journal article·2015-04

Corrosion and stress corrosion cracking of ultra-high-purity Mg5Zn

Zhiming Shi, Joelle Hofstetter, Fuyong Cao, Peter J. Uggowitzer, Matthew S. Dargusch, Andrej Atrens

Corrosion Science· Volume 93
Publisher page

Abstract

This paper reports on the measurement of the corrosion rate, and the stress corrosion cracking threshold stress, for ultra-high-purity Mg-5Zn. The corrosion rate was higher than the intrinsic corrosion rate of ultra-high-purity Mg, attributed to the quality of the corrosion product film. The threshold stress for stress corrosion cracking, at an applied stress rate of 0.00016 MPa s(-1), was equal to 0.7 times the yield stress in air. The ductility of the cracking indicated that the stress corrosion cracking mechanism was probably hydrogen enhanced localized plasticity. (C) 2015 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Hydrogen Storage and Materials · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. J.F. Löffler, P.J. Uggowitzer, C. Wegmann, M. Becker, H.K. Feichtinger, Process and Apparatus for Vacuum Distillation of High-Purity Magnesium: European Patent Application PCT/EP 2013/000131-WO2013/107644, 2012.
2. Assessing the degradation performance of ultrahigh-purity magnesium in vitro and in vivo10.1016/j.corsci.2014.09.008 ↗
3. Corrosion of ultra-high-purity Mg in 3.5% NaCl solution saturated with Mg(OH)210.1016/j.corsci.2013.05.018 ↗
4. Production of high purity magnesium alloys by melt purification with Zr10.1002/adem.201200054 ↗
5. Corrosion mechanisms of magnesium alloys10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
6. Understanding magnesium corrosion mechanism: a framework for improved alloy performance10.1002/adem.200310405 ↗
7. Corrosion mechanism applicable to biodegradable magnesium implants10.1016/j.mseb.2010.12.017 ↗
8. Advances in Mg corrosion and research suggestions10.1016/j.jma.2013.09.003 ↗
9. Review of recent developments in the field of magnesium corrosion
10. Calculated phase diagrams and the corrosion of die-cast Mg–Al alloys10.1016/j.corsci.2008.12.015 ↗
11. Corrosion behaviour in salt spray and in 3.5% NaCl solution saturated with Mg(OH)2 of as-cast and solution heat-treated binary Mg-X alloys: X=Mn, Sn, Ca, Zn, Al, Zr, Si, Sr10.1016/j.corsci.2013.06.030 ↗
12. Corrosion behaviour in salt spray and in 3.5% NaCl solution saturated with Mg(OH)2 of as-cast and solution heat-treated binary Mg–RE alloys: RE=Ce, La, Nd, Y, Gd10.1016/j.corsci.2013.06.032 ↗
13. High-strength low-alloy (HSLA) Mg–Zn–Ca alloys with excellent biodegradation performance10.1007/s11837-014-0875-5 ↗
14. Corrosion behaviour of a nominally high purity Mg ingot produced by permanent mould direct chill casting10.1016/j.corsci.2012.04.030 ↗
15. Corrosion performance and mechanical properties of sputter-deposited MgY and MgGd alloys10.1016/j.corsci.2013.08.027 ↗
16. Stress corrosion cracking of magnesium alloys10.1002/adem.200900287 ↗
17. A critical review of the stress corrosion cracking (SCC) of magnesium alloys10.1002/adem.200500071 ↗
18. Comparison of the linearly increasing stress test and the constant extension rate test in the evaluation of transgranular stress corrosion cracking of magnesium10.1016/j.msea.2007.03.021 ↗
19. Characterisation of stress corrosion cracking (SCC) of Mg–Al Alloys10.1016/j.msea.2007.11.064 ↗
20. The fractography of stress corrosion cracking (SCC) of Mg–Al Alloys10.1007/s11661-008-9475-8 ↗
21. Evaluation of the delayed hydride cracking mechanism for transgranular stress corrosion cracking of magnesium alloys10.1016/j.msea.2007.03.020 ↗
22. Stress-corrosion cracking of magnesium alloys
23. Transgranular SCC in Mg–Al alloys10.1016/S0010-938X(71)80020-3 ↗
24. In-vitro characterization of stress corrosion cracking of aluminium-free magnesium alloys for temporary bio-implant application10.1016/j.msec.2014.06.018 ↗
25. Stress corrosion cracking of rare-earth containing magnesium alloys ZE41, QE22 and Elektron 21 (EV31A) compared with AZ8010.1016/j.msea.2007.07.070 ↗
26. Stress corrosion cracking of new Mg–Zn–Mn wrought alloys containing Si10.1016/j.corsci.2008.02.012 ↗
27. F. Cao, Z. Shi, G. Song, M. Liu, M.S. Dargusch, A. Atrens, Stress corrosion cracking of several solution heat-treated Mg–X alloys, in: F.Cao, PhD Thesis, The University of Queensland, 2015.10.1016/j.corsci.2015.04.010 ↗
28. Role of chlorides on pitting and hydrogen embrittlement of Mg–Mn wrought alloy10.1016/j.corsci.2013.05.030 ↗
29. Stress corrosion cracking of a wrought Mg–Mn alloy under plane strain and plane stress conditions10.1016/j.engfracmech.2013.02.018 ↗
30. Stress corrosion cracking of a recent rare-earth containing magnesium alloy, EV31A, and a common Al-containing alloy, AZ91E10.1016/j.corsci.2013.01.001 ↗
31. Stress corrosion cracking behavior of magnesium alloys EV31A and AZ91E10.1016/j.msea.2013.06.085 ↗
32. Stress corrosion cracking susceptibility of a high strength Mg–7%Gd–5%Y–1%Nd–0.5%Zr alloy10.1016/j.jma.2014.11.004 ↗
33. An innovative specimen configuration for the study of Mg corrosion10.1016/j.corsci.2010.09.016 ↗
34. Linearly increasing stress test (LIST) for SCC research10.1088/0957-0233/4/11/017 ↗