Influence of boron contents on oxidation behavior and the diffusion mechanism of Fe–B based alloys at 1073K in air
Source abstract
Abstract
Abstract The microstructure and oxidation behavior of Fe–B alloys have been investigated. Oxide scale cross-sectional microstructures oxidized at 1073 K for 100 h have been studied. EPMA investigations show that B 2 O 3 –SiO 2 oxides accumulates in the inner oxide layer which improves the oxidation behavior and oxide layer adhesion considerably. Cyclic oxidation kinetics data indicates that Fe–B 3.08 wt.% alloy presents the best oxidation resistance. The formation of diffusion zone in the Fe–B alloys indicate that the oxidation of the Fe 2 B boride is controlled by boron diffusion. The diffusion zone increases with time and reaches a maximum width of 60–65 μm.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metal Alloys Wear and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Abrasion resistance of high Cr cast irons at an elevated temperature10.1016/S0043-1648(01)00665-2 ↗
2. Effect of phase stability on the wear resistance of white cast iron at 800°C10.1016/S0043-1648(02)00015-7 ↗
3. Effect of boron on the sliding wear of directionally solidified high-chromium white irons10.1016/j.wear.2008.11.009 ↗
4. Chromium oxide scale growth on iron-Chromium alloys II. Influence of alloy composition
5. Solidification structure in a cast B-bearing stainless steel10.1016/j.matlet.2007.02.037 ↗
6. Structural variations in heat treated B-bearing stainless steel10.1016/j.matdes.2008.05.046 ↗
7. Effect of variable heat treatment modes on microstructures of Fe–Cr–B cast iron alloy
8. Effect of heat treatment on microstructure and mechanical properties of high boron white cast iron10.1016/j.msea.2010.09.092 ↗
9. Microstructure and mechanical properties of high boron white cast iron10.1016/j.msea.2007.10.017 ↗
10. ASM handbook
11. Study on improvement of hard phase morphology and properties of hypoeutectic Fe–C–B alloy10.1016/j.jallcom.2013.10.173 ↗
12. High-temperature behavior of the boride layer of 45# carbon steel10.1016/S0254-0584(01)00270-X ↗
13. Effect of boron addition on the cavitation erosion resistance of Fe-based hardfacing alloy10.1016/j.matlet.2006.07.015 ↗
14. High temperature oxidation of γ/γ′-strengthened Co-base superalloys10.1016/j.corsci.2011.02.033 ↗
15. Microstructure and oxidation resistance of Mo–Si–B coating on Nb based in situ composites10.1016/j.corsci.2014.07.006 ↗
16. Low-temperature specific heat of different B2O3 glasses10.1103/PhysRevB.56.32 ↗
17. Temperature effect on structural properties of boron oxide thin films deposited by MOCVD method10.1016/j.tsf.2004.05.107 ↗
18. Investigations on microstructures and toughness of Fe–B cast alloy containing titanium and nitrogen10.1007/s11665-013-0787-5 ↗
19. Effect of boron and heat treatment on mechanical properties of white cast iron for mining application10.1016/S1006-706X(11)60114-3 ↗
20. Effect of yttrium on the cyclic oxidation behaviour of HP40 heat-resistant steel at 1373K10.1016/j.corsci.2010.09.039 ↗
21. Microstructure and crystallography of borides and mechanical properties of Fe–B–C–Cr–Al alloys10.1016/j.jallcom.2015.11.171 ↗
22. Boron solubility in Fe–Cr–B cast irons10.1016/S0921-5093(02)00449-5 ↗
23. High temperature solid state reactivity between iron and chromium monoborides10.1023/A:1012693915788 ↗
24. Growth of boride layers on the 13% Cr steel surface in a mixture of amorphous boron and KBF410.1007/s10853-007-1512-2 ↗
25. J. Jackman. The effect of grain boundary segregation of boron in cast alloy 718 on HAZ microfissuring-A SIMS analysis10.1016/S1359-6454(97)00017-7 ↗
26. D Microstructure and crystallization texture of a low carbon stript cast steel
27. Study on an Fe–TiC surface composite produced in situ10.1016/S0261-3069(98)00049-1 ↗
28. Study on improving the toughness of Fe–B–C alloy
29. Xu · 2003 · 341
30. Three-body abrasive wear behavior of low carbon Fe–B cast alloy and its microstructures under different casting process10.1007/s11249-011-9748-z ↗
31. Effect of rare earth and titanium additions on the microstructures and properties of low carbon Fe–B cast steel10.1016/j.msea.2007.02.032 ↗
32. Bansal · 1986
33. Glass sealants for carbon–carbon composites10.1007/BF01151661 ↗
34. Microstructure and oxidation behavior of directionally solidified Mo–Mo5SiB2 (T2)–Mo3Si alloys10.1016/j.jallcom.2007.08.064 ↗
35. Boronated carbons: structural characterization and low temperature physical properties of disordered solids10.1039/a703625f ↗
36. Improved antioxidative ability of porous carbons by boron-doping10.1016/S1872-5805(09)60007-X ↗
37. Effect of low-level boron doping on oxidation behavior of polyimide-derived carbon films10.1016/S0008-6223(99)00245-6 ↗
38. Oxidation behavior of αMo–Mo3Si–Mo5SiB2 (T2) three phase system10.1016/S0966-9795(01)00118-2 ↗
39. Oxidation behaviour of two-dimensional C/SiC modified with self-healing Si–B–C coating in static air10.1016/j.corsci.2012.08.003 ↗
40. Preparation and oxidation protection of CVD SiC/a-BC/SiC coatings for 3D C/SiC composites10.1016/j.corsci.2009.01.026 ↗
41. Graham oxidation of Fe–C alloys at 500°C10.1007/BF00609975 ↗
42. High-temperature corrosion of electric-arc coatings sprayed from powder core wires based on the Fe–Cr–B–Al system10.1007/s11003-009-9131-5 ↗
43. Liquid metal corrosion of 316L stainless steel, 410 stainless steel, and 1015 carbon steel in a molten zinc bath10.1007/s11661-007-9320-5 ↗
44. Effect of Fe2B orientation on erosion-corrosion behavior of Fe-3.5wt.% B steel in flowing zinc10.1016/j.corsci.2015.05.039 ↗
45. Interface characteristics and corrosion behaviour of oriented bulk Fe2B alloy in liquid zinc10.1016/j.corsci.2013.08.033 ↗
46. J. Zhang. Microstructure and crystallography of borides and secondary precipitation in 18wt.% Cr-4wt.% Ni-1wt.% Mo-3.5wt.% B-0.27wt.%C steel10.1016/j.actamat.2011.11.004 ↗
47. Diffusion of near surface defects during the thermal oxidation of silicon10.1063/1.365420 ↗
48. A diffusion model for describing the bilayer growth (FeB/Fe2B) during the iron powder-pack boriding10.1016/j.apsusc.2005.01.016 ↗
49. Oxidation of alloys involving noble metals10.1149/1.2430159 ↗