Effect of temperature gradient on the ablation and flexural behavior of C/C-ZrC composites
Source abstract
Abstract
Abstract A new ablation condition was designed to investigate the effect of temperature gradient on the ablation and flexural behavior of the C/C-ZrC composites. The sample not only suffers the gradient temperature ablation ranging from 1000 to 2000 ℃ but withstands flexural load caused by the high-speed airflow scouring. The volume ablation rate of the C/C-ZrC was 0.06 mm3/s, which was only 6.81 % of the rate of the C/C. The volume change caused by ZrC→ZrO2 together with the ZrO2 crystalline transformation was beneficial for releasing internal stress, thereby contributing to the higher flexural strength retention of the C/C-ZrC composites.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. UHTC composites for hypersnoic applications
2. High temperature creep of 20 vol%. SiC-HfB2 UHTCs up to 2000 ℃ and the effect of La2O3 addition10.1016/j.jeurceramsoc.2017.08.028 ↗
3. Materials characterization and mechanical properties of Cf-UHTC powder composites10.1016/j.jeurceramsoc.2018.12.043 ↗
4. Influence of preparation temperature on the oxidation resistance and mechanical properties of C/SiC coated C/C composites10.1016/j.corsci.2014.05.009 ↗
5. Oxidation and mechanical properties of SiC/SiC-MoSi2-ZrB2 coating for Carbon/Carbon composites10.1016/j.jmst.2013.09.006 ↗
6. Effect of PyC interface phase on the cyclic ablation resistance and flexural properties of two-dimensional Cf/HfC composites10.1016/j.jeurceramsoc.2020.08.049 ↗
7. New thermal protection system using high-temperature carbon fibre-reinforced plastic sandwich panel10.1016/j.actaastro.2019.02.004 ↗
8. The future of carbon-carbon composites10.1016/0008-6223(87)90116-3 ↗
9. A novel Hf-Si-O wire drawing phenomenon after ablation of SiCnws/HfC-SiC coating on C/C composites10.1016/j.jmat.2020.03.001 ↗
10. Mechanical, thermal, and oxidation properties of refractory hafnium and zirconium compounds10.1016/S0955-2219(99)00129-6 ↗
11. Effect of HfC-SiC transition layer on the ablation resistance of SiC/HfC-SiC/HfC multi-layer coating for C/C composites10.1016/j.vacuum.2019.108886 ↗
12. Effects of h-BN particles on the structure, oxidation behaviour, and kinetics of C/C composites10.1016/j.corsci.2020.109059 ↗
13. Oxidation behaviour and related microstructural changes of two β0-phase containing TiAl alloys between 600 ℃ and 900 ℃10.1016/j.corsci.2020.109085 ↗
14. An oxidation and ablation protective WSi2-HfB2-SiC coating for SiC coated C/C composites at 1973 K and above10.1016/j.corsci.2020.108964 ↗
15. Difference evaluation on ablation behaviors of ZrC-based and ZrB2 based UHTCs coatings
16. Long-term oxidation behaviors of C/SiC composites with a SiC/UHTC/SiC three-layer coating in a wide temperature range10.1016/j.corsci.2018.10.017 ↗
17. Materials characterization and mechanical properties of Cf-UHTC powder composites10.1016/j.jeurceramsoc.2018.12.043 ↗
18. UHTCs: ultra-high temperature ceramic materials for extreme environment applications
19. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
20. Processing and properties of ultra-high temperature ceramics for space applications10.1016/j.msea.2007.08.054 ↗
21. Effects of precursor feeding rate on the microstructure and ablation resistance of gradient C/C ZrC SiC composites prepared by chemical liquid-vapor deposition10.1016/j.vacuum.2019.03.030 ↗
22. Mechanical properties and ablation behavior of C/C-ZrC and C/C-ZrC-SiC composites prepared by precursor infiltration and pyrolysis combined with chemical vapor infiltration - ScienceDirect10.1016/j.ceramint.2018.09.131 ↗
23. Reactive infiltration processing (RIP) of ultra high temperature ceramics (UHTC) into porous C/C composite tubes10.1016/j.jeurceramsoc.2010.10.013 ↗
24. Microstructural characterization on ZrC doped carbon/carbon composites10.1016/j.ceramint.2011.08.002 ↗
25. Microstructure and ablation properties of zirconium carbide doped carbon/carbon composites10.1016/j.carbon.2009.09.035 ↗
26. Effect of the Al2O3 additive on the high temperature ablation behavior of the ZrC–ZrO2 coating for SiC-coated carbon/carbon composites10.1016/j.ceramint.2019.08.014 ↗
27. ZrC ablation protective coating for carbon/carbon composites10.1016/j.carbon.2009.07.047 ↗
28. Influence of CLVD thermal gradient on the deposition behavior, microstructure and properties of C/C-ZrC composites10.1016/j.ceramint.2018.05.232 ↗
29. Preparation of co-deposited C/C-ZrC composites by CLVD process and its properties10.1016/j.jallcom.2015.12.178 ↗
30. Mechanical, oxidation and ablation properties of C/(C-SiC)CVI-(ZrC-SiC)PIP composites10.1016/j.corsci.2019.108200 ↗
31. Effect of ZrC particle size on the ablation resistance of C/C-ZrC-SiC composites10.1016/j.matdes.2017.05.019 ↗
32. Ablation behavior of C/C-ZrC and C/SiC-ZrC composites fabricated by a joint process of slurry impregnation and chemical vapor infiltration10.1016/j.ceramint.2017.12.062 ↗
33. Ultra-high-temperature ablation behavior of SiC–ZrC–TiC modified carbon/carbon composites fabricated via reactive melt infiltration10.1016/j.jeurceramsoc.2019.10.027 ↗
34. Enhanced anti-ablation performance of carbon/carbon composites modified with ZrC-SiC10.1016/j.vacuum.2018.07.025 ↗
35. Effects of preform pore structure on infiltration kinetics and microstructure evolution of RMI-derived Cf /ZrC-ZrB2 -SiC composite10.1016/j.jeurceramsoc.2019.11.020 ↗
36. Effect of reaction melt infiltration temperature on the ablation properties of 2D C/C–SiC–ZrC composites10.1016/j.corsci.2012.01.001 ↗
37. Ablation behavior of sharp-shape C/C-SiC-ZrB2 composites under oxyacetylene flame10.1016/j.jallcom.2017.04.188 ↗
38. UHTC coating reinforced by HfC nanowires against ablation for C/C composites10.1016/j.surfcoat.2017.01.014 ↗
39. Oxidation and ablation protection of double layer HfB2-SiC-Si/SiC-Si coating for graphite materials10.1016/j.jallcom.2018.12.256 ↗
40. Oxidation/ablation behaviors of hafnium carbide-silicon carbonitride systems at 1500 and 2500 ℃10.1016/j.ceramint.2020.06.161 ↗
41. Ablation behaviour and mechanical property of the B-modified SiC/HfC-SiC composites in cyclic ablation environment10.1016/j.corsci.2020.108829 ↗
42. Oxidation resistance analysis of zirconium carbide sintered by hot-pressing