects dechlorinated in alkali solution10.1016/j.corsci.2017.12.028 ↗
46. The point-defect model for the passive state10.1149/1.2069096 ↗
47. The history of the point defect model for the passive state: a brief review of film growth aspects10.1016/j.electacta.2010.11.005 ↗
48. Selective dissolution sensitive to minor alloying in CuZr-based metallic glasses10.1016/j.corsci.2013.07.021 ↗
49. Phase stability in high entropy alloys: formation of solid-solution phase or amorphous phase10.1016/S1002-0071(12)60080-X ↗
50. Gale · 2004