journal article·2011-04

Corrosion behaviour of a 2219 aluminium alloy treated with a chromate conversion coating exposed to a 3.5% NaCl solution

Rossana Grilli, Mark A. Baker, James E. Castle, Barrie Dunn, John F. Watts

Corrosion Science· Volume 53· Issue 4
Publisher page

Abstract

This study investigates the formation of a chromate conversion coating at Al–Cu–Fe–Mn intermetallic sites of an Al2219 alloy and the corrosion initiation at these sites in a 3.5% NaCl solution, using SEM, AES and EDX. Changes in the surface chemistry were monitored after progressive exposures to the solution up to 42 h. The coating was found to be thinner and more defective on the intermetallic. Initially, Al is dissolved and Al(OH)3 deposited on and around the intermetallic. After 42 h of exposure, Al(OH)3, Fe and Mn oxides and small particles of elemental Cu are deposited as corrosion products.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. European Space Agency. “Assessment of chemical conversion coatings for the protection of aluminium alloys”. ESA STM-236; 2008.
2. Shao · Mater. Sci. Eng. · 2003 · A344 · 32310.1016/S0921-5093(02)00445-8 ↗
3. Zhu · Corros. Sci. · 2003 · 45 · 216310.1016/S0010-938X(03)00060-X ↗
4. Liao · Electrochim. Acta · 1999 · 45 · 88110.1016/S0013-4686(99)00299-6 ↗
5. Oki · Mater. Lett. · 2009 · 63 · 199010.1016/j.matlet.2009.06.033 ↗
6. Grilli · Surf. Interface Anal. · 2008 · 40 · 13210.1002/sia.2793 ↗
7. Rabbetts · Trans. Inst. Met. Finish. · 1998 · 76 · B4
8. Brown · Corros. Sci. · 1992 · 33 · 137110.1016/0010-938X(92)90178-6 ↗
9. Brown · Corros. Sci. · 1993 · 34 · 104510.1016/0010-938X(93)90288-R ↗
10. Brown · Corros. Sci. · 1993 · 35 · 25310.1016/0010-938X(93)90156-B ↗
11. Liu · Corros. Sci. · 2005 · 47 · 14510.1016/j.corsci.2004.05.012 ↗
12. Hagans · Surf. Interface Anal. · 1994 · 21 · 6510.1002/sia.740210203 ↗
13. Juffs · Corros. Sci. · 2002 · 44 · 175510.1016/S0010-938X(01)00181-0 ↗
14. Campestrini · Electrochim. Acta · 2001 · 46 · 255310.1016/S0013-4686(01)00475-3 ↗
15. Liu · Corros. Sci. · 2005 · 47 · 34110.1016/j.corsci.2004.06.005 ↗
16. Ramsey · J. Electrochem. Soc. · 1999 · 146 · 407610.1149/1.1392594 ↗
17. Hughes · Surf. Interface Anal. · 1997 · 25 · 22310.1002/(SICI)1096-9918(199704)25:4<223::AID-SIA225>3.0.CO;2-D ↗
18. Lunder · Corros. Sci. · 2005 · 47 · 160410.1016/j.corsci.2004.08.012 ↗
19. Wang · Corros. Sci. · 2010 · 3 · 94310.1016/j.corsci.2009.11.017 ↗
20. Dong · Langmuir · 2010 · 26 · 1083310.1021/la100699u ↗
21. R. Grilli. “Conversion coatings for aluminium alloys: a surface investigation for corrosion mechanisms”, Thesis (Ph.D.), University of Surrey; 2010.
22. Grilli · Corros. Sci. · 2010 · 52 · 285510.1016/j.corsci.2010.04.035 ↗
23. Grilli · Surf. Interface Anal. · 2010 · 42 · 61010.1002/sia.3318 ↗
24. Baker · Corros. Sci. · 1992 · 33 · 129510.1016/0010-938X(92)90137-R ↗
25. Baker · Corros. Sci. · 1993 · 34 · 66710.1016/0010-938X(93)90279-P ↗
26. Castle · Corros. Sci. · 1990 · 30 · 40910.1016/0010-938X(90)90047-9 ↗
27. Castle · Corros. Sci. · 1994 · 36 · 109310.1016/0010-938X(94)90206-2 ↗
28. Akhtar · Appl. Surf. Sci. · 2008 · 254 · 481310.1016/j.apsusc.2008.01.113 ↗
29. Alodine 1200S. Technical process bulletin, Henkel. Surface Technologies; 1999.
30. .
31. Fu · Surf. Sci. · 2004 · 573 · 42610.1016/j.susc.2004.10.007 ↗
32. Buchheit · J. Electrochem. Soc. · 2000 · 147 · 11910.1149/1.1393164 ↗